Inorganic-organic hybrid electrocatalyst derived from metal-organic frameworks enabling large-current-density hydrogen evolution

Ning Song ,  Wenhao Wu ,  Guojia Li ,  Wenzhuo Liu ,  Hongjun Dong ,  Yun Wang ,  Yangyang Yu ,  Chunmei Li

Citation:  Ning Song, Wenhao Wu, Guojia Li, Wenzhuo Liu, Hongjun Dong, Yun Wang, Yangyang Yu, Chunmei Li. Inorganic-organic hybrid electrocatalyst derived from metal-organic frameworks enabling large-current-density hydrogen evolution[J]. Chinese Chemical Letters, 2027, 38(1): 113242. doi: 10.1016/j.cclet.2026.113242 shu

Inorganic-organic hybrid electrocatalyst derived from metal-organic frameworks enabling large-current-density hydrogen evolution

English

  • The global energy shortage and environmental pollution, driven by excessive consumption of fossil fuels, have intensified the urgency for clean energy solutions [1-6]. Hydrogen, as a zero-emission energy carrier, exhibits tremendous application potential for achieving carbon neutrality [7-10]. Among various hydrogen production technologies, electrocatalytic water splitting stands out for its scalability and efficiency [11-13]. The hydrogen evolution reaction (HER) under acidic conditions exhibits faster kinetics and higher energy efficiency, which are crucial for low-energy, high-yield hydrogen production. However, the cost-effective nickel-based catalysts applied in industry still exhibit limitations such as elevated energy consumption and susceptibility to deactivation, primarily attributed to their inherent high overpotential and inadequate corrosion resistance [14]. Therefore, the development of efficient and stable catalysts is of great significance for large-scale electrolysis of water for hydrogen production.

    Inorganic-organic hybrid materials have been attracting attention in the field of scalable device manufacturing due to their lightweight nature, flexibility, and facile processability [15]. For example, Peng et al. synthesized an organic-inorganic hybrid heterojunction using oxalate and polyaniline (PANI) by an electrodeposition method. The localized d electrons in Co0.59Ni0.41C2O4 and the delocalized π electrons in PANI exhibited strong π-d electron coupling, which resulted in a low overpotential and the reliable stability for HER [16]. Metal-organic frameworks (MOFs) exhibit intrinsically high specific surface areas, tunable pore sizes and topologies‌, versatile functionalization potential, and rational designability [17-19]. These properties enable pristine MOFs and their derivatives‌ to serve as versatile platforms for diverse applications, including gas storage/separation, heterogeneous catalysis, environmental remediation, energy conversion/storage, and biomedicine ‌ among others‌ [20-22]. However, pristine MOFs often face intrinsic limitations in electrocatalysis, such as insufficient electrical conductivity and structural vulnerability under harsh operational conditions [23,24]. The conversion of MOFs into inorganic-organic hybrid materials‌ represents a distinctive strategy in electrocatalytic material engineering because this methodology can effectively control active sites, optimize charge transfer networks, and improve structural robustness, thereby achieving high-performance catalysts.

    In this study, based on the electrochemical reconstruction strategy of MOFs, we developed a new inorganic-organic hybrid electrocatalyst. As shown in Fig. 1a, when a Zn2+-containing solution with a trace amount of Rh ions is added to the 2-methylimidazole solution, during the crystal growth process of Zn-ZIF-L, Rh atoms replace Zn nodes to form two-dimensional RhZn-ZIF-L nanosheets. Driven by electrochemical activation, RhZn-ZIF-L is transformed into a functionalized polyacrylonitrile (FPAN) rich in carboxyl (COOH) and amide (CONH2) groups, and the Rh ions released from RhZn-ZIF-L are simultaneously in situ reduced to Rh quantum dots (QDs) on the surface of the functionalized PAN, forming the RhQDs/FPAN electrocatalyst. Experimental results show that the electrocatalytic performance of the best RhQDs/FPAN-3 is significantly superior to that of commercial Pt/C and the reported inorganic-organic hybrid electrocatalysts so far, and it can maintain stable operation for 520 h at a large current density (1000 mA/cm2), demonstrating promising application potential.

    Figure 1

    Figure 1.  (a) Preparation diagram of RhQDs/FPAN electrocatalyst. SEM images of (b) Zn-ZIF-L, (c) Rh0.1Zn0.9-ZIF-L and (d) RhQDs/FPAN-3. (e) TEM, (f) diameter size statistics of Rh QDs, (g) HRTEM, and (h) HAADF-TEM and corresponding mapping images of RhQDs/FPAN-3.

