Modulating oxygen vacancies in BiOI for enhanced piezo-photocatalytic synergistic degradation

Wenbo Fu ,  Yao Zhang ,  Yong Jiang ,  Wenfeng Lin ,  Zhi Li ,  Jiayue Hu ,  Chunyang Zhai ,  Mingshan Zhu

Citation:  Wenbo Fu, Yao Zhang, Yong Jiang, Wenfeng Lin, Zhi Li, Jiayue Hu, Chunyang Zhai, Mingshan Zhu. Modulating oxygen vacancies in BiOI for enhanced piezo-photocatalytic synergistic degradation[J]. Chinese Chemical Letters, 2027, 38(1): 112884. doi: 10.1016/j.cclet.2026.112884 shu

Modulating oxygen vacancies in BiOI for enhanced piezo-photocatalytic synergistic degradation

English

  • Solar-driven photocatalytic degradation of organic pollutants offers an economically attractive and environmentally sustainable strategy for advanced oxidation processes [1]. This technology is based on redox reactions, which are initiated by photo-excitation semiconductors generating electron-hole pairs, producing highly oxidizing substances, thereby effectively decomposing organic pollutants [2-5]. Notable advantages are mild operating conditions, high oxidation capacity, and minimal formation of toxic by-products [6-8]. The pervasive bulk-phase recombination of photogenerated charge carriers, however, continues to impede broader implementation, presenting an overarching challenge to reaction efficiency [9-11]. Piezoelectric catalysis is a catalytic process wherein a piezopotential is generated in non-centrosymmetric materials upon the application of mechanical stress [12], thereby driving photoinduced charge separation and accelerating redox reactions [13,14]. The synergistic coupling of light and mechanical energy can substantially enhance piezo-photocatalytic activity [15], holding great promise for a wide range of advanced applications. Nevertheless, most strategies focus predominantly on suppressing surface recombination, paying inadequate attention to bulk recombination mediated by defect trapping [16]. Thus, developing new approaches to effectively inhibit bulk recombination is essential for enhancing photocatalytic performance and advancing real-world applications in water treatment and environmental remediation [17].

    Defect engineering has emerged as a promising pathway to address bulk charge recombination [18]. By deliberately introducing vacancies [19], interstitial atoms [20], or substitutional dopants into the crystal lattice [21], this methodology enables precise modulation of the electronic and band structure characteristics in semiconductor photocatalysts. Such modifications not only improve visible-light absorption but also significantly suppress non-radiative bulk recombination [22]. Defect sites serve as effective electron trapping centers, thereby enhancing the longevity of photogenerated charge carriers [23]. In addition, a favorable density of defects is capable of inducing localized internal electric fields, driving the preferential migration and spatial partitioning of charges-a key factor in achieving efficient charge separation [24], thereby enhancing overall piezocatalytic efficiency [25,26]. Various defect types, like anion vacancies [27], cation vacancies [28], and doping-induced defects, have recently demonstrated considerable potential in modulating bulk recombination across different photocatalytic materials. For example, Li et al. synthesized few-layer Bi2O2(OH)NO3 nanosheets with tunable oxygen vacancies and explored their piezocatalytic performance, achieving a 5-fold enhancement in H2O2 yield via dual-channel 2e- ORR and 2e- WOR reactions from pure water and air [29]. In addition, Kong et al. developed Bi2WO6 nanosheets with surface OVs and integrated them with BiOI, achieving enhanced surface-active site regulation and charge separation in CO2 photoreduction [30]. Collectively, these studies underscore the versatility of defect engineering in suppressing bulk recombination and optimizing charge separation, offering a robust material-design paradigm for overcoming recombination losses in photocatalysis [31-38].

    In this work, we designed BiOI photocatalysts enriched with OVs via a glycerol-assisted solvothermal method. Glycerol functioned as both a solvent and a mild reductant, promoting selective cleavage of Bi-O bonds under controlled reaction conditions and enabling in situ formation of tunable surface OVs. Under combined visible-light irradiation and ultrasonic excitation, the optimized BiOI-OVs-1 sample delivered outstanding tetracycline (TC) degradation performance, achieving 89.1% removal within 20 min. Upon ultrasonic excitation, BiOI-OVs exhibited piezoelectric-induced band bending: The conduction band (CB) edge shifted upward, enhancing e- reduction ability and promoting •O2- formation from O2. Valence band (VB) edge shifted downward, strengthening the oxidizing power of holes (h+). The synergistic action of these highly oxidizing species enabled efficient TC degradation. Degradation tests confirmed that BiOI-OVs-1 exhibits significantly enhanced oxidative performance under piezo-photocatalytic coupling compared to pristine BiOI, retaining about 80% efficiency after five successive cycles. Moreover, the catalyst maintained over 70% degradation efficiency under a broad spectrum of pH conditions, in the presence of competing anions, and in diverse real water samples, demonstrating strong environmental adaptability and practical potential. This work systematically elucidates the role of oxygen vacancy concentration in enhancing the catalytic behavior of advanced oxidation catalysts and provides a practical materials design strategy for efficient treatment of antibiotic-contaminated wastewater.

    Detailed information on the chemicals, sample synthesis procedures, additional experimental and characterization methods, as well as degradation testing protocols is provided in Supporting information.

    In addition, the nomenclature for the control samples is summarized as follows: The time-series samples (denoted as BiOI-OVs-x, where x represents the reaction time) were synthesized at 180 ℃ for different durations (0.5, 1, 2, 6, and 18 h). The temperature-series samples (labeled as BiOI-OVs-T, where T denotes the reaction temperature) were prepared at different temperatures (140, 180, and 220 ℃) for 1 h (Fig. S1 in Supporting information).

