Synergistic microstructure engineering and surface coating boosting lithium storage performance in high-nickel cathodes

Wanming Teng ,  Zhizhan Li ,  Jinguo Cheng ,  Pei Xiao ,  Jiaye Liu ,  Kangli Wang ,  Hongfang Liu ,  Kai Jiang ,  Deli Wang

Citation:  Wanming Teng, Zhizhan Li, Jinguo Cheng, Pei Xiao, Jiaye Liu, Kangli Wang, Hongfang Liu, Kai Jiang, Deli Wang. Synergistic microstructure engineering and surface coating boosting lithium storage performance in high-nickel cathodes[J]. Chinese Chemical Letters, 2027, 38(1): 111996. doi: 10.1016/j.cclet.2025.111996 shu

Synergistic microstructure engineering and surface coating boosting lithium storage performance in high-nickel cathodes

English

  • High-nickel layered ternary cathode materials have emerged as a prominent choice for lithium-ion batteries (LIBs) due to their enhanced specific capacity, prolonged cycle life compared with traditional single-component materials such as LiFePO4, LiCoO2, and LiMn2O4 [1-3]. However, the intrinsic structural and interfacial instabilities of high-nickel cathode materials often result in safety concerns, including substantial capacity degradation and insufficient thermal stability [4-6]. During the cycling process, these materials undergo irreversible phase transitions, and the uneven stresses generated by these transitions contribute to the formation of microcracks. The development of microcracks accelerates the electrolyte penetration, further facilitating the degradation of the layered structure into a rock salt phase. The structural degradation is accompanied by oxygen release, which significantly compromises the structural and thermal stability of the cathode [7,8]. Moreover, high-nickel cathode materials are particularly sensitive to ambient H2O and CO2. The presence of residual lithium oxides (Li2O, Li2O2) on the cathode surface tends to interact with these atmospheric components, resulting in the formation of residual lithium compounds, such as LiOH and Li2CO3. This reaction contributes to an increase in electrical resistance on the cathode surface, thereby hindering the transport of Li+ [9,10]. The structural and interfacial instability of high-nickel cathode materials not only adversely impacts their electrochemical performance but may also give rise to safety concerns such as thermal runaway.

    Various strategies have been formulated to mitigate the structural and interfacial instability of high nickel cathode materials, such as elemental doping [11-13], surface coating [14-17], particle engineering [18-20], and morphology optimization [21-24]. Elemental doping is a prevalent method for modifying cathode materials, with the properties of different valence elements showing significant variability. Thus, selectively employing these elements can effectively regulate battery performance and cost. For instance, low valence elements like Mg2+ [25], Na+ [26], and K+ [27] are known to enhance cycling and thermal stability. Aurora et al. [25] demonstrated that magnesium occupies lithium sites and provides structural support in high-nickel LiNi1−x−yMnxCoyO2(NMC), thereby inhibiting phase transitions and significantly improving both cycling and thermal stability. Furthermore, Sun et al. [28] conducted a comprehensive investigation into how various high valence elements (Al3+, Ti4+, Ta5+, and Mo6+) influenced the geometry and crystalline structure of grains in high Ni cathode materials (Li[Ni0.91Co0.09]O2), ultimately affecting the cycling performance of LIBs. The presence of high-valence dopants resulted in highly oriented anode particles, elongated grains, and the formation of a superlattice structure with systematically arranged Li/TM cations, which contributed to suppressing internal resistance and enhancing capacity retention. Surface coatings significantly enhance the interfacial chemical stability of high-nickel cathode materials [29]. Oxide coatings, such as ZrO2 [30], Al2O3 [31], and CeO2 [32] prevent direct contact between the cathode material and the electrolyte, thus minimizing parasitic reactions and enhancing the structural integrity of the cathode. Tan et al. [33] improved the cycling stability of the ultra-high-nickel cathode material LiNi0.9Co0.05Mn0.05O2 (NCM90) through ZrTiO4 (ZTO) surface coating. The epitaxial ZTO layer and bulk Zr doping effectively suppressed internal strain and lattice oxygen release, thereby reducing particle cracking and structural degradation. Nevertheless, the insulating characteristics of these oxide coatings lead to reduced charge transfer rates. Consequently, fast ionic conductors like Li3PO4 [34], and LiAlO2 [15] are increasingly favored as coating materials. Adjusting grain microstructures, such as employing single crystals or radially ordered polycrystals, has proven effective in enhancing the mechanical stability of ultrahigh-nickel cathodes. In particular, Zhou et al. [18] synthesized high-performance ultrahigh nickel polycrystalline cathodes, specifically LiNi0.92Co0.04Mn0.04O2, by fine-tuning the precipitation reaction of the precursor alongside lithiation crystallization. The highly radially ordered configuration of the slender primary grains not only mitigated microcrack formation but also demonstrated exceptional long-term cycling performance and thermal stability. In contrast to polycrystalline structures, single-crystal high-nickel ternary cathode materials offer distinct advantages in terms of compaction density and safety performance. For example, Han et al. [35] successfully synthesized single-crystal LiNi0.83Co0.12Mn0.05O2 (NCM83), measuring 3.7 μm in size. The even distribution of stress contributed to a capacity retention of 88.1% after 1000 cycles in a fully soft-packed cell, indicating that the removal of internal grain boundaries and intergranular fractures significantly enhanced the cycling performance of the high-nickel cathode. When a concentration gradient, the high-nickel-layered oxide is utilized as the internal component while the low-nickel-layered oxide serves as the external layer, effectively achieving a balance between elevated specific capacity and cycling stability. Kim et al. [36] synthesized a Li[Ni0.9Co0.05Mn0.05]O2 cathode (CSG90) comprising multicomponent particles, in which the high-nickel core, Li[Ni0.94Co0.038Mn0.022]O2, is enveloped by a concentration gradient shell layer, with the outermost layer being Li[Ni0.841Co0.077Mn0.082]O2. The core component experiences a significant lattice contraction during the formation of the H3 phase, while the low-nickel shell layer demonstrates a delayed H3 phase transition, mitigating abrupt changes in crystalline cell dimensions, effectively suppressing microcrack propagation, minimizing side reactions, and greatly improving cycling performance and thermochemical stability.