    First, 2-methylimidazole (1.298 g) was dissolved in 40 mL of deionized water and stirred in a water bath at 30 ℃ for 30 min to form solution A. Next, Zn(NO3)2·6H2O (0.5171 g) and RhCl3·3H2O (0.0509 g) were dissolved in 40 mL of deionized water and stirred in a water bath at 30 ℃ for 30 min to form solution B. After solution B was poured into solution A and stirred for 2 h. The resulting solid was centrifuged and washed with deionized water and dried under vacuum at 60 ℃ to obtain Rh0.1Zn0.9-ZIF-L (Rh:Zn = 1:9). Finally, the electrochemical reaction of Rh0.1Zn0.9-ZIF-L at 0.5 V vs. RHE for 12 h in 0.5 mol/L H2SO4, using a three-electrode configuration, yielded RhQDs/FPAN-3. The performance of the catalysts was optimized by varying the molar ratio of Rh to Zn, and the corresponding products were Zn-ZIF-L (Rh:Zn = 0:10), Rh0.166Zn0.830-ZIF-L (Rh:Zn = 1:5), Rh0.125Zn0.875-ZIF-L (Rh:Zn = 1:7) and Rh0.083Zn0.917-ZIF-L (Rh:Zn = 1:11), which were named as FPAN, RhQDs/FPAN-1, RhQDs/FPAN-2, RhQDs/FPAN-4 after electrochemical activation, respectively.

    Experimental details for the instrument characterizations and the electrochemical test procedures are shown in Supporting information.

    The morphology evolutions of the sample during the electrochemical activation process were investigated by scanning electron microscopy (SEM). Fig. 1b and Fig. S1 (Supporting information) present the SEM images of Zn-ZIF-L, demonstrating a uniform leaf-shaped nanosheet with smooth surfaces and well-defined edges, which confirms the successful fabrication of Zn-ZIF-L with high crystallinity. Fig. 1c shows a SEM image of Rh0.1Zn0.9-ZIF-L, indicating that the replacement of Zn nodes with Rh atoms does not cause any morphological changes. Fig. 1d shows a SEM image of RhQDs/FPAN-3, in which although the morphology of RhQDs/FPAN-3 has changed, it maintains a two-dimensional nanosheet structure. No large agglomerated nanoparticles are observed, indicating the high dispersion of Rh QDs on the surface of FPAN. As evidenced by the transmission electron microscopy (TEM) image in Fig. 1e, a large number of high-density and uniformly distributed Rh QDs are embedded on the surface of FPAN. Further diameter size statistics reveal that the average size of these ultra-small Rh QDs is only 3.45 nm (Fig. 1f). Furthermore, as shown in Fig. 1g, the high-resolution TEM (HRTEM) image obtained from the Rh QDs displays a lattice spacing of 0.192 nm, corresponding to the (200) crystal plane of metal Rh. Fig. 1h shows high-angle annular dark-field TEM (HAADF-TEM) and corresponding elemental mapping images of RhQDs/FPAN-3, showing the uniform distribution of C, N, O, and Rh elements, which also confirms the uniform distribution of Rh QDs on the FPAN nanosheets. This ultra-small, high-density and highly dispersed structural feature of Rh QDs on FPAN may be related to the fixed-point reduction of Rh nodes in Rh0.1Zn0.9-ZIF-L during the electrochemical activation process as it transforms into FPAN, which not only can enhance the conductivity and stability of FPAN matrix, but also may induce the nano-island effect, thereby enhancing HER performance [25].

