Rapid Joule heating transforms asphalt into high-value porous carbon for enhanced capacitive energy storage

Zhipeng Wang ,  Zhengxun Ma ,  Jintao Huang ,  Shuhao Zhang ,  Jiangfeng Ni ,  Gaoyi Han ,  Sheng Zhu

Citation:  Zhipeng Wang, Zhengxun Ma, Jintao Huang, Shuhao Zhang, Jiangfeng Ni, Gaoyi Han, Sheng Zhu. Rapid Joule heating transforms asphalt into high-value porous carbon for enhanced capacitive energy storage[J]. Chinese Chemical Letters, 2027, 38(1): 112120. doi: 10.1016/j.cclet.2025.112120 shu

Rapid Joule heating transforms asphalt into high-value porous carbon for enhanced capacitive energy storage

English

  • Compared to batteries, supercapacitors (SCs) exhibit superior power density, extended cycle life, and rapid charge/discharge capabilities [1-5]. Among carbon-based SCs, electric double-layer capacitors (EDLCs) dominate the charge storage mechanism through electrostatic adsorption. Consequently, diverse carbon nanostructures have been engineered as electrode materials [6]. To enhance EDLC capacity, designing and synthesizing carbon materials with highly porous architectures is critical [7,8]. Such structures not only boost energy density but also improve ion transport kinetics [5,9]. While polymers, coal, biomass, and other feedstocks have been used to synthesize porous carbon, achieving optimized pore structures that improve capacitive energy storage performance remains challenging-a key focus of contemporary research [10].

    Asphalt offers distinct advantages as a carbon precursor for high-value carbon materials, including high carbon yield, low melting point, cost efficiency, and processability [11]. In order to control the structure of the products, asphalt usually is treated by concentrated sulfuric acid [12], concentrated nitric acid [13], hydrogen peroxide [14], and potassium permanganate [15] as oxidizing agents to obtain the water-soluble asphalt via introducing polarized groups, then the hydrophilic asphalt is thermally treated and activated to obtain the porous carbon. However, these processes may raise seriously environmental concerns [8,16-18]. Molten-salt method is considered to offer a green approach for constructing and manipulating carbon materials because it can provide a homogeneous liquid-phase reaction environment and allow operation at temperatures below the melting point of individual salts [19-22]. Nevertheless, traditional molten-salt processes suffer from prolonged durations and high energy consumption, underscoring the need for efficient alternatives. Therefore, there is an urgent need to develop a cost-effective molten-salt method for preparing high-performance porous carbon materials. The flash Joule heating technique has recently emerged as a promising solution [23-28]. Compared to conventional heating methods such as tubular and muffle furnaces, Joule heating offers significant advantages, including near-perfect energy conversion efficiency (~100%), extremely rapid heating and cooling rates (>103 K/s), and the ability to achieve transient high temperatures exceeding 1500 K. These properties make it particularly suitable for the ultrafast synthesis, structural modulation, and scalable production of nanomaterials. Combining molten salts with Joule heating enables instantaneous salt melting into microdroplets during ultrafast carbonization, concurrently achieving carbonization and activation [29]. However, to the best of acknowledge, such a rapid Joule heating has not been employed in the high-value transformation of asphalt.

    In this work, we develop a rapid Joule heating assisted by molten salt to transform asphalt into high-value porous carbon. A KCl/K2CO3 system serves as the reaction medium, transforming asphalt into porous carbon within 15 s. Compared to conventionally pyrolyzed carbon (PPC), the Joule-heated carbon (JPC) exhibits a unique nanostructure featuring well-defined nanosheets and an extensive micropore network. JPC demonstrates a higher specific surface area of 1017.5 m2/g vs. PPC’s 683 m2/g and a 20% increase in specific capacitance. SCs based on JPC further display superior electrochemical performance across alkaline, inorganic salt, and water-in-salt electrolytes, indicating enhanced active sites and accelerated ion transport.