    Traditional single modification approaches have shown limited efficacy and face challenges in concurrently optimizing particle microstructure and interfacial properties, both of which are vital for developing long-lasting high nickel cathodes. In this investigation, W-doped and Li3PO4-coated Li[Ni0.95Co0.025Mn0.025]O2 (W-NCM@LP) cathodes were created to refine the structure of the particles and the chemical stability of the surface. The findings revealed that the dual-modified W-NCM@LP cathode not only increased the structural resilience of NCM but also curtailed the H2-H3 phase transition by introducing robust W-O covalent bonds and extending the lattice spacing. Furthermore, an in situ Li3PO4 ion-conducting coating was formed on the cathode surface, enhancing the integrity of the cathode-electrolyte interface (CEI), facilitating rapid Li+ transport, preventing electrolyte-induced degradation of the NCM cathode and alleviating detrimental interfacial side reactions as well as surface deterioration. Through synergistic modification, the integration of the particle microstructure with the surface coating produces impressive results, allowing W-NCM@LP to demonstrate exceptional cycling performance at a current density of 0.5 C while maintaining a high specific discharge capacity of 175.6 mAh/g after 300 cycles. These results underscore the feasibility of fabricating high-nickel-layered cathodes with structural and interfacial stability for next-generation electric vehicles.

    The spherical Ni0.95Co0.025Mn0.025(OH)2 precursor was synthesized via a co-precipitation method, which has been previously reported in our group [37]. The W-NCM@LP cathode material was prepared using a one-step high-temperature solid-phase method and surface chemical treatment (Fig. 1a). The average chemical composition of NCM, W-NCM, and W-NCM@LP cathodes were analyzed by ICP-OES, as shown in Table S1. The analysis results show that the chemical composition of NCM is Li[Ni0.949Co0.025Mn0.026]O2, W-NCM is Li[Ni0.942Co0.023Mn0.024W0.011]O2, and W-NCM@LP is Li[Ni0.941Co0.024Mn0.025W0.001]O2. The analytical results showed that the relative fractions of Ni, Co, and Mn in all samples were close to the originally designed molar ratio of 95:2.5:2.5, including the molar ratio of the doping element W to the transition metal, which also matched the target value.

    Figure 1

    Figure 1.  (a) Schematic diagram of W-NCM@LP preparation. (b–d) XRD patterns of NCM, W-NCM, W-NCM@LP cathodes and the magnified sections of characteristic peaks. (e) Magnified XRD profiles and intensity ratio of (003)/(104) peaks. (f–h) Rietveld refinement of XRD for all samples.