    X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectra, and Raman spectra were used to study the structure of Zn-ZIF-L, Rh0.1Zn0.9-ZIF-L, and RhQDs/FPAN-3. Fig. 2a reveals the diffraction peaks of Zn-ZIF-L are well consistent the simulated pattern, confirming the successful synthesis of Zn-ZIF-L with a high purity. Based on the tunable properties of metal nodes of Zn-ZIF-L, Rh0.1Zn0.9-ZIF-L was also prepared by replacing the Zn nodes with Rh atoms, as its XRD pattern is similar to that of Zn-ZIF-L. However, the magnified XRD (Fig. 2b) show that the diffraction peaks of Rh0.1Zn0.9-ZIF-L exhibit distinct shifts compared to those of Zn-ZIF-L, which may be because the partial substitution of Rh atoms for Zn nodes adjusts the skeleton structure of Zn-ZIF-L. FT-IR spectra are used to analyze the molecular structure of the samples. As shown in Fig. 2c, the FT-IR spectrum of Zn-ZIF-L aligns with that of previous reports [26]. The characteristic absorption peak at 421 cm-1 is attributed to the Zn–N bonds, while two sets of absorption bands at 600–800 and 900–1350 cm-1 are the out-of-plane and in-plane bending of the imidazole ring, respectively. In addition, the absorption peaks at 2927 and 3135 cm-1 stem from the stretching vibrations of aliphatic and aromatic C—H bonds in imidazole, respectively. The peaks at 675/693, 1350–1500, and 1584 cm-1 originate from the stretching vibrations of N—H groups, imidazole ring, and C═N bonds, respectively. These typical peaks in the FT-IR spectrum of Rh0.1Zn0.9-ZIF-L are nearly identical to those of Zn-ZIF-L, indicating that the framework structure of Zn-ZIF-L has been well preserved after replacing some of the Zn nodes with Rh atoms. Furthermore, Raman spectrum of Rh0.1Zn0.9-ZIF-L is also the same as that of Zn-ZIF-L (Fig. 2d), in which several important fingerprint peaks are located at 176, 283, 684, 760, 833, 954, 1021, 1155, 1182, 1310, 1383, 1500, 1505, 2931, 3114, and 3137 cm-1, which correspond to the typical vibrational modes of Zn-ZIF-L framework (Table S1 in Supporting information) [27], confirming the results obtained from FT-IR spectra. The nitrogen adsorption-desorption isotherms were employed to investigate the changes in specific surface area and pore size after the Rh atoms replace the Zn nodes of Zn-ZIF-L (Figs. S2 and S3 in Supporting information). The specific surface area of Rh0.1Zn0.9-ZIF-L increases to 57.9 m2/g compared to that of Zn-ZIF-L (33.0 m2/g), while the average pore size of Rh0.1Zn0.9-ZIF-L decreases to 5.5 nm compared to that of Zn-ZIF-L (7.9 nm). This structural adjustment is more conducive to electrochemical activation, promoting the structural transformation from Zn-ZIF-L to FPAN. The Rh and Zn contents in Rh0.1Zn0.9-ZIF-L were detected via inductively coupled plasma optical emission spectrometry (Table S2 in Supporting information). The resulting atomic ratio of Rh to Zn is determined as 0.1:0.87, which is close to the theoretical value (0.1:0.9).

    Figure 2

    Figure 2.  (a, b) XRD, (c) FT-IR and (d) Raman spectra of Zn-ZIF-L and Rh0.1Zn0.9-ZIF-L. (e) XRD and (f) FT-IR spectra of commercial PAN, FPAN and RhQDs/FPAN-3.

    It is worth noting that, during the electrochemical activation process, we observed a significant attenuation in the chronoamperometry curve until it was stabilized (Fig. S4 in Supporting information), suggesting that a structural transformation may have occurred in Rh0.1Zn0.9-ZIF-L. Therefore, the XRD analysis of Zn-ZIF-L and Rh0.1Zn0.9-ZIF-L after electrochemical activation was carried out again. As shown in Fig. 2e, apart from the carbon paper background, the new diffraction peaks for the FPAN obtained from the activated Zn-ZIF-L match well with standard commercial PAN, demonstrating the structural transformation from Zn-ZIF-L to FPAN. Additionally, in the XRD of RhQDs/FPAN-3 obtained from the activated Rh0.1Zn0.9-ZIF-L, several diffraction peaks corresponding to metallic Rh are generated (PDF #97–42–6969), preliminarily indicating the formation of the RhQDs/FPAN hybrid structure [28]. These were further confirmed by the subsequent FT-IR analysis performed on commercial PAN, FPAN, and RhQDs/FPAN-3. As shown in Fig. 2f, the FT-IR spectrum of commercial PAN is consistent with previous reports [29,30], including C—H out-of-plane stretching vibration peaks (1230 and 1367 cm-1), C—H bending vibration peak (1450 cm-1), C≡N stretching vibration peak (2245 cm-1), C—H stretching vibration peak (2930cm-1), and C—O stretching vibration peak of residual copolymer monomers (1062 and 1736 cm-1). Compared to commercial PAN, FPAN and RhQDs/FPAN exhibit the disappearance of the stretching vibration peak of C≡N at 2245 cm-1. Meanwhile, the out-of-plane bending vibration peak of O—H in COOH groups and stretching vibration peak of N—H in CONH2 groups are generated at 970 and 3430 cm-1, respectively [31,32]. These results demonstrate that the electrochemical activation process promotes the hydrolysis reaction of C≡N moieties, generating abundant COOH and CONH2 groups, in which the former can act as a proton transfer station to enhance HER reaction kinetics, while the latter can coordinate with the surface atoms of Rh QDs to enhance stability and electron transfer efficiency, thereby collaboratively achieving high HER activity and stability.