    Fig. 1a illustrates the synthesis pathways for asphalt-derived porous carbon. Initially, KCl and K2CO3 were mixed uniformly with asphalt according to eutectic points. Following this step, three pathways were employed for the conversion of asphalt into porous carbon through the molten salt process: Conventional pyrolysis (Route 1), flash Joule heating (Route 2), and rapid Joule heating (Route 3). In Route 1, PPC synthesis involved 2-h pyrolysis at 700 ℃ (2.5 ℃/min heating rate) in a muffle furnace (Fig. 1b), gradually fused into a liquid phase during slow heating. For comparison, in Route 2 (Table S1 in Supporting information), the PPC sample further underwent an ultrafast Joule heating process at about 2800 ℃ with a heating rate of 2.8 × 104 ℃/s (Fig. 1c). In Route 3, JPC was produced via 8-s Joule heating of KCl/K2CO3/asphalt composite at 850 ℃, where binary KCl/K2CO3 salts instantaneously melt during rapid heating process (567 ℃/s), as shown in Fig. 1d. It is evident that, due to the short reaction time, the energy consumption of the Joule heating process in Route 2 (1 s) and Route 3 (8 s) is significantly lower than that in Route 1 (2 h), with synthesis efficiency markedly improved compared to Route 1.

    Figure 1

    Figure 1.  (a) Schematic illustration for fabrication routes of JPC, FPC, and PPC. (b) The curve of temperature over time in Route 1. (c) The curves of temperature and current over time in Route 2. (d) The curves of temperature and current over time in Route 3.

    The microstructures of porous carbon products were characterized by using scanning electron microscopy (SEM) and transmission electron microscopy (TEM) techniques. Unlike raw asphalt (bulk morphology, Fig. S1 in Supporting information), all PPC samples obtained at different annealing temperatures exhibit porous sheet-like structures (Fig. 2a and Fig. S2 in Supporting information). This morphology likely results from prolonged muffle furnace processing, where molten salt aggregation forms large droplets that template polydisperse pores [30]. Similar morphology is observed for FPC (Fig. 2b and Fig. S3 in Supporting information). JPC exhibits a relatively uniform porous architecture (Figs. 2c and d, Fig. S4 in Supporting information) with smooth surface, formed as the KCl/K2CO3 mixture rapidly melts into fine droplets during Joule heating. The fast Joule heating synergized molten-salt engineering prevents salt coalescence, yielding abundant macropores, mesopores and micropores visible on carbon sheets.

    Figure 2

    Figure 2.  SEM images of (a) PPC, (b) FPC, and (c) JPC. (d) TEM image of JPC. (e) N2 adsorption-desorption isotherms of FPC, PPC, and JPC. (f) Pore size distribution curves of PPC, FPC, and JPC.

    Nitrogen adsorption isotherms and pore size distribution curves characterize the specific surface area and porosity of asphalt-derived porous carbons (Figs. 2e and f). All samples exhibit combined type Ⅰ/Ⅳ isotherms, indicative of abundant micropores and small mesopores [31,32]. The specific surface areas for JPC, PPC, and FPC are calculated to be about 1017.5, 971.0, and 884.5 m2/g, respectively, and the total pore volume is about 0.61 cm3/g in JPC, which is larger than that of PPC (0.56 cm3/g) and FPC (0.48 cm3/g) (Fig. S5 and Table S2 in Supporting information). These results can be linked to the ultrafast heating rate of Joule-heating assisted molten-salt method. The rapid kinetics promotes intense random motion and chemical activation among the molten-salt ions, which consequently facilitates the creation of a porous structure and a higher surface area. However, the instantaneous high-temperature flash Joule heating can enhance the graphitization of FPC, leading to relatively low surface area and pore volume. The micropore area to BET surface area ratio (Smicro/SBET) further elucidates the pore structure. The asphalt-derived porous carbons present high Smicro/SBET values over 70%, indicating that molten-salt treatment favors the development of a primarily microporous structure. The abundance of micropores provides numerous ion adsorption sites, while the mesopore network facilitates electrolyte transport. Collectively, these structural features are expected to enhance the electrochemical performance of asphalt-derived porous carbons [33].