    To investigate the effect of reaction time on the crystal structure of the samples, we performed characterizations on the BiOI-OVs samples synthesized at 180 ℃ with different reaction time. Fig. 1a shows the X-ray diffraction (XRD) patterns of the as-prepared samples. All samples exhibit distinct diffraction peaks at 29.6° and 31.6°, which correspond to the (102) and (110) crystal planes of the tetragonal phase of BiOI (JCPDS 10–0445), respectively [39]. Obviously, when the reaction time reached 6 h, a new diffraction peak of zero-valent bismuth (Bi0) appeared at 27.2°, suggesting that the formation of metallic bismuth [40]. Furthermore, as the reaction time increases, the diffraction intensity of the BiOI-OVs samples on the (110) plane significantly enhance. This can be attributed to the selective coordination between the trihydroxy functional groups in glycerol molecules and Bi3+ ions, which induces anisotropic crystal growth along the (110) direction [41].

    Figure 1

    Figure 1.  (a) XRD patterns of the samples at 180 ℃ with different reaction time. High-resolution XPS spectra of the samples for (b) Bi 4f, and (c) O 1s. (d) The ratio of peak areas of defect and Bi-O for BiOI samples in the O 1s spectrum. The SEM images of the samples at 180 ℃ with different reaction time (e) 0.5 h, (f) 1 h, (g) 2 h, (h) 18 h.

    The elemental composition and surface chemical states of the BiOI-OVs samples were characterized using X-ray photoelectron spectroscopy (XPS). The high-resolution Bi 4f spectrum (Fig. 1b) shows spin-orbit doublet peaks for Bi 4f7/2 and Bi 4f5/2 at 159.4 and 164.7 eV, respectively. Additionally, satellite peaks attributed to metallic bismuth (Bi0) are observed at 157.5 and 163.1 eV, and the peak area of the metallic bismuth (Bi0) gradually increases with reaction time [42]. In the O 1s XPS spectrum (Fig. 1c), the peak at 530.2 eV is attributed to Bi-O bonds within the (Bi2O2)2+ slabs of BiOI, that at 531.1 eV corresponds to oxygen species at defect sites with low oxygen coordination, and that at 533.2 eV corresponds to surface-adsorbed oxygen species. The oxygen species associated with defect sites exhibit a characteristic shift in binding energy relative to lattice oxygen, attributable to the modified local electronic environment induced by adjacent OVs, and the intensity of this defect-related peak shows a positive correlation with the concentration of OVs in the BiOI lattice [43]. A marked enhancement in the vacancy peak intensity is observed in BiOI-OVs-18 compared to BiOI-OVs-0.5, which is attributed to its substantially greater oxygen vacancy concentration. As demonstrated in Fig. 1d, the peak area corresponding to defects and its ratio to the Bi-O peak area increase significantly with extended reaction time, further confirming the oxygen vacancy-induced metallic bismuth generation. In the I 3d spectrum (Fig. S2 in Supporting information), peaks at binding energies of 619.4 and 630.9 eV correspond to I 3d5/2 and I 3d3/2, respectively, indicating the presence of iodine in the stable I- oxidation state [44].

    These XPS results suggest that oxygen vacancies not only change the surface chemical state of BiOI, but also affect the local coordination environment around Bi centers. The removal of lattice oxygen disrupts the local Bi-O bonding network and makes the coordination structure around nearby Bi atoms less complete [45]. As a result, partially under-coordinated Bi sites may be generated on the surface. These sites are expected to show higher surface reactivity and to be more favorable for the adsorption and activation of small molecules, especially dissolved O2. Therefore, oxygen vacancies contribute not only to charge separation, but also to interfacial reaction activation during the piezo-photocatalytic process.

    To investigate the effect of reaction time on the morphology of BiOI-OVs, scanning electron microscopy (SEM) images were acquired for samples synthesized at 180 ℃ for different durations (Figs. 1e-h). BiOI-OVs exhibits a flower-like architecture formed in the glycerol solution, with thicknesses ranging from 3 nm to 12 nm, confirming that glycerol-assisted synthesis effectively yields ultrathin BiOI-OVs nanosheets [46]. As the reaction time increases, BiOI-OVs particles grow larger and the nanosheets thicken. It suggests that extended reaction time provides higher atomic migration energy, accelerating the diffusion of precursor ions (Bi3+, I-), promoting directional crystal growth along the (001) planes, and ultimately leading to larger-sized crystals. However, larger particle sizes result in a decreased specific surface area, potentially reducing active sites of catalysts [47].

    Fig. 2 depicts the influence of different reaction temperatures on the catalyst structure and composition (reaction time fixed at 1 h), with conclusions similar to those from varying reaction time. As shown in Fig. 2a, the peak area of metallic bismuth (Bi0) increases progressively with rising reaction temperature. Fig. 2b also shows a gradual rise in the XPS peak area of metallic bismuth (Bi0). Fig. 2c demonstrates a corresponding increase in the relative concentration of OVs. As shown in Fig. 2d, the ratio of defect to Bi-O increases with the reaction temperature. And in the I 3d spectrum (Fig. S3 in Supporting information), iodine in the stable I-oxidation state. Correspondingly, SEM images in Figs. 2e-g reveal that higher reaction temperatures lead to increased BiOI-OVs particle size and nanosheet thickening. Enhanced thermal disturbance at elevated temperatures increases the concentration of bulk OVs, thereby promoting the escape of lattice oxygen. Simultaneously, larger crystals exhibit more active sites, which may enrich highly active surface OVs.

    Figure 2

    Figure 2.  (a) XRD patterns of the samples at 1 h with different reaction temperatures. High-resolution XPS spectra of the samples for (b) Bi 4f, and (c) O 1s. (d) The ratio of peak areas of defect and Bi-O for samples. The SEM images of the samples at 1 h with different reaction temperature (e) 180 ℃, (f) 140 ℃, (g) 220 ℃.