    The chemical states and compositions of RhQDs/FPAN-3 are investigated via X-ray photoelectron spectroscopy (XPS). The survey spectrum reveals the presence of C, O, N, and Rh elements in RhQDs/FPAN-3 (Fig. S5 in Supporting information). The C 1s XPS of RhQDs/FPAN-3 is deconvoluted into five characteristic peaks at binding energies of 284.8 eV (C–C), 285.8 eV (C–N), 290.4 eV (O–C═O), 291.7 eV (π-π), and 293.3 eV (CF3), respectively (Fig. 3a) [33-36]. The deconvolution of the O 1s XPS in Fig. 3b shows two characteristic peaks at binding energies of 532.5 eV (O–C═O groups) and 535.2 eV (adsorbed H2O molecules), respectively [37,38]. In addition, as shown in Fig. 3c, the N 1s XPS of RhQDs/FPAN-3 can be deconvoluted into two characteristic peaks at 400.2 eV (Rh–N bonds) and 401.9 eV (NH2) [39,40]. Based on the results from C 1s, O 1s, and N 1s XPS, we deduce that some C≡N moieties in RhQDs/FPAN-3 undergo hydrolysis during the electrochemical activation process, producing CONH2 and COOH groups, further confirming the results from FT-IR spectra. Particularly, the Rh–N bonds are formed between Rh QDs and FPAN matrix, which improves the stability and accelerates electron transfer kinetics, thus enhancing the HER performance. As shown in Fig. 3d, the Rh 3d XPS shows two distinct peaks at 307.3 and 312.6 eV, which originate from the Rh0 3d5/2 and Rh0 3d3/2 states of metal Rh, respectively, suggesting the generation of Rh QDs [41]. Additionally, the other two peaks at 310.1 and 315.0 eV correspond to the Rh3+ 3d5/2 and Rh3+ 3d3/2 states, respectively, which may be attributed to the surface oxidation of the Rh QDs [42].

    Figure 3

    Figure 3.  XPS spectra of RhQDs/FPAN-3: (a) C 1s, (b) O 1s, (c) N 1s, and (d) Rh 3d.

    Fig. 4a shows the linear sweep voltammetry (LSV) curves for the HER in 0.5 mol/L H2SO4 solution. FPAN has almost no electrocatalytic HER activity. However, after replacing Zn nodes with Rh atoms in Zn-ZIF-L framework, a series of derived RhQDs/FPAN catalysts have been endowed with HER performance far exceeding that of commercial Pt/C. Specifically, without performing iR compensation, RhQDs/FPAN-3 requires only an overpotential of 14 mV to achieve a current density of 10 mA/cm2, which is significantly lower than FPAN (294 mV), RhQDs/FPAN-1 (19 mV), RhQDs/FPAN-2 (17 mV), RhQDs/FPAN-4 (18 mV), and commercial Pt/C (32 mV). The corresponding Tafel plot is shown in Fig. 4b, where the Tafel slope of RhQDs/FPAN-3 is only 23.3 mV/dec within the current density range of 5–18 mA/cm2, which is significantly lower than that of FPAN (154.0 mV/dec), RhQDs/FPAN-1 (32.2 mV/dec), RhQDs/FPAN-2 (29.4 mV/dec), RhQDs/FPAN-4 (30.1 mV/dec), and commercial Pt/C (32.5 mV/dec), indicating its fastest HER kinetics [43-45]. For the convenience of comparison, the LSV curves after iR compensation are also plotted for the optimal RhQDs/FPAN-3 (Fig. S6 in Supporting information), which exhibits overpotential of 5 and 98 mV at the current densities of 10 and 1000 mA/cm2, respectively. As summarized in Fig. 4c, the HER activity of RhQDs/FPAN-3 far exceeds that of the inorganic-organic hybrid electrocatalysts reported so far (Table S3 in Supporting information). Furthermore, Fig. 4d shows the mass activity comparison, where the mass activity of RhQDs/FPAN-3 is as high as 1085.63 A/g at an overpotential of 100 mV, achieving 2.1 times that of commercial Pt/C (519.72 A/g). Remarkably, Fig. 4e shows an overpotential of only 360 mV at a large current density of 1000 mA/cm2, which is significantly lower than that of commercial Pt/C (431 mV), clearly demonstrating significant practical application potential.

    Figure 4

    Figure 4.  (a) LSV curves and (b) Tafel plots of various samples. (c) Comparison of overpotential at 10 mA/cm2 of RhQDs/FPAN-3 with reported catalysts. (d) Mass activity of RhQDs/FPAN-3 and Pt/C. (e) Large-current-density LSV curves for FPAN, RhQDs/FPAN-3, and Pt/C.