    Raman spectroscopy further confirms the disordered structure of the asphalt-derived carbon materials (Fig. 3a, Figs. S6 and S7a in Supporting information). The D band (1340 cm−1) corresponds to structural defects and sp3-hybridized carbon atoms in graphitic lattices, while the G band (1580 cm−1) originates from the ordered graphitic domains. Typically, the intensity ratio of D and G bands (ID/IG) quantitatively reflects the defect density [34]. JPC exhibits the highest ID/IG ratio of 1.78, exceeding that of asphalt (1.21), PPC (1.58), and FPC (1.49), confirming its elevated structural disorder. X-ray diffraction (XRD) patterns (Fig. 3b and Fig. S8 in Supporting information) reveal two characteristic peaks for all materials, corresponding to the (002) and (100) planes of carbon. Notably, the (002) peak of JPC exhibits a distinct left shift and broadening compared to the other carbons, signifying an increased interlayer spacing (d002). Thus, rapid Joule heating significantly expands the interlayer spacing of asphalt-derived carbon materials, which is favorable for electrochemical energy storage [35].

    Figure 3

    Figure 3.  (a) Raman spectra of asphalt, JPC, FPC, and PPC samples. (b) XRD patterns of asphalt, JPC, FPC, and PPC samples. (c) FTIR spectra of asphalt, JPC, FPC, and PPC samples. XPS (d) survey spectra, (e) C 1s XPS spectra. (f) The sp3/sp2 hybrid carbon ratios of asphalt, JPC, FPC, and PPC samples.

    Fourier transform infrared (FTIR) spectroscopy reveals changes in functional groups between asphalt and the molten-salt-derived porous carbons (JPC, FPC, PPC) (Fig. 3c and Fig. S9 in Supporting information). All spectra display absorption peaks between 1000 cm−1 and 1500 cm−1, corresponding to C–H bending vibrations and/or aromatic ring structures characteristic of both asphalt and its derived carbons [36]. Weak peaks in the 2850–3000 cm−1 region, attributable to C–H stretching vibrations, indicate the retention of some C–H bonds in all materials [37]. Crucially, peaks in the 700–1000 cm−1 region, associated with C–H out-of-plane bending vibrations, disappear after annealing, indicating thermal decomposition or elimination of specific functional groups [38]. These spectral changes demonstrate effective removal of heteroatom-containing groups and inorganic impurities during annealing, suggesting material purification and the development of a more stable carbon framework [39]. Regarding production yield, JPC exhibits the highest value at approximately 63%, exceeding PPC (55%). Notably, the yield of FPC is about 95% based on PPC.

    The surface elemental composition and chemical bonding states of the asphalt-derived porous carbons were further analyzed by X-ray photoelectron spectroscopy (XPS) (Fig. 3d, Fig. S10 and Table S3 in Supporting information). Compared to asphalt, JPC exhibits a carbon content of 86.87% and an oxygen content of 11.98%. Deconvolution of the C 1s spectrum (Fig. 3e) reveals four distinct components: C=C (284.7 eV, sp2 hybridized carbon), C–C (286.2 eV, sp3 hybridized carbon), and C=O (288.7 eV). The sp2-hybridized carbon forms the conductive skeletal framework of the porous carbon, while the sp3-hybridized carbon content correlates with increased structural defects. These defects promote the adsorption/desorption of charge carriers [40]. As shown in Fig. 3f, JPC exhibits a higher sp3/sp2 value, indicating a greater number of defect sites, confirming the Raman analyses in Fig. 3a. The greater number of defect sites can be attributed to the highly porous structure and elevated surface area created by the ultrafast molten-salt method. These defect sites can serve as additional active sites for charge storage, which facilitate ion transport by providing more accessible pathways, and improve wettability between the electrode and electrolyte [41]. Moreover, structural defects can induce localized electronic states that enhance charge accumulation, thereby contributing to both electric double-layer capacitance and pseudocapacitive behavior [42].