    The microstructure and crystal lattice of BiOI-OVs-1 were characterized by transmission electron microscopy (TEM) to support the study of its surface OVs. As shown in Fig. 3a, the microstructure is characterized by a flower-like morphology constituted of randomly oriented flakes, an observation corroborated by the corresponding SEM images. High-resolution TEM (HRTEM) images (Figs. 3b and c) reveal lattice spacings of 0.282 and 0.301 nm, corresponding to the (110) and (102) crystal planes of BiOI, respectively [48,49]. Furthermore, a series of interrupted lattice fringes are observable in Fig. 3d, indicating the presence of OVs in the BiOI-OVs-1 sample. Figs. 3e-h display the elemental distribution maps (mapping) of BiOI-OVs-1, clearly showing uniform distribution of Bi, O and I elements throughout the sample. Furthermore, energy-dispersive X-ray spectroscopy (EDS) data presented in Fig. 3i validate the presence of the constituent elements within the BiOI material.

    Figure 3

    Figure 3.  (a, b) TEM images of BiOI-OVs-1. (c, d) HRTEM images of BiOI-OVs-1. (e-h) Mapping images of Bi, O and I element of BiOI-OVs-1. (i) EDS of BiOI-OVs-1.

    To further verify the existence of OVs, Raman spectra were collected in the range of 50–200 cm−1 at room temperature. As shown in Fig. 4a and b, all samples show characteristic peaks near 92 and 144 cm−1, assigned to the Bi-I stretching vibrations of the A1g and Eg modes, respectively [50]. The peak intensity of the Eg mode is significantly lower than that of A1g, indicating weakened in-plane vibration due to reduced oxygen content caused by OVs. Meanwhile, the stronger A1g peak suggests decreased central atomic symmetry induced by OVs, leading to a tilted built-in electric field and thereby enhanced piezoelectric performance. Additionally, a deconvoluted peak corresponding to OVs is observed near 110 cm−1 [51]. As the reaction time and temperature increase, the peak area ratio of OVs to A1g gradually increases, demonstrating that the concentration of OVs can be effectively regulated by adjusting external reaction conditions.

    Figure 4

    Figure 4.  (a, b) Raman spectra and (c) EPR spectra of the BiOI-OVs samples.

    To obtain direct evidence of the presence of OVs in the samples, electron spin resonance (EPR) tests were conducted. As shown in Fig. 4c, all samples exhibit distinct EPR signals at g = 2.002, thereby confirming the existence of OVs [52]. Among them, BiOI-OVs-18 shows the strongest signal response, while BiOI-OVs-140 exhibits the weakest. The EPR signal intensity increases with longer reaction time and higher preparation temperature, indicating that both parameters promote the formation of OVs.

    The degradation of TC in aqueous solution was used to systematically evaluate the piezo-photocatalytic performance of the synthesized materials. As illustrated in Fig. 5a, the degradation efficiencies achieved by the individual photocatalytic and piezocatalytic systems within 20 min were 61.1% and 37.7%, respectively, in the presence of BiOI-OVs. In contrast, the piezo-photocatalytic system exhibited a significant synergistic effect, resulting in a notably higher degradation efficiency of 89.2%, surpassing the performance of each standalone system. In Table S1 (Supporting information), compared with recently reported BiOI-based photocatalysts, the BiOI-OVs-1 developed in this study demonstrates comparable or better catalytic efficiency in degrading pollutants. Meanwhile, the negligible TC removal in the blank system and the lower activity of BiOI (without OVs) exclude the interference of photolysis or sonolysis, and further confirm the crucial role of OVs in the enhanced piezo-photocatalytic performance. To assess the impact of OVs concentration on the catalytic degradation performance of TC, samples synthesized under different preparation durations and temperatures were subjected to piezo-photocatalytic experiments. As depicted in Fig. 5b, all BiOI-OVs samples, synthesized via the glycerol method, exhibited improved piezo-photocatalytic activity, suggesting that OVs aid in the effective separation of piezo-photogenerated carriers and the generation of ROS for degradation. Among these, the BiOI-OVs-1 sample (prepared with a 1 h reaction time) displayed optimal performance. Samples prepared for 2 and 6 h showed intermediate efficiency, while those synthesized for 0.5 and 18 h exhibited the lowest activity. This trend reveals that an insufficient reaction time (0.5 h) leads to inadequate OVs formation, whereas excessive reaction time (18 h) promotes the generation of surplus vacancies that act as carrier recombination centers, consequently compromising piezo-photocatalytic efficiency. Fig. 5c demonstrates that within the 140–180 ℃ temperature range, elevating the preparation temperature increased OVs concentration and markedly enhanced catalytic activity. However, beyond 180 ℃, excessive vacancies induced structural distortion at the material surface, resulting in diminished piezo-photocatalytic activity. In summary, the relationship between oxygen vacancy concentration and TC degradation efficiency follows a non-monotonic dependence, exhibiting a well-defined optimal window. Based on these experimental evidence, the optimal preparation parameters are identified as 180 ℃ and 1 h.

    Figure 5

    Figure 5.  (a) Tetracycline degradation curves for blank control, pure BiOI, and BiOI-OVs-1 under varied conditions. (b, c) Efficiency of TC degradation under ultrasonic vibration and visible light irradiation.