    Electrochemical impedance spectra (EIS) were employed to investigate the charge transfer kinetics between the catalyst surface and the electrolyte in the HER (Fig. 5a). The equivalent circuit model was fitted based on Nyquist plots (Fig. S7 in Supporting information). The results show that the charge transfer resistance (Rct) of RhQDs/FPAN-3 is 623.9 Ω, which is significantly lower than that of FPAN (77,852.0 Ω), RhQDs/FPAN-1 (1268.0 Ω), RhQDs/FPAN-2 (885.0 Ω), and RhQDs/FPAN-4 (1179.0 Ω), suggesting that it has higher electron transfer efficiency [46,47]. In addition, the double-layer capacitance (Cdl) is further calculated by cyclic voltammetry curves at different scan rates in the non-Faraday region to investigate electrochemical active surface area (ECSA) of the samples (Fig. S8 in Supporting information). As depicted in Fig. 5b, RhQDs/FPAN-3 has the highest Cdl value of 4.48 mF/cm2, which is significantly higher than that of FPAN (0.18 mF/cm2), RhQDs/FPAN-1 (2.64 mF/cm2), RhQDs/FPAN-2 (3.78 mF/cm2), and RhQDs/FPAN-4 (3.18 mF/cm2). Because of the linear positive correlation between Cdl and ECSA, RhQDs/FPAN-3 has the largest ECSA among all the samples, suggesting that it has the largest number of accessible active sites to enhance HER performance [48]. To evaluate the practical application potential of RhQDs/FPAN catalysts, the chronoamperometric experiments were conducted on RhQDs/FPAN-3. As shown in Fig. 5c, RhQDs/FPAN-3 can maintain stable operation for 137 and 520 h without any curve decay at current densities of 10 and 1000 mA/cm2, respectively. Notably the LSV curve of RhQDs/FPAN-3 after stable operation almost coincides with that of its initial state, and the overpotential only shows a decay of 2 mV at a current density of 1000 mA/cm2 (Fig. 5d). To comprehensively assess the structural and chemical stability of RhQDs/FPAN-3 following prolonged HER, morphological and spectroscopic characterizations were conducted after the reaction. Comparative TEM analysis (Fig. S9 in Supporting information) revealed that RhQDs remained uniformly dispersed on the FPAN before and after prolonged HER, with no detectable aggregation or particle coarsening, confirming structural integrity. FT-IR spectra (Fig. S10 in Supporting information) further demonstrated negligible shifts or intensity variations in characteristic absorption peaks, indicating effective preservation of the functional group. These results demonstrate that RhQDs/FPAN-3 possesses outstanding stability, confirming the great potential in acidic HER applications.

    Figure 5

    Figure 5.  (a) EIS and (b) Cdl plots of various samples. (c) Chronoamperometric curves of RhQDs/FPAN-3. (d) LSV curves of RhQDs/FPAN-3 before and after HER. (e) In situ SHINERS of RhQDs/FPAN-3 in the HER. (f) The possible HER mechanism over RhQDs/FPAN catalyst. All electrochemical tests were carried out in 0.5 mol/L H2SO4.

    To investigate the HER mechanism of RhQDs/FPAN electrocatalysts, in situ shell-isolated nanoparticle enhanced Raman spectroscopy (SHINERS) experiments were conducted on RhQDs/FPAN-3. As shown in Fig. 5e, a series of Raman peaks related to the framework structure of FPAN are also observed (Table S4 in Supporting information) at open-circuit potential (OCP). Besides these, a strong fingerprint peak appears at 296 cm-1, which originate from the vibration absorption of the Rh–N bond in RhQDs/FPAN-3 [49], being consistent with XPS analyses. This indicates that Rh QDs are firmly anchored to the FPAN surface through the strong bonding effect between the CONH2 groups and the surface Rh atoms, which significantly improves the conductivity and stability of the catalyst. Additionally, two strong vibration absorption peaks appear at 678 and 1413 cm-1 under the OCP condition, which originate from the CONH2 groups [50,51]. Another strong vibration absorption peak observed at 1139 cm-1 can be attributed to the COOH groups [52]. We observed that these peaks are weakened after applying potential, suggesting that the HER process facilitates the hydrolysis of CONH2 groups that are not bonded to Rh QDs and hydrogen spillover from COOH groups to the surface atoms of Rh QDs. Meanwhile, a strong Raman peak of Rh-H intermediate (1910–2020 cm-1) is also detected under the OCP condition [53,54], further indicating a strong hydrogen spillover from COOH groups to Rh QDs. Nevertheless, the Raman peak of the Rh-H intermediate is weakened but remains stable after applying voltages, indicating that the Rh QDs surface can rapidly release hydrogen gas and has outstanding hydrogen evolution kinetics. Consequently, a plausible electrocatalytic HER mechanism for the RhQDs/FPAN electrocatalysts was proposed (Fig. 5f). Upon HER initiation, the H+ dissociates from the COOH group and migrates to the surface of Rh QDs via hydrogen spillover, forming a Rh–H intermediate upon electron uptake. The resultant COO- group then functions as a proton transfer station, binding a H+ from the electrolyte to regenerate the COOH group. Subsequently, the COOH group releases a H+ again, reverting to COO-, while this H+ reacts with the hydrogen atom of the Rh–H intermediate to yield hydrogen gas upon electron uptake. Upon HER completion, the COO- group recaptures a H+ from the electrolyte, thereby restoring the catalyst to its initial state.