    The energy storage performance of the asphalt-based carbon was firstly evaluated in a three-electrode system using cyclic voltammetry (CV), galvanostatic charge-discharge (GCD), and electrochemical impedance spectroscopy (EIS) measurements in 6.0 mol/L KOH electrolyte [43]. The CV curves (Figs. S11-S14, S15a and c in Supporting information) of asphalt-based carbon electrodes exhibit EDLC characteristics at a scan rate of 5.0 mV/s. PPC, FPC, and JPC still exhibit relatively undistorted electric double-layer characteristics at a scan rate of 200.0 mV/s, including desirable rate performance and lower hysteresis resistance [44]. As shown in Fig. S15b (Supporting information), the GCD curves of these samples present near-isosceles triangles at 1.0 A/g, demonstrating a high Coulombic efficiency. The specific capacitance of JPC is further divided into two components: surface capacitance controlled by surface processes and insertion capacitance controlled by diffusion, with the former being limited by the scan rate [45]. Figs. S15d and e (Supporting information) shows the fitted capacitance ratios, where the surface capacitance contributions are 56% and 85% at scan rates of 5 and 100 mV/s, respectively, indicating that JPC primarily exhibits EDLC characteristics. The remaining contribution may arise from pseudocapacitance provided by hetero elements [46,47]. As shown in Fig. S15f (Supporting information), the capacitance contribution reveals that pseudocapacitance significantly decreases at high scan rates, primarily due to the shorter diffusion time under these conditions. In Fig. S15g (Supporting information), the specific capacitance (Cg) of the JPC electrode is calculated at 362.9 F/g, exceeding that of PPC (274.4 F/g), and FPC (247.8 F/g) at a current density of 0.5 A/g. This enhancement is attributed to the rapid Joule heating method, which results in large specific surface area with an optimal number of active sites [38,48].

    The electrochemical impedance spectroscopy (EIS) plots of JPC, FPC, PPC electrodes were shown in Fig. S15h (Supporting information). The impedance curves of all asphalt-based electrodes exhibit typical semicircles and linear sections. The semicircle in the high-frequency region represents the characteristics related to internal resistance, specifically the charge transfer process between the carbon material electrode and the electrolyte. JPC exhibits the smallest semicircle, indicating the lowest charge transfer resistance (Rct) [49]. The slope in the low-frequency region is associated with ion diffusion performance, and JPC has the smallest diffusion resistance [50]. JPC possesses a more abundant hierarchical pore structure (a combination of micropores and mesopores), which not only provides more charge storage sites but also improves the efficiency of ion transport in the electrolyte, thereby reducing resistance [51]. The results show that the characteristic frequencies at a phase angle of 45° for JPC, FPC, and PPC are 0.38, 0.32, and 0.18 Hz, with corresponding relaxation time constants τ0 of 2.63, 3.12, and 5.56 s, respectively. The distribution of relaxation times (DRT) analysis of JPC (Fig. S15i in Supporting information) reveals the synergistic optimization effect of its unique pore structure on electrochemical kinetics. Benefiting from hierarchical pore channels (dominated by micro-/mesopores) and high specific surface area, the double-layer capacitive response in the high-frequency region (<0.01 s) of the DRT spectrum demonstrates rapid and stable capacitive behavior, indicating that the abundant pore-electrolyte interfaces significantly enhance charge storage efficiency [52]. The mid-frequency dominant peak (~0.1 s, ~1.6 Hz), corresponding to the charge transfer process, exhibits relatively low polarization intensity (narrow peak width), attributed to accelerated electron transport enabled by the 3D interconnected conductive network and reduced reaction activation energy due to active sites on the micropore surface [53]. Notably, the diffusion-related features in the low-frequency region (>1 s) maintain smooth evolution even under high voltages (0.7–0.9 V), confirming that mesopore-dominated ion transport channels alleviate concentration polarization, ensuring efficient mass transport under high-voltage conditions [54]. This pore structure-kinetics coupling mechanism provides critical guidance for designing high-performance energy storage electrodes through precise regulation of pore size distribution and surface defect density.