    Fig. 6a demonstrates the robust performance of BiOI-OVs-1 across a wide pH range (5–11), with TC degradation efficiency remaining above 77%. The marginal decline under alkaline conditions underscores its promising potential for practical wastewater treatment applications. BiOI-OVs-1 exhibited remarkable resistance to common anion interference, as evidenced in Fig. 6b. The degradation efficiency showed negligible deterioration in the presence of Cl-, CO32-, HCO3-, and SO42-, underscoring its applicability in water bodies with complex co-existing anions. Fig. 6c shows that TC degradation efficiency reached a saturation point at a dosage of 20 mg. A subsequent increase to 40 mg only yielded a minor improvement, justifying the selection of 20 mg as the optimal catalyst dosage for all subsequent tests. To assess its practical application potential, TC solution were prepared using five distinct water sources (distilled water, tap water, rainwater, seawater and river water) to simulate real wastewater treatment scenarios. As presented in Fig. 6d, BiOI-OVs-1 maintained high piezo-photocatalytic efficiency across different water matrices. The reduced degradation efficiency in seawater and river water is mainly attributed to the combined matrix effects of suspended particles, natural organic matter, and coexisting ions, (Figs. S5-S7 and Table S2 in Supporting information) which interfere with active sites, reactive species utilization, and interfacial mass transfer during the piezo-photocatalytic process [53]. To evaluate BiOI-OVs-1 stability, cycling experiments of piezo-photocatalysis were conducted over 100 min. The reusability of BiOI-OVs-1 was evaluated over five cycles. The catalyst exhibited remarkable stability, as evidenced in Fig. 6e, preserving a TC degradation rate above 80% over multiple operational cycles with minimal performance decay. The marginal decrease in catalytic activity after cycling mainly arises from the slight depletion of surface oxygen vacancies caused by the occupation and passivation of active sites by reaction intermediates during repeated reactions (Fig. S4 in Supporting information).

    Figure 6

    Figure 6.  BiOI-OVs-1 in piezo-photocatalysis: (a-c) Different pH, anions and catalyst dosage on the degradation efficiency of TC, (d) degradation efficiency of different water samples and (e) cycling experiment of TC degradation efficiency.

    To evaluate the influence of oxygen vacancy concentration on charge carrier mobility, the sample with the highest oxygen vacancy content (BiOI-OVs-18) and the sample exhibiting optimal degradation efficiency (BiOI-OVs-1) were selected for electrochemical characterization. The radius of the impedance arc in the EIS Nyquist plot serves as a quantitative indicator of charge transfer kinetics: A smaller diameter reflects facilitated carrier separation and mobility, while a larger one impedes this process. As shown in Fig. 7a, the EIS for BiOI-OVs-1 displays a smaller impedance arc radius compared to BiOI-OVs-18, indicating its lower charge transfer resistance. The superior steady-state piezo-photocurrent observed for BiOI-OVs-1 in Fig. 7b is indicative of efficient charge transfer, driven by a piezoelectric field derived from mechanical vibration. To elucidate the synergistic effect of the piezo-phototronic coupling, comparative measurements of piezo-photocurrent, photocurrent, and piezocurrent were conducted (Fig. S8 in Supporting information). The results demonstrate that the piezo-photocurrent substantially exceeds the sum of the individual photocurrent and piezocurrent, unequivocally confirming a synergistic enhancement beyond simple additive effects. This observation is consistent with the higher electron mobility, which implies enhanced separation efficiency of piezo-photogenerated electron-hole pairs and is generally associated with increased ROS generation capability. Fig. 7c displays the photoluminescence (PL) spectra of the samples excited at 415 nm. The significantly reduced PL intensity of BiOI-OVs-1 compared to BiOI-OVs-18 indicates that the moderate oxygen vacancy concentration in BiOI-OVs-1 effectively suppresses the recombination of photo-generated electron-hole pairs, leading to enhanced charge separation and migration efficiency [54].

    Figure 7

    Figure 7.  (a) Nyquist plot of electrochemical impedance spectroscopy (EIS). (b) Piezo-photocatalytic current density-time curves of BiOI-OVs-1 and BiOI-OVs-18. (c) PL spectra of BiOI-OVs-1 and BiOI-OVs-18. (d) Phase-voltage hysteresis loop and amplitude-voltage displacement curve of BiOI-OVs-1.

    The piezoelectric properties of the samples were directly characterized by piezoresponse force microscopy (PFM). As depicted in Fig. 7d, the amplitude-voltage butterfly loop and phase-voltage hysteresis loop of BiOI-OVs-1 were measured. Application of a bias voltage sweeping from −10.0 V to +10.0 V triggered localized hysteresis behavior, resulting in sustained deformation of the material surface. A significant shift in the phase angle was observed for BiOI-OVs-1. As the phase shift serves as an indicator of the material’s polarization under an external electric field, the marked phase angle deviation signifies distinct polarization reversal at the surface. The observed 180° phase-switching hysteresis loop confirms genuine piezoelectric response, distinguishing it from non-piezoelectric effects such as electrostriction. The results indicate that BiOI-OVs-1 is characterized by spontaneous polarization, which creates an inherent surface electric field and validates its significant piezoelectric nature [55].

    Band structure analysis is essential for elucidating the charge-carrier transport and redox potential in semiconductor piezo-photocatalysts. The Mott-Schottky plots of BiOI-OVs-1 (Fig. 8a) and BiOI-OVs-18 (Fig. 8b) at different frequencies exhibit positive slopes, characteristic of n-type semiconductors [56]. This result is consistent with the Hall effect measurement (Fig. 8c), in which BiOI-OVs-1 shows a negative Hall coefficient, confirming electrons as the dominant charge carriers (Table S3 in Supporting information). The flat-band potentials (Efb) of BiOI-OVs-1 and BiOI-OVs-18, determined from the X-axis intercepts of the Mott-Schottky plots, are −1.23 V and −1.12 V (vs. Ag/AgCl), respectively. Considering E(Ag/AgCl) ≈ +0.197 V (vs. NHE), the conduction band potentials (ECB) of BiOI-OVs-1 and BiOI-OVs-18 are calculated to be −1.03 V and −0.92 V (vs. NHE), respectively [57].