    In summary, we prepared a new inorganic-organic hybrid electrocatalyst through the electrochemical reconstruction of MOFs during the electrochemical activation. In the fabricated RhQDs/FPAN electrocatalyst, Rh QDs are anchored to the FPAN surface by forming Rh–N bonds with CONH2 groups through their surface atoms, which can enhance the conductivity and stability. Meanwhile, the COOH group can act as a proton transfer station and generate hydrogen spillover to promote proton transfer from it to Rh ODs. As a result, RhQDs/FPAN-3 achieves the current densities of 10 and 1000 mA/cm2 at overpotentials of only 14 and 360 mV, respectively, which are significantly better than the commercial Pt/C (32 and 431 mV) and the reported inorganic-organic hybrid electrocatalysts so far. Meanwhile, RhQDs/FPAN-3 can maintain stable operation for 137 and 520 h at current densities of 10 and 1000 mA/cm2, respectively. In consequence, the developed inorganic-organic hybrid electrocatalyst RhQDs/FPAN has significant prospects for industrial applications, such as electrolysis and renewable energy conversion.

    Ning Song: Writing – original draft, Formal analysis, Data curation, Conceptualization. Wenhao Wu: Validation, Formal analysis. Guojia Li: Validation, Formal analysis. Wenzhuo Liu: Validation, Formal analysis. Hongjun Dong: Writing – review & editing, Validation, Supervision, Methodology. Yun Wang: Writing – review & editing, Supervision, Conceptualization. Yangyang Yu: Writing – review & editing, Validation, Resources. Chunmei Li: Writing – review & editing, Supervision, Funding acquisition.

    The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

    This work is supported by the National Natural Science Foundation of China (No. 52072153), the Graduate Research Innovation Program of Jiangsu Provincial (No. KYCX24_4008), and the College Student Innovation and Entrepreneurship Project (Nos. X2025102990467, X2025102990460).

    Supplementary material associated with this article can be found, in the online version, at doi:10.1016/j.cclet.2026.113242.


    1. [1]

      R. Ram, L. Xia, H. Benzidi, et al., Science 384 (2024) 1373–1380. doi: 10.1126/science.adk9849

    2. [2]

      C. Li, J. Wang, L. Tong, et al., Coordin. Chem. Rev. 502 (2024) 215623. doi: 10.1016/j.ccr.2023.215623

    3. [3]

      H. Dong, C. Qu, C. Li, et al., Chin. J. Catal. 70 (2025) 142–206. doi: 10.3390/a18030142

    4. [4]

      Y. Zhou, L. Sheng, L. Chen, et al., Chin. Chem. Lett. 36 (2025) 109588. doi: 10.1016/j.cclet.2024.109588

    5. [5]

      J. Cheng, N. Song, H. Liu, et al., Int. J. Hydrogen Energ. 156 (2025) 150410. doi: 10.1016/j.ijhydene.2025.150410

    6. [6]

      Y. Yi, X. Chen, Y. Zhao, et al., Energy Technol-Gen. 13 (2025) 2301520. doi: 10.1002/ente.202301520

    7. [7]

      W. Zhao, J. Ma, D. Tian, et al., Chin. J. Catal. 62 (2024) 287–295. doi: 10.1016/S1872-2067(24)60057-4

    8. [8]

      J. Li, J. Jia, D. Wang, et al., Chem. Eng. J. 498 (2024) 155194. doi: 10.1016/j.cej.2024.155194

    9. [9]

      Y. Pan, J. Gao, E. Lv, et al., Adv. Funct. Mater. 33 (2023) 2303833. doi: 10.1002/adfm.202303833

    10. [10]

      X. Liu, H. Pang, X. Kou, et al., Chin. Chem. Lett. 37 (2026) 111567. doi: 10.1016/j.cclet.2025.111567

    11. [11]

      P. Zhang, S. Hong, N. Song, et al., Chin. Chem. Lett. 35 (2024) 109073. doi: 10.1016/j.cclet.2023.109073

    12. [12]

      H. Li, X. Zi, J. Wu, et al., Nano Res. 18 (2025) 94907146. doi: 10.26599/nr.2025.94907146

    13. [13]