    According to Figs. S16-S18 (Supporting information), the optimal operating voltages in 1.0 mol/L Na2SO4 and 17.0 mol/L NaClO4 electrolytes are 1.8 V and 2.3 V, respectively. This significant voltage expansion is expected to enhance the achievable energy density. To assess practical potential, symmetric JPC-based supercapacitors were assembled in three electrolytes: 6.0 mol/L KOH, 1.0 mol/L Na2SO4, and 17.0 mol/L NaClO4). The CV curves for all JPC-SCs exhibit quasi-rectangular shapes at 50 mV/s, all CV curves of JPC-SCs show quasi-rectangular shapes at a scan rate of 50 mV/s, and GCD curves show high symmetry (Figs. 4a, d and g). Specific capacitance values at 0.5 A/g are 175.8 F/g (KOH), 138.4 F/g (Na2SO4), and 146.1 F/g (NaClO4) for the assembled SCs. Impressive rate capability is evidenced by retained capacitances of 111.5 F/g (KOH), 93.0 F/g (Na2SO4), and 101.7 F/g (NaClO4) at 10 A/g. Due to the increased operating voltage, the JPC-SCs with NaClO4 electrolyte deliver a high energy density of 26.7 Wh/kg at 286.7 W/kg, significantly exceeding values in KOH (6.1 Wh/kg at 124.8 W/kg) and Na2SO4 (15.5 Wh/kg at 224.5 W/kg), as shown in Figs. 4b, e and h. The excellent capacitive performance of the JPC//NaClO4//JPC device is illustrated in Fig. S19 (Supporting information) through a radar plot. EIS analysis confirms ideal capacitive behavior (near-vertical lines at low frequencies in Figs. 4c, f and i and low resistance (minimal high-frequency intercept and small semicircle diameter), signifying low equivalent series resistance (ESR) and charge transfer resistance (Rct) [55,56]. Furthermore, all devices demonstrate excellent cycling stability (above 85% capacitance retention) with stable Coulombic efficiency after 10,000 cycles in different electrolytes. Carbon materials generally undergo electrochemical oxidation in oxygen-containing electrolytes, which can compromise their cycling performance.

    Figure 4

    Figure 4.  (a) GCD curves of JPC-based SCs under different current densities, (b) Ragone plots and (c) cycling stability along with Coulombic efficiency of JPC-based SCs in 6.0 mol/L KOH electrolyte. (d) GCD curves of JPC-based SCs under different current densities, (e) Ragone plots and (f) cycling stability along with Coulombic efficiency of JPC-based SCs in 1.0 mol/L Na2SO4 electrolyte. (g) GCD curves of JPC-based SCs under different current densities, (h) Ragone plots and (i) cycling stability along with Coulombic efficiency of JPC-based SCs in 17.0 mol/L NaClO4 electrolyte.

    In summary, we report a one-pot ultrafast molten-salt method for the green synthesis of asphalt-based porous carbon. The Joule heating generates an instantaneous temperature of 850 ℃ and a heating rate above 567 ℃/s, this process efficiently transforms asphalt into carbon sheets with large specific surface area and multiscale pore structure. As expected, the JPC electrode in 6.0 mol/L KOH electrolyte achieves a specific capacitance of 362.9 F/g at 0.5 A/g. The JPC//KOH//JPC SC demonstrates an impressive specific energy of 6.1 Wh/kg at a power density of 124.8 W/kg, as well as excellent cycling stability (99.7% of capacitance retention after 10,000 cycles). When utilizing the 17.0 mol/L NaClO4 electrolyte, an extended operational voltage of 2.3 V is achieved with an enhanced specific energy of 26.7 Wh/kg. Our work opens new avenues for the high-value transformation of asphalt and other crude materials, and will find extensive applications in the energy and environmental areas.

    Zhipeng Wang: Writing – original draft, Software, Investigation, Formal analysis. Zhengxun Ma: Investigation, Formal analysis. Jintao Huang: Investigation, Formal analysis. Shuhao Zhang: Methodology, Formal analysis. Jiangfeng Ni: Writing – review & editing, Supervision, Funding acquisition. Gaoyi Han: Writing – review & editing, Supervision, Funding acquisition. Sheng Zhu: Writing – review & editing, Supervision, Resources, Funding acquisition.

    The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

    This work was financially supported by the National Natural Science Foundation of China (Nos. 52402284, U1510121, 52372213, and 52172219). We thank the Saiyin Materials Co., Ltd. for the technical support and the Joule heating system (No. FJH-2024B) for this work.