    Figure 8

    Figure 8.  Mott-Schottky curves of (a) BiOI-OVs-1 and (b) BiOI-OVs-18. (c) Hall measurement fitting curve of the BiOI-OVs-1. (d, e) UV–vis DRS and band gap of BiOI-OVs-1/BiOI-OVs-18. (f) Energy band structure diagram (pH 7.01).

    The optical absorption properties of the samples were characterized by diffuse reflectance spectroscopy (DRS). As shown in Fig. 8d, the absorption edges of BiOI-OVs-1 and BiOI-OVs-18 are identified at approximately 487.8 nm and 508.2 nm, respectively. The band gaps (Eg) were calculated using the equation Eg = 1240/λg (eV), yielding values of 2.59 eV for BiOI-OVs-1 and 2.44 eV for BiOI-OVs-18 (Fig. 8e). It suggests that the formation of more OVs slightly decreases the band gap of BiOI. The valence band potentials (EVB) were derived using the equation EVB = Eg + ECB, resulting in values of +1.56 V and +1.52 V (vs. NHE) for BiOI-OVs-1 and BiOI-OVs-18, respectively.

    The valence band X-ray photoelectron spectroscopy (VB-XPS, Fig. S9 in Supporting information) analysis measured the energy differences between the Fermi level (EF) and the valence band maximum as 1.31 eV and 1.27 eV for BiOI-OVs-1 and BiOI-OVs-18, respectively. For n-type semiconductors, Efb is equivalent to the flat-band potential. The valence band potential relative to the normal hydrogen electrode, EVB,NHE was calculated using the equation: EVB,NHE = φ + EVB,XPS-4.44 [58], where φ is the instrument work function (4.69 eV). BiOI-OVs-1 and BiOI-OVs-18 exhibited calculated EVB, NHE values of +1.56 V and +1.52 V, aligning well with the optically derived.

    Based on the determined conduction band (CB) and valence band (VB) positions of the as-synthesized BiOI-OVs, the corresponding energy band structures were constructed. As illustrated in Fig. 8f, BiOI-OVs-18 exhibits a narrower bandgap in pH 7.01, which validates the phenomenon that a higher concentration of OVs can lead to bandgap narrowing [59]. However, this narrowing is accompanied by a downshift of the conduction band minimum (CBM), resulting in a weakened reduction capability of the material. Furthermore, the introduced defects serve as recombination centers, hindering charge separation and migration, thereby compromising the overall catalytic efficiency. It explains the detrimental effect of excessive OVs concentration and highlights why BiOI-OVs-1, with a moderate OVs level, exhibits superior piezo-photocatalytic performance. Additionally, the CB potential of BiOI-OVs-1 is −1.03 eV vs. NHE, which is sufficiently negative to reduce O2 to •O2- (O2/•O2- = −0.33 V vs. NHE). It confirms the feasibility of •O2- generation, a conclusion further supported by the subsequent radical trapping experiments.

    The active species generated by BiOI-OVs-1 were primarily investigated through radical quenching experiments. The quenchers disodium ethylenediaminetetraacetate (EDTA-2Na), tert-butanol (TBA), p-benzoquinone (BQ), silver nitrate (AgNO3), and furfuryl alcohol (FFA) were employed to trap holes (h+), hydroxyl radicals (•OH), superoxide radicals (•O2-), electrons (e-) and singlet oxygen (1O2), respectively. As shown in Fig. 9a and b, after the addition of EDTA-2Na, BQ and AgNO3, the degradation efficiency of TC decreased significantly to 21.3%, 12.1% and 16.2%, respectively. In contrast, the introduction of TBA and FFA resulted in only a slight reduction in degradation efficiency, to 87.1% and 79.0%, respectively. These results indicate that •O2- and h+ are the predominant active species in the TC degradation process by BiOI-OVs-1, followed by e-. To detect •O2-, EPR spin-trapping experiments were performed using DMPO as the trapping agent. As illustrated in Fig. 9c, no significant EPR signal was observed in the dark. However, a distinct 1:1:1:1 quartet characteristic of DMPO-•O2- adducts emerged under the piezo-photocatalytic system, with a calculated hyperfine coupling constant of 13.3 G (1.33 mT), demonstrating that BiOI-OVs-1 can generate •O2- radicals under light irradiation and ultrasound. To further confirm the presence of active species, EPR measurements were carried out using TEMPO as a spin trapping agent. As seen in Fig. 9d, the TEMPO probe exhibited a typical 1:1:1 triplet EPR signal, whose intensity decreased significantly under the piezo-photocatalytic system due to the formation of TEMPO-h+ adducts via the reaction of TEMPO with photogenerated holes (h+). The above results confirm that •O2- and h+ are the key active species, which synergistically facilitate the piezo-photocatalytic degradation reaction.

    Figure 9

    Figure 9.  BiOI-OVs-1 in piezo-photocatalysis: (a, b) TC degradation with different scavengers. (c, d) EPR spectra in the presence of DMPO-•O2- and TEMPO-h+.

    Based on the aforementioned results, the formation mechanism of surface OVs and the enhanced oxidative performance of BiOI-OVs-1 can be elucidated as follows. Glycerol in the solvent acts as a mild reductant, selectively cleaving the relatively weak Bi-O bonds in BiOI and resulting in the in-situ formation of surface OVs. These OVs function as efficient electron trapping sites, thereby mitigating the bulk recombination of charge carriers. In the piezo-photocatalytic system, BiOI is photoexcited under visible light to generate electrons (e-) and holes (h+) (Eq. 1) [60]. Concurrently, mechanical strain induced by ultrasonic vibration leads to piezoelectric polarization, causing band bending: an upward shift of the conduction band (CB) enhances the reduction capability of e-, while a downward shift of the valence band (VB) strengthens the oxidation power of h+ [61]. Subsequently, the adsorbed O2 molecules capture electrons to form superoxide radicals (•O2-) (Eq. 2) [62].In addition, the OV-induced change in the local coordination environment around Bi centers may also facilitate interfacial O2 activation. Ultimately, organic compounds (e.g., TC) are degraded into CO2 and H2O under the synergistic oxidation of •O2- and h+ (Eq. 3). The primary reaction pathways involved in the piezo-photocatalysis of BiOI-OVs are summarized below:

    $ \mathrm{BiOI}+\mathrm{Vis}+\mathrm{Us} \rightarrow \mathrm{BiOI}\left(\mathrm{~h}^{+}+\mathrm{e}^{-}\right) $

    (1)

    $ \mathrm{O}_2+e^{-} \rightarrow \mathrm{^{\cdot}O}_2^{-} $

    (2)

    $ \mathrm{h}^{+} / \mathrm{^{\cdot}O}_2^{-}+\mathrm{TC} \rightarrow \mathrm{CO}_2+\mathrm{H}_2 \mathrm{O} $

    (3)

    Based on this work, oxygen vacancy-enriched BiOI nanosheets were successfully prepared through a glycerol-assisted solvothermal method. By controlling synthesis parameters, the oxygen vacancy concentration could be systematically tuned, demonstrating a clear optimal window for maximizing piezo-photocatalytic activity. Both insufficient and excessive OVs were found to diminish degradation performance. It revealed that OVs serve as effective electron traps, simultaneously capturing photogenerated and piezoelectric-induced electrons. The optimal sample (BiOI-OVs-1) achieved a TC degradation rate of 89.2% within 20 min. It significantly suppresses bulk charge recombination and promotes reactive oxygen species generation. •O2- and h+ were identified as the primary active species driving the degradation process. The synergistic coupling between the piezoelectric field and OVs enhances charge carrier separation and migration, as confirmed by comprehensive characterization. The optimized catalyst exhibited excellent cycling stability and maintained high degradation efficiency across various pH conditions, competing anions, and real water matrices. This work provides both a practical defect-engineering strategy for designing efficient piezo-photocatalysts and fundamental insights into the critical role of OVs in charge separation processes, demonstrating significant potential for environmental remediation applications Fig. 10.

    Figure 10

    Figure 10.  The possible piezo-photocatalytic mechanism of BiOI-OVs.

    Wenbo Fu: Writing – original draft, Investigation, Data curation. Yao Zhang: Formal analysis, Data curation. Yong Jiang: Investigation, Data curation. Wenfeng Lin: Formal analysis, Data curation. Zhi Li: Writing – review & editing, Supervision, Funding acquisition. Jiayue Hu: Writing – review & editing, Supervision. Chunyang Zhai: Writing – review & editing, Supervision, Project administration, Funding acquisition. Mingshan Zhu: Supervision, Conceptualization.

    The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

    This study was financially supported by the National Natural Science Foundation of China (No. 22506055), the National Natural Science Foundation of China (No. 22406002) and the Science and Technological Program of Ningbo (No. 2024S083) and the China Postdoctoral Science Foundation (2026T190333).

    Supplementary material associated with this article can be found, in the online version, at doi:10.1016/j.cclet.2026.112884.


    1. [1]

      Q. Guo, J.D. Zhang, J. Li, X. Feng, Nano-Micro Lett. 18 (2025) 18:49.

    2. [2]

      S. He, Y. Chen, J. Fang, Y. Liu, Z. Lin, Chem. Soc. Rev. 54 (2025) 2154–2187. doi: 10.1039/d4cs00317a

    3. [3]

      J. Wang, W. Liao, Y. Tan, et al., Chem. Soc. Rev. 54 (2025) 6553–6596. doi: 10.1039/d5cs00512d

    4. [4]

      J. Wang, S. Shen, X. Li, J. Li, F. Dong, Chem. Rev. 125 (2025) 7811–7917. doi: 10.1021/acs.chemrev.5c00074

    5. [5]

      Y. Pan, W. Liang, Z. Wang, et al., Interd. Mater. 3 (2024) 935–945. doi: 10.1002/idm2.12203

    6. [6]

      Q. Cai, Y. Chen, L. Lu, et al., Appl. Catal. B: Environ. 382 (2026) 125991. doi: 10.1016/j.apcatb.2025.125991

    7. [7]

      R. Wang, J. Hou, J. He, et al., Chin. Chem. Lett. 37 (2026) 112143. doi: 10.1016/j.cclet.2025.112143

    8. [8]

      B. Wang, H. Chen, W. Zhang, et al., Adv. Mater. 36 (2024) 2312676. doi: 10.1002/adma.202312676

    9. [9]

      Z. Liu, Y. Ma, J. Li, et al., Adv. Mater. 38 (2026) e12150. doi: 10.1002/adma.202512150

    10. [10]

      Y. Gao, Z. Liu, H. Lu, et al., Adv. Energy Mater. 15 (2025) 2403752. doi: 10.1002/aenm.202403752

    11. [11]

      B. Wang, H. Chen, F. Huang, et al., Appl. Catal. B: Environ. 374 (2025) 125394. doi: 10.1016/j.apcatb.2025.125394

    12. [12]

      Y. Zhu, H. Chen, L. Wang, et al., Chin. Chem. Lett. 35 (2024) 108884. doi: 10.1016/j.cclet.2023.108884

    13. [13]

      C. Wang, S. Tu, F. Chen, T. Ma, H. Huang, Adv. Mater. 37 (2025) 2505592. doi: 10.1002/adma.202505592

    14. [14]

      C. Hu, J. Hu, Z. Zhu, et al., Angew. Chem. Int. Ed. 61 (2022) e202212397. doi: 10.1002/anie.202212397

    15. [15]

      Z. Chen, Y. Yan, J. Luo, et al., Chin. Chem. Lett. 36 (2025) 111302. doi: 10.1016/j.cclet.2025.111302

    16. [16]