      T. Long, H. Wang, Chin. Chem. Lett. 37 (2026) 110623. doi: 10.1016/j.cclet.2024.110623

    14. [14]

      C. Chen, P. Olu, R. Fan, et al., ChemSusChem 18 (2025) e202401415. doi: 10.1002/cssc.202401415

    15. [15]

      S. Cogal, G. Cogal, M. Mičušík, et al., Int. J. Hydrogen Energ. 49 (2024) 689–700. doi: 10.1016/j.ijhydene.2023.09.002

    16. [16]

      S. Zhao, L. Yin, L. Deng, et al., Adv. Funct. Mater. 33 (2023) 2211576. doi: 10.1002/adfm.202211576

    17. [17]

      N. Song, J. Jiang, S. Hong, et al., Chin. J. Catal. 59 (2024) 38–81. doi: 10.1016/S1872-2067(23)64622-4

    18. [18]

      S. Sanati, R. Varma, M. Liu, et al., Energy Environ. Sci. 18 (2025) 7733–7755. doi: 10.1039/d5ee02029h

    19. [19]

      Y. Li, J. Li, H. Dong, et al., Chin. Chem. Lett. 37 (2026) 112101. doi: 10.1016/j.cclet.2025.112101

    20. [20]

      N. Rosi, J. Eckert, M. Eddaoudi, et al., Science 300 (2003) 1127–1129. doi: 10.1126/science.1083440

    21. [21]

      C. Serre, F. Millange, C. Thouvenot, et al., J. Am. Chem. Soc. 124 (2002) 13519–13526. doi: 10.1021/ja0276974

    22. [22]

      P. Zhang, H. Cheng, F. Gu, et al., Surf. Interfaces 42 (2023) 103368. doi: 10.1016/j.surfin.2023.103368

    23. [23]

      Z. Gao, C. Wang, J. Li, et al., Acta Phys. Chim. Sin. 37 (2021) 2010025.

    24. [24]

      S. Yuan, L. Feng, K. Wang, et al., Adv. Mater. 30 (2018) 1704303. doi: 10.1002/adma.201704303

    25. [25]

      B. Chen, P. Hu, F. Yang, et al., Small 19 (2023) 2207177. doi: 10.1002/smll.202207177

    26. [26]

      Z. Low, J. Yao, Q. Liu, et al., Cryst. Growth Des. 14 (2014) 6589–6598. doi: 10.1021/cg501502r

    27. [27]

      J. Mor, P. Utpalla, R. Kumar, et al., Chem. Mater. 35 (2023) 6625–6636. doi: 10.1021/acs.chemmater.3c00292

    28. [28]

      Q. Ouyang, Y. Chen, X. Wang, et al., J. Polym. Res. 22 (2015) 229. doi: 10.1007/s10965-015-0865-5

    29. [29]

      Y. Zhang, L. Wang, L. Li, et al., J. Membrane Sci. 679 (2023) 121694. doi: 10.1016/j.memsci.2023.121694

    30. [30]

      V. Gunka, Y. Hrynchuk, I. Sidun, et al., Chem. Chem. Technol. 16 (2022) 475–483. doi: 10.23939/chcht16.03.475

    31. [31]

      X. Feng, F. Wu, Y. Li, et al., Adv. Mater. 38 (2026) e01779. doi: 10.1002/adma.202501779

    32. [32]

      W. Lyu, Y. Shi, Y. Zheng, et al., J. For. Res. 30 (2019) 739–743. doi: 10.1007/s11676-018-0598-5

    33. [33]

      L. Tang, B. Chen, Z. Zhang, et al., Nat. Commun. 14 (2023) 2301. doi: 10.1038/s41467-023-37997-6

    34. [34]

      Y. Liu, J. Wei, X. Yan, et al., Chin. Chem. Lett. 32 (2021) 861–865. doi: 10.1016/j.cclet.2020.05.037

    35. [35]

      Y. Huang, X. Zhang, N. Chen, et al., Small 19 (2023) 2302841. doi: 10.1002/smll.202302841

    36. [36]

      Y. Luo, R. Chitumalla, S. Ham, et al., ACS Energy Lett. 8 (2023) 5003–5011. doi: 10.1021/acsenergylett.3c01964

    37. [37]

      R. Li, J. Yu, F. Chen, et al., Adv. Funct. Mater. 33 (2023) 2214304. doi: 10.1002/adfm.202214304

    38. [38]

      X. Li, Q. Yang, Y. Yuan, et al., Small 20 (2024) 2401168. doi: 10.1002/smll.202401168

    39. [39]