    Supplementary material associated with this article can be found, in the online version, at doi:10.1016/j.cclet.2025.112120.


    1. [1]

      A.M. Homayounfard, M. Maleki, H.B.M. Emrooz, et al., J. Mater. Chem. A 12 (2024) 22045–22060. doi: 10.1039/d4ta03118k

    2. [2]

      K. Li, J. Zhang, Sci. China Mater. 61 (2018) 210–232. doi: 10.1007/s40843-017-9154-2

    3. [3]

      S. Liu, J. Yang, P. Chen, et al., Electrochem. Energy Rev. 7 (2024), 1007/s41918-024-00222-z.

    4. [4]

      Q. Zhang, M. Yuan, L. Liu, et al., Langmuir 40 (2024) 5326–5337. doi: 10.1021/acs.langmuir.3c03790

    5. [5]

      W. Feng, C. Liu, Z. Liu, H. Pang, Chin. Chem. Lett. 35 (2024) 109552. doi: 10.1016/j.cclet.2024.109552

    6. [6]

      J. Wang, T. Huo, Y. Zhao, R. Lu, X. Wu, J. Energy Storage 110 (2025) 115216. doi: 10.1016/j.est.2024.115216

    7. [7]

      Q. Bao, M. Zhang, J. Li, et al., Renew. Energy. 225 (2024) 120209. doi: 10.1016/j.renene.2024.120209

    8. [8]

      H. Jiang, Y. Zhang, J. Li, et al., J. Energy Storage 90 (2024) 111922. doi: 10.1016/j.est.2024.111922

    9. [9]

      X. Shi, S. Zhang, X. Chen, et al., Carbon 1157 (2020) 55–63.

    10. [10]

      Y. Yin, Q. Liu, Y. Zhao, et al., Energy Fuels 37 (2023) 3523–3554. doi: 10.1021/acs.energyfuels.2c04093

    11. [11]

      S. Li, Z. Yang, M. Wu, et al., Energy Environ. Mater. 5 (2022) 1238–1250. doi: 10.1002/eem2.12240

    12. [12]

      P. Waribam, S.D. Ngo, T.T.V. Tran, et al., Waste Manage. 105 (2020) 492–500. doi: 10.1016/j.wasman.2020.02.042

    13. [13]

      Y. Yang, P. Zuo, S. Qu, Fuel 311 (2022) 122514. doi: 10.1016/j.fuel.2021.122514

    14. [14]

      Y.L. Wang, X.H. Chen, M.J. Ding, J.Z. Li, Energy Fuels. 32 (2018) 796–800. doi: 10.1021/acs.energyfuels.7b02010

    15. [15]

      Q.Q. Zhuang, J.P. Cao, Y. Wu, et al., J. Power Sources 508 (2021) 230330. doi: 10.1016/j.jpowsour.2021.230330

    16. [16]

      R. Zhao, J. Hao, X. Yang, et al., Phys. Chem. Chem. Phys. 26 (2024) 6037–6048. doi: 10.1039/d3cp05873e

    17. [17]

      O. Boujibar, F. Ghamouss, A. Ghosh, O. Achak, T. Chafik, J. Power Sources 436 (2019) 226882. doi: 10.1016/j.jpowsour.2019.226882

    18. [18]

      V. Pusarapu, R.Narayana Sarma, P. Ochonma, G. Gadikota, NPJ Mater. Sustain. 2 (2024) 16. doi: 10.1038/s44296-024-00020-0

    19. [19]

      H. Liu, S. Zhu, Y. Zhang, et al., Small 19 (2023) 2204119. doi: 10.1002/smll.202204119

    20. [20]

      Y. Tao, D. Wu, T. Wang, P. Ren, D. Jia, J. Power Sources 573 (2023) 233114. doi: 10.1016/j.jpowsour.2023.233114

    21. [21]

      H. Guan, W. Li, J. Han, et al., Nat. Commun. 12 (2021) 1376. doi: 10.1038/s41467-021-21693-4

    22. [22]