    The structural characteristics of NCM, W-NCM, and W-NCM@LP were characterized by XRD, revealing that all three samples crystallize in the hexagonal α-NaFeO2 structure belonging to the R-3m space group. The obvious splitting of the diffraction peaks indicates that all materials have a well-ordered layer structure (Figs. 1b-d). Furthermore, the intensity ratios of the I(003)/I(104) peaks of NCM, W-NCM, and W-NCM@LP are 1.78, 1.72, and 1.75 much higher than 1.2, indicating a low degree of cation mixing in all cathodes [38]. It can be observed that after doping with W, the characteristic peaks of (003) and (104) change significantly to lower angles (Fig. 1e). Furthermore, XRD Rietveld refinement analysis was performed to determine the crystallographic parameters following elemental doping, as shown in Figs. 1f-h and Table S2 (Supporting information). The calculated results show that the lattice parameter of materials increases after W doping. Compared to Ni3+ (0.56 Å), Co3+ (0.545 Å), and Mn4+ (0.53 Å), W has a larger radius (0.60 Å). The larger W6+ ions replace the relatively smaller transition metal cations, directly expanding the crystal framework and primarily promoting growth along the a-axis direction. The incorporation of the high-valent W6+ ion induces a charge compensation effect, partially reducing Ni3+ to Ni2+, which has a larger ionic radius and exhibits significant Jahn-Teller activity. The lattice parameters of W-NCM@LP and W-NCM are nearly identical, indicating that the Li3PO4 coating is primarily confined to the surface layer and does not alter the overall crystal structure [39-41].

    The microscopic morphology of the NCM, W-NCM, and W-NCM@LP cathode material particles was examined using SEM. As illustrated in Figs. 2a–c and Fig. S1 (Supporting information), the secondary particles in all samples exhibited a spherical shape with an average particle size distribution of approximately 3–5 μm, with the secondary particles being closely aggregated from the primary nanoscale particles. Notably, the particles of pristine NCM, W-NCM, and W-NCM@LP cathodes exhibit significant differences in both shape and size. The primary particles of the pristine NCM were isometric and randomly arranged, showing an aspect ratio close to 1. In contrast, the primary particles of W-NCM and W-NCM@LP displayed an elongated configuration, tightly clustered and stretched along the radial direction, with aspect ratios around 4–5. The average particle aspect ratios of the pristine NCM, W-NCM, and W-NCM@LP cathodes effectively illustrate the morphological distinctions of the primary particles, indicating that W doping induces alterations in the surface energy of the crystals. Furthermore, the relatively smooth surfaces of the NCM and W-NCM particles, compared with the rougher surfaces of the Li3PO4-coated W-NCM@LP particles, confirm the successful application of the coating layers to the particle surfaces. The surface morphology and elemental distribution of W-NCM@LP were further characterized using TEM (Figs. 2d–j). Notably, a distinct coating layer (indicated by the red dashed line) is uniformly enveloped by the cathode particles on the W-NCM@LP surface, with a thickness of approximately 10 nm. The elemental distributions of the W-NCM@LP samples were assessed via EDS, revealing that the elements Ni, Co, Mn, W, and P are uniformly dispersed. This finding validates the uniformity of Li3PO4 coating layers, confirming the homogeneity of the distribution of W and P elements within the Li3PO4 layer.

    Figure 2

    Figure 2.  SEM images of (a) NCM and (b) W-NCM@LP. (c) TEM and (d–i) EDS patterns of W-NCM@LP.