      H. Wu, R. Liang, G. Song, et al., Chin. Chem. Lett. 35 (2024) 109131. doi: 10.1016/j.cclet.2023.109131

    17. [17]

      Y. Guo, Q. Guan, X. Li, et al., Energ. Environ. Sci. 18 (2025) 5539–5551. doi: 10.1039/d5ee00605h

    18. [18]

      S. Bai, N. Zhang, C. Gao, Y. Xiong, Nano Energy 53 (2018) 296–336. doi: 10.1016/j.nanoen.2018.08.058

    19. [19]

      Z. Yang, M. Yuan, B. Liu, et al., Adv. Mater. 37 (2025) 2412069. doi: 10.1002/adma.202412069

    20. [20]

      Q. Xu, L. Wang, X. Sheng, et al., Appl. Catal. B: Environ. 338 (2023) 123058. doi: 10.1016/j.apcatb.2023.123058

    21. [21]

      Q.L. Ma, J. Wei, Z. Lin, et al., Appl. Catal. B: Environ. 378 (2025) 125547. doi: 10.1016/j.apcatb.2025.125547

    22. [22]

      F. Chen, Z. Liu, R. Miao, et al., Chem. Eng. J. 506 (2025) 159996. doi: 10.1016/j.cej.2025.159996

    23. [23]

      H. Ali, Z. Ajmal, A.Y.A. Alzahrani, et al., InfoMat 7 (2025) e70040. doi: 10.1002/inf2.70040

    24. [24]

      E. Cui, Y. Lu, Z. Li, et al., Chin. Chem. Lett. 36 (2025) 110288. doi: 10.1016/j.cclet.2024.110288

    25. [25]

      M. Zhang, W. Guo, Y. Chen, et al., Chin. Chem. Lett. 34 (2023) 108229. doi: 10.1016/j.cclet.2023.108229

    26. [26]

      Z. Li, S. Lan, M. Zhu, Environ. Sci. Ecotech. 18 (2024) 100329.

    27. [27]

      Q. Zhong, Y. Sun, S.G. Yang, et al., Angew. Chem. Int. Ed. 64 (2025) e202507265. doi: 10.1002/anie.202507265

    28. [28]

      W. Ding, Y. Hai, X. Li, et al., J. Environ. Chem. Eng. 12 (2024) 113141. doi: 10.1016/j.jece.2024.113141

    29. [29]

      Y. Li, X. Zhang, T. Li, et al., Chin. J. Catal. 75 (2025) 105–114. doi: 10.1007/s42243-024-01270-x

    30. [30]

      X.Y. Kong, W.Q. Lee, A.R. Mohamed, S.P. Chai, Chem. Eng. J. 372 (2019) 1183–1193. doi: 10.1016/j.cej.2019.05.001

    31. [31]

      Q. Wang, Z. Liu, D. Liu, et al., Appl. Catal. B: Environ. 236 (2018) 222–232. doi: 10.1016/j.apcatb.2018.05.029

    32. [32]

      X. Cao, X. Liu, Y. Wang, et al., Chin. Chem. Lett. 37 (2026) 112112. doi: 10.1016/j.cclet.2025.112112

    33. [33]

      C. Li, J. He, T. Cai, et al., Chin. J. Catal. 74 (2025) 130–143. doi: 10.1016/S1872-2067(25)64649-3

    34. [34]

      K. Wang, X. Guo, C. Han, et al., ACS Nano 19 (2025) 3818–3829. doi: 10.1021/acsnano.4c14974

    35. [35]

      X. Li, K. Li, D. Ding, et al., Sep. Purif. Technol. 309 (2023) 123054. doi: 10.1016/j.seppur.2022.123054

    36. [36]

      C. Li, W. Liu, X. Chen, et al., Chin. Chem. Lett. 35 (2024) 109652. doi: 10.1016/j.cclet.2024.109652

    37. [37]

      W. Wang, F. Hu, B. Li, et al., Appl. Catal. B: Environ. 367 (2025) 125103. doi: 10.1088/1361-6463/adaa84

    38. [38]

      H. Bian, X. Yuan, N. Zhang, et al., Chin. Chem. Lett. 36 (2025) 111034. doi: 10.1016/j.cclet.2025.111034

    39. [39]

      R.Q. Miao, Z.H. He, B.T. Wu, et al., Chem. Eng. J. 481 (2024) 148293. doi: 10.1016/j.cej.2023.148293

    40. [40]

      D. Song, M. Li, F. Yang, et al., Chin. Chem. Lett. 35 (2024) 108591. doi: 10.1016/j.cclet.2023.108591

    41. [41]

      M. Arumugam, Y. Yu, H.J. Jung, et al., Environ. Res. 197 (2021) 111080. doi: 10.1016/j.envres.2021.111080

    42. [42]

      L. Chen, C. Li, Y. Zhao, et al., Chem. Eng. J. 425 (2021) 131599. doi: 10.1016/j.cej.2021.131599

    43. [43]

      J. Huang, X. Zheng, Y. Liu, et al., J. Hazard. Mater. 412 (2021) 125147. doi: 10.1016/j.jhazmat.2021.125147

    44. [44]

      W. Qu, C. Chen, Z. Tang, et al., Appl. Catal. B: Environ. 304 (2022) 120970. doi: 10.1016/j.apcatb.2021.120970

    45. [45]

      D. Ma, H. Yi, S. Yang, et al., Chem. Eng. J. 529 (2026) 172583. doi: 10.1016/j.cej.2026.172583

    46. [46]

      P. Gao, Z. Zhang, L. Feng, et al., Chem. Eng. J. 426 (2021) 130764. doi: 10.1016/j.cej.2021.130764

    47. [47]

      A. Hussain, J. Hou, M. Tahir, et al., Catal. Rev. 66 (2024) 119–173. doi: 10.1080/01614940.2022.2041836

    48. [48]