      C. Ma, J. Gong, S. Zhao, et al., Green Energy Environ. 7 (2022) 818–828. doi: 10.1016/j.gee.2020.12.004

    23. [23]

      D.X. Luong, K.V. Bets, W.A. Algozeeb, et al., Nature 577 (2020) 647–651. doi: 10.1038/s41586-020-1938-0

    24. [24]

      X. Zhu, L. Lin, M. Pang, et al., Nat. Commun. 15 (2024) 3218. doi: 10.1038/s41467-024-47603-y

    25. [25]

      W. Yang, L. Shang, X. Liu, et al., Chin. Chem. Lett. 35 (2024) 109501. doi: 10.1016/j.cclet.2024.109501

    26. [26]

      K.M. Wyss, R.D. De Kleine, R.L. Couvreur, et al., Commun. Eng. 1 (2022) 3. doi: 10.1038/s44172-022-00006-7

    27. [27]

      L. Zhang, L. Peng, Y. Lu, et al., Nat. Commun. 14 (2023) 5015. doi: 10.1038/s41467-023-40737-5

    28. [28]

      B. Deng, R.A. Carter, Y. Cheng, et al., Nat. Commun. 14 (2023) 6371. doi: 10.1038/s41467-023-41898-z

    29. [29]

      J. Huang, S. Zhu, J. Zhang, et al., ACS Mater. Lett. 6 (2024) 2144–2152. doi: 10.1021/acsmaterialslett.4c00275

    30. [30]

      Q. Li, Y. Wang, R. Zhu, et al., Colloids Surf. A 682 (2024) 132900. doi: 10.1016/j.colsurfa.2023.132900

    31. [31]

      Z. Wu, K. Tian, T. Huang, et al., ACS Appl. Mater. Interfaces 10 (2018) 11108–11115. doi: 10.1021/acsami.7b17264

    32. [32]

      F. Xu, Z. Tang, S. Huang, et al., Nat. Commun. 6 (2015) 7221. doi: 10.1038/ncomms8221

    33. [33]

      P. Chang, L. Li, F. Yang, et al., Electrochim. Acta 477 (2024) 143786. doi: 10.1016/j.electacta.2024.143786

    34. [34]

      R. Yuan, Y. Guo, I. Gurgan, et al., Carbon 238 (2025) 120214. doi: 10.1016/j.carbon.2025.120214

    35. [35]

      X. Huang, X. Lyu, G. Wu, et al., Adv. Energy Mater. 14 (2024) 2303417. doi: 10.1002/aenm.202303417

    36. [36]

      B. Pei, H. Yu, L. Zhang, et al., Adv. Mater. 37 (2025) 2504574. doi: 10.1002/adma.202504574

    37. [37]

      X. Gong, Q. Ma, L. Wang, et al., NPJ. Clean. Water. 7 (2024) 80. doi: 10.1038/s41545-024-00372-z

    38. [38]

      L. Cheng, C.S. Yeung, L. Huang, et al., Nat. Commun. 15 (2024) 2925. doi: 10.1038/s41467-024-47341-1

    39. [39]

      T. Lian, L. Xu, D. Piankova, et al., Nat. Commun. 15 (2024) 6199. doi: 10.1038/s41467-024-50476-w

    40. [40]

      S. Ghosh, G. Pagani, A. Macrelli, et al., Chem. Eng. J. 520 (2025) 166402. doi: 10.1016/j.cej.2025.166402

    41. [41]

      H. Li, Y. Zhang, Y. Wu, F. Hu, J. You, K. Zhu, J. Colloid Interface Sci. 700 (2025) 138557. doi: 10.1016/j.jcis.2025.138557

    42. [42]

      H. Li, Q. Yan, J. Li, J. Qiu, H. Zhang, Adv. Funct. Mater. 35 (2025) 2504272. doi: 10.1002/adfm.202504272

    43. [43]

      M. Mehmandoust, G. Li, N. Erk, Ind. Eng. Chem. Res. 62 (2023) 4628–4635. doi: 10.1021/acs.iecr.2c03058

    44. [44]

      Z. Li, M. Xu, Y. Xia, et al., Nat. Commun. 16 (2025) 3704. doi: 10.1038/s41467-025-59015-7

    45. [45]