    The chemical compositions and valence states of all cathode materials were evaluated using XPS, with the comprehensive XPS spectra for the NCM, W-NCM, and W-NCM@LP samples illustrated in Fig. S2a (Supporting information). The peaks attributable to W and P were observed in the modified samples (Fig. S2b in Supporting information). To assess the influence of W doping and the application of a Li3PO4 coating on the elemental and electronic configuration of the NCM surface, a detailed analysis of the high-resolution XPS spectra for NCM and W-NCM@LP were performed. As can be seen in Fig. S2c (Supporting information), the Ni 2p3/2 peak was resolved into two characteristic peaks at 854.2 and 855.6 eV, corresponding to Ni2+ and Ni3+, respectively. In particular, the peak areas associated with Ni2+ and Ni3+ in W-NCM@LP demonstrated significant variations compared with NCM. The relative abundance of Ni2+ was determined, revealing that the relative content of Ni2+ in the NCM material was 48.7%. While for the W-NCM@LP material, the Ni2+ content increased to 52.5%. This finding aligns with previous XRD Rietveld refinement results and reinforces the conclusion that W doping facilitates the partial reduction of Ni3+ to Ni2+. The high-resolution XPS spectrum for Co 2p displayed two principal peaks at 779.7 and 794.8 eV, which correlate with the Co 2p3/2 and Co 2p1/2 peaks, respectively (Fig. S2d in Supporting information). Fig. S2e (Supporting information) illustrates the XPS spectrum of C 1s, which can be deconstructed into four components corresponding to C–C, C–O, PVDF, and O—CO2. The area of the peak attributed to O—CO2 decreases after surface modification, suggesting that the residual lithium compound on the surface of the NCM material is progressively consumed after modification with H3PO4, resulting in the conversion of O—CO2 into a Li3PO4 coating layer. The O 1s XPS spectra exhibited two closely situated peaks at 531.5 and 528.7 eV. The peak at 531.6 eV originated predominantly from surface adsorbates such as LiOH, Li2CO3, and Li3PO4, while the O 1s peak at 528.9 eV was primarily caused by lattice oxygen within the cathode. Compared with NCM, the intensity of the O 1s peak in W-NCM@LP at 531.6 eV was slightly elevated, attributable to the presence of the Li3PO4 coating on the material surface (Fig. S2f in Supporting information).

    The lithium storage capabilities of NCM, W-NCM, and W-NCM@LP electrodes as cathodes for lithium half-cells were evaluated within a voltage range of 2.7–4.3 V. Fig. 3a illustrates the initial charge-discharge profiles of the various electrodes at a current density of 0.1 C (1 C = 270 mA/g). It can be found that the initial discharge capacities of the NCM, W-NCM, and W-NCM@LP materials are quite similar, measured to be 230.8, 235.5, and 235.4 mAh/g, respectively. The slightly enhanced initial discharge capacities of W-NCM and W-NCM@LP compared with that of NCM are attributed to the primary particle extension. The particle extension direction in W-NCM and W-NCM@LP aligns parallel to the Li+ transport direction within the lattice, which favors Li+ de-embedding. Fig. 3b presents the rate performance of the three electrodes at current densities of 0.2, 0.5, 1, and 2 C. It can be seen that at 0.2 C, the discharge-specific capacities of NCM, W-NCM, and W-NCM@LP are comparable. However, the capacity of NCM experiences a significant reduction with increasing the current density, attributed to slower Li+ diffusion kinetics. When the current density reaches 2 C, the discharge capacity of the W-NCM@LP electrode markedly exceeds that of the NCM electrode, indicating superior rate capability. This phenomenon can be explained by two factors. One is that W-NCM exhibits a more stable layered structure and a distinct rod morphology that enhances the rapid diffusion of Li+. The other is that the Li3PO4 coating on the surface of the W-NCM acts as an ionic conductor layer, further facilitating rapid Li+ transport.

    Figure 3

    Figure 3.  (a) Initial charge-discharge curves at 0.1 C and 25 ℃. (b) Rate performance. (c) Cycle performance at 0.5 C. (d) Capacity retention at 0.5 C.

    Figs. 3c and d provide a comparative analysis of the cycling stability exhibited by three cathodes at 0.5 C. Following 100 cycles, the capacity retention of NCM was recorded at a mere 79.2%. The improvement in cycling performance observed with W-NCM was notably less significant than that with W-NCM@LP. Although W-NCM effectively reduced cation disorder, inhibited structural transformations, and reduced cumulative strain to enhance Li+ reversibility, it faced challenges in maintaining structural integrity and preventing side reactions during cycling, which culminated in the absence of substantial gains in cycling performance. In stark contrast, W-NCM@LP demonstrated remarkable cycling performance at 0.5 C, achieving capacity retention of 90.2%, exceeding the results of previous studies (Table S3 in Supporting information). This improvement can be attributed to the functioning of the Li3PO4 coating as a protective barrier, thereby significantly reducing side reactions between the electrode and electrolyte, which in turn enhances the diffusion efficiency of Li+ at the interface. Therefore, the synergistic approach of W element doping paired with the Li3PO4 surface coating substantially bolsters the structural stability and electrochemical performance of NCM.