      L. Ye, X. Jin, X. Ji, et al., Chem. Eng. J. 291 (2016) 39–46. doi: 10.1016/j.cej.2016.01.032

    49. [49]

      J. Sun, J. Wen, G. Wu, et al., Adv. Funct. Mater. 30 (2020) 2004108. doi: 10.1002/adfm.202004108

    50. [50]

      L. Zeng, F. Zhe, Y. Wang, et al., J. Colloid Interf. Sci. 539 (2019) 563–574. doi: 10.1016/j.jcis.2018.12.101

    51. [51]

      E.M. Kira, M.M. Elsenety, A.B.A.A. Nassr, T.S. Eldin Kassem, M.M. Emara, Mater. Today Chem. 47 (2025) 102842. doi: 10.1016/j.mtchem.2025.102842

    52. [52]

      J. Yan, J. Zhang, Y. Wang, et al., Sep. Purif. Technol. 361 (2025) 131486. doi: 10.1016/j.seppur.2025.131486

    53. [53]

      Y. Mo, J. Wu, W. Liu, et al., Adv. Powder Mater. 4 (2025) 100307. doi: 10.1016/j.apmate.2025.100307

    54. [54]

      Q. Li, Y. Li, B. Li, et al., Appl. Catal. B: Environ. 289 (2021) 120041. doi: 10.1016/j.apcatb.2021.120041

    55. [55]

      Y. Li, X. Zhang, R. Sha, et al., Chem. Eng. J. 480 (2024) 147976. doi: 10.1016/j.cej.2023.147976

    56. [56]

      H. Zhong, X. Ji, C. Yang, et al., ACS Catal. 14 (2024) 6272–6291. doi: 10.1021/acscatal.4c00121

    57. [57]

      H. Zhou, J. Cao, Y. Ji, M. Xia, W. Yao, Small 20 (2024) 2402679. doi: 10.1002/smll.202402679

    58. [58]

      X. Li, B. Kang, F. Dong, et al., Nano Energy 81 (2021) 105671. doi: 10.1016/j.nanoen.2020.105671

    59. [59]

      Q. Xu, J. Jiang, X. Sheng, et al., Inorg. Chem. Front. 10 (2023) 2939–2950. doi: 10.1039/d3qi00405h

    60. [60]

      Z. Yin, T. Liu, Y. Yang, et al., J. Alloy Compd. 1027 (2025) 180566. doi: 10.1016/j.jallcom.2025.180566

    61. [61]

      H. Fei, G. Liu, J. Wu, et al., Chem. Eng. J. 519 (2025) 165536. doi: 10.1016/j.cej.2025.165536

    62. [62]

      Y. Yang, J. Sun, J. Liu, X. Chang, Q. Yan, J. Environ. Manag. 392 (2025) 126779. doi: 10.1016/j.jenvman.2025.126779

  • Figure 1  (a) XRD patterns of the samples at 180 ℃ with different reaction time. High-resolution XPS spectra of the samples for (b) Bi 4f, and (c) O 1s. (d) The ratio of peak areas of defect and Bi-O for BiOI samples in the O 1s spectrum. The SEM images of the samples at 180 ℃ with different reaction time (e) 0.5 h, (f) 1 h, (g) 2 h, (h) 18 h.

    Figure 2  (a) XRD patterns of the samples at 1 h with different reaction temperatures. High-resolution XPS spectra of the samples for (b) Bi 4f, and (c) O 1s. (d) The ratio of peak areas of defect and Bi-O for samples. The SEM images of the samples at 1 h with different reaction temperature (e) 180 ℃, (f) 140 ℃, (g) 220 ℃.

    Figure 3  (a, b) TEM images of BiOI-OVs-1. (c, d) HRTEM images of BiOI-OVs-1. (e-h) Mapping images of Bi, O and I element of BiOI-OVs-1. (i) EDS of BiOI-OVs-1.

    Figure 4  (a, b) Raman spectra and (c) EPR spectra of the BiOI-OVs samples.

    Figure 5  (a) Tetracycline degradation curves for blank control, pure BiOI, and BiOI-OVs-1 under varied conditions. (b, c) Efficiency of TC degradation under ultrasonic vibration and visible light irradiation.

    Figure 6  BiOI-OVs-1 in piezo-photocatalysis: (a-c) Different pH, anions and catalyst dosage on the degradation efficiency of TC, (d) degradation efficiency of different water samples and (e) cycling experiment of TC degradation efficiency.

    Figure 7  (a) Nyquist plot of electrochemical impedance spectroscopy (EIS). (b) Piezo-photocatalytic current density-time curves of BiOI-OVs-1 and BiOI-OVs-18. (c) PL spectra of BiOI-OVs-1 and BiOI-OVs-18. (d) Phase-voltage hysteresis loop and amplitude-voltage displacement curve of BiOI-OVs-1.

    Figure 8  Mott-Schottky curves of (a) BiOI-OVs-1 and (b) BiOI-OVs-18. (c) Hall measurement fitting curve of the BiOI-OVs-1. (d, e) UV–vis DRS and band gap of BiOI-OVs-1/BiOI-OVs-18. (f) Energy band structure diagram (pH 7.01).

    Figure 9  BiOI-OVs-1 in piezo-photocatalysis: (a, b) TC degradation with different scavengers. (c, d) EPR spectra in the presence of DMPO-•O2- and TEMPO-h+.

    Figure 10  The possible piezo-photocatalytic mechanism of BiOI-OVs.

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  133
  • HTML全文浏览量:  12
文章相关
  • 发布日期:  2027-01-12
  • 收稿日期:  2026-02-24
  • 接受日期:  2026-05-03
  • 修回日期:  2026-04-29
  • 网络出版日期:  2026-05-05
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章