      E. Murphy, Y. Liu, I. Matanovic, et al., Nat. Commun. 14 (2023) 4554. doi: 10.1038/s41467-023-40174-4

    40. [40]

      Y. Wu, X. Song, S. Xu, et al., Catal. Lett. 149 (2019) 2575–2585. doi: 10.1007/s10562-019-02874-9

    41. [41]

      Y. Guo, X. Yang, X. Liu, et al., Adv. Funct. Mater. 33 (2023) 2209134. doi: 10.1002/adfm.202209134

    42. [42]

      Q. Wang, M. Ming, S. Niu, et al., Adv. Energy Mater. 8 (2018) 1801698. doi: 10.1002/aenm.201801698

    43. [43]

      J. Jia, R. Wang, C. She, et al., Int. J. Hydrogen Energ. 131 (2025) 20–25. doi: 10.1016/j.ijhydene.2025.04.296

    44. [44]

      Y. Yang, J. Hao, C. Lyu, et al., Adv. Funct. Mater. 35 (2025) 2507225. doi: 10.1002/adfm.202507225

    45. [45]

      C. Cai, K. Liu, L. Zhang, et al., Angew. Chem. Int. Ed. 62 (2023) e202300873. doi: 10.1002/anie.202300873

    46. [46]

      H. Dong, L. Tong, P. Zhang, et al., J. Mater. Sci. Technol. 179 (2024) 251–261. doi: 10.1016/j.jmst.2023.10.012

    47. [47]

      Q. Wang, Y. Gong, Y. Tan, et al., Chinese J. Catal. 54 (2023) 229–237. doi: 10.3390/s24010229

    48. [48]

      N. Song, J. Han, M. Zhang, et al., J. Alloy. Compd. 1044 (2025) 184342.

    49. [49]

      C. Clark, C. Reddy, H. Xu, et al., ACS Catal. 10 (2020) 494–509. doi: 10.1021/acscatal.9b03239

    50. [50]

      M. Fernandez-Liencres, A. Navarro, J. Lopez-Gonzalez, et al., Chem. Phys. 266 (2001) 1–17.

    51. [51]

      G. Brown, G. Hope, Electroanal. Chem. 397 (1995) 293–300. doi: 10.1016/0022-0728(95)04159-3

    52. [52]

      W. Shan, R. Liu, H. Zhao, et al., ACS Nano 14 (2020) 11363–11372. doi: 10.1021/acsnano.0c03534

    53. [53]

      M. Wei, Y. Sun, J. Zhang, et al., Energy Environ. Sci. 16 (2023) 4009–4019. doi: 10.1039/d3ee01929b

    54. [54]

      Y. Shimizu, J. Harada, A. Fukazawa, et al., ACS Energy Lett. 8 (2023) 1010–1017. doi: 10.1021/acsenergylett.2c02573

  • Figure 1  (a) Preparation diagram of RhQDs/FPAN electrocatalyst. SEM images of (b) Zn-ZIF-L, (c) Rh0.1Zn0.9-ZIF-L and (d) RhQDs/FPAN-3. (e) TEM, (f) diameter size statistics of Rh QDs, (g) HRTEM, and (h) HAADF-TEM and corresponding mapping images of RhQDs/FPAN-3.

    Figure 2  (a, b) XRD, (c) FT-IR and (d) Raman spectra of Zn-ZIF-L and Rh0.1Zn0.9-ZIF-L. (e) XRD and (f) FT-IR spectra of commercial PAN, FPAN and RhQDs/FPAN-3.

    Figure 3  XPS spectra of RhQDs/FPAN-3: (a) C 1s, (b) O 1s, (c) N 1s, and (d) Rh 3d.

    Figure 4  (a) LSV curves and (b) Tafel plots of various samples. (c) Comparison of overpotential at 10 mA/cm2 of RhQDs/FPAN-3 with reported catalysts. (d) Mass activity of RhQDs/FPAN-3 and Pt/C. (e) Large-current-density LSV curves for FPAN, RhQDs/FPAN-3, and Pt/C.

    Figure 5  (a) EIS and (b) Cdl plots of various samples. (c) Chronoamperometric curves of RhQDs/FPAN-3. (d) LSV curves of RhQDs/FPAN-3 before and after HER. (e) In situ SHINERS of RhQDs/FPAN-3 in the HER. (f) The possible HER mechanism over RhQDs/FPAN catalyst. All electrochemical tests were carried out in 0.5 mol/L H2SO4.

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  134
  • HTML全文浏览量:  14
文章相关
  • 发布日期:  2027-01-12
  • 收稿日期:  2026-04-09
  • 接受日期:  2026-07-27
  • 修回日期:  2026-06-22
  • 网络出版日期:  2026-07-28
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章