      G. Wang, H. Li, F. Babbe, et al., Adv. Energy Mater. 15 (2025) 2500886. doi: 10.1002/aenm.202500886

    46. [46]

      J. Li, Z. Xia, X. Wang, et al., Adv. Mater. 36 (2024) 2310422. doi: 10.1002/adma.202310422

    47. [47]

      X.Y. Luo, Y. Chen, Y. Mo, New Carbon Mater. 36 (2021) 49–68. doi: 10.1016/S1872-5805(21)60004-5

    48. [48]

      T. Wang, R. Pan, M.L. Martins, et al., Nat. Commun. 14 (2023) 4607. doi: 10.1038/s41467-023-40282-1

    49. [49]

      Y. Zhao, X. Zhang, Sci. Rep. 11 (2021) 6825. doi: 10.1038/s41598-021-85661-0

    50. [50]

      S. Wang, J. Zhang, O. Gharbi, et al., Nat. Rev. Methods Primers 1 (2021) 41. doi: 10.1038/s43586-021-00039-w

    51. [51]

      H. Sun, J. Zhu, D. Baumann, et al., Nat. Rev. Mater. 4 (2019) 45–60.

    52. [52]

      D.Y. Semerukhin, A.V. Kubarkov, V.G. Sergeyev, O.A. Semenikhin, E.V. Antipov, Electrochim. Acta 486 (2024) 144092. doi: 10.1016/j.electacta.2024.144092

    53. [53]

      X. Cai, C. Zhang, H. Ruan, et al., Adv. Sci. 11 (2024) 2406934. doi: 10.1002/advs.202406934

    54. [54]

      T. Paul, P.W. Chi, P.M. Wu, M.K. Wu, Sci. Rep. 11 (2021) 12624. doi: 10.1038/s41598-021-91871-3

    55. [55]

      H. Liu, L. Hu, R.A. Soomro, B. Xu, Mater. Chin. Chem. Lett. 34 (2023) 108004. doi: 10.1016/j.cclet.2022.108004

    56. [56]

      M.Y. Perdana, B.A. Johan, M. Abdallah, et al., Chem. Rec. 24 (2024) e202400007. doi: 10.1002/tcr.202400007

  • Figure 1  (a) Schematic illustration for fabrication routes of JPC, FPC, and PPC. (b) The curve of temperature over time in Route 1. (c) The curves of temperature and current over time in Route 2. (d) The curves of temperature and current over time in Route 3.

    Figure 2  SEM images of (a) PPC, (b) FPC, and (c) JPC. (d) TEM image of JPC. (e) N2 adsorption-desorption isotherms of FPC, PPC, and JPC. (f) Pore size distribution curves of PPC, FPC, and JPC.

    Figure 3  (a) Raman spectra of asphalt, JPC, FPC, and PPC samples. (b) XRD patterns of asphalt, JPC, FPC, and PPC samples. (c) FTIR spectra of asphalt, JPC, FPC, and PPC samples. XPS (d) survey spectra, (e) C 1s XPS spectra. (f) The sp3/sp2 hybrid carbon ratios of asphalt, JPC, FPC, and PPC samples.

    Figure 4  (a) GCD curves of JPC-based SCs under different current densities, (b) Ragone plots and (c) cycling stability along with Coulombic efficiency of JPC-based SCs in 6.0 mol/L KOH electrolyte. (d) GCD curves of JPC-based SCs under different current densities, (e) Ragone plots and (f) cycling stability along with Coulombic efficiency of JPC-based SCs in 1.0 mol/L Na2SO4 electrolyte. (g) GCD curves of JPC-based SCs under different current densities, (h) Ragone plots and (i) cycling stability along with Coulombic efficiency of JPC-based SCs in 17.0 mol/L NaClO4 electrolyte.

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  137
  • HTML全文浏览量:  8
文章相关
  • 发布日期:  2027-01-12
  • 收稿日期:  2025-09-07
  • 接受日期:  2025-11-13
  • 修回日期:  2025-11-13
  • 网络出版日期:  2025-11-14
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章