    To investigate the intricate relationship between capacity degradation and phase transitions occurring during the charging and discharging cycles, we performed the dQ/dV curves for all cathodes across various cycles. As depicted in Fig. S3 (Supporting information), the materials NCM, W-NCM, and W-NCM@LP experience a sequence of phase transitions during charging, specifically transitioning from H1 (hexagonal 1) to M (monoclinic), then to H2 (hexagonal 2), and finally to H3 (hexagonal 3), accompanied by the corresponding inverse phase transitions during discharging [42,43]. The redox peak observed at 4.2 V is significantly associated with the H2–H3 phase transition process. Throughout the Li+ charging and discharging mechanisms, the cathode material exhibits continuous intercalation and deintercalation behavior, leading to anisotropic lattice contraction and expansion due to the H2–H3 phase transition, which induces structural stresses and volume alterations. Such changes adversely affect the mechanical integrity of the anode particles, resulting in the formation of microcracks. As these microcracks expand, there is an increased penetration of electrolytes into the particles, exacerbating surface-side reactions and rapidly accelerating the degradation of cathode cycle life [44]. Considerably, the peak variations associated with the H2–H3 phase transition differ significantly between various cathodes after cycling. Following 200 cycles, there was a marked decrease in peak intensity corresponding to the phase transition of NCM, along with a shift in peak position and a gradual increase in polarization voltage (the difference between the anode and cathode peaks), suggesting that the material underwent an irreversible phase transition, resulting in substantial capacity loss. On the contrary, the redox peaks and the reversibility of the phase transition of W-NCM and W-NCM@LP were effectively preserved throughout the cycling process, demonstrating that the modified materials possess a more stable crystal structure and reduced polarization, as well as improved reversibility of the phase transition. This stability is mainly ascribed to the augmented structural integrity achieved through bulk phase doping, wherein W replaces transition metal positions, forming a more stable octahedral configuration with adjacent O2– (Fig. S4 in Supporting information). The W–O bond exhibits stronger bonding energy than the TM–O bond, thus improving crystal lattice stability and preventing lattice collapse during Li+ extraction [45]. Furthermore, the distinctive primary particle microstructure of W-NCM@LP serves to effectively alleviate drastic changes in lattice parameters and mitigate stress inhomogeneity, which is crucial to reinforce the structural stability of the material.

    To deeply investigate the benefits of the Li3PO4 surface coating and multiple W-doping modification strategies, the CV curves of NCM and W-NCM@LP at various scan rates ranging from 0.1 mV/s to 1 mV/s. As depicted in Fig. S5 (Supporting information), the current peak intensity progressively increases with the scan rate. A linear correlation exists between the peak current (Ip) and the square root of the scan rate (V1/2), conforming to the classical Randles-Sevchik equation:

    Ip=2.69×105×n1.5×A×DLi0.5+×CLi×ν0.5

    (1)

    where n is the number of electrons in specific electrochemical reactions, A is the electrode area (cm2), D is the lithium diffusion coefficient of lithium, ν is the potential scan rate (V/s) and C is the initial concentration of Li+ in the cathode (mol/cm3). Due to polarization effects and irreversible behavior, the anodic peak height consequently increases, while the cathodic peak height diminishes. The redox peak current (Ip) shows a linear relationship with the square root of the scan rate (V1/2). Furthermore, the Li+ diffusion coefficients (DLi+) calculated from equations, presented in Table S4 (Supporting information), are notably higher for the W-NCM@LP cathode material compared to NCM and W-NCM. This enhancement is mainly attributed to the Li3PO4 coating on the surface of the W-NCM@LP cathode, which significantly improves the diffusion ability during the insertion/extraction kinetics of Li+.

    To further examine the influence of W doping and Li3PO4 coating on the long-term cyclic stability of the cathode, both the NCM and W-NCM@LP cathodes were subjected to 300 cycles at a rate of 0.5 C (Fig. S6 in Supporting information). The original NCM demonstrated a rapid decrease in capacity after 300 cycles, achieving a specific discharge capacity of 116.5 mAh/g. In contrast, the W-NCM@LP cathode material demonstrated remarkable cycling performance, retaining a reversible capacity of 175 mAh/g after 300 cycles. Figs. 4a and b illustrate the morphologies of the NCM and W-NCM@LP electrode materials, respectively, following 300 cycles. Notable cracks were observed on the surface of the NCM cathode after cycling, and these fractures extended through the material along the grain boundaries of the primary particles. The intensified microcracks in the original NCM correlate with the dQ/dV analysis (Fig. S3a in Supporting information). In contrast, the W-NCM@LP cathode preserved its particle integrity after cycling, with no microcracks detected on the surface of the secondary particles. These findings indicate that W doping and Li3PO4 coating can effectively mitigate the phase transition and the formation of microcracks.

    Figure 4

    Figure 4.  SEM images of the cathodes: (a) NCM and (b) W-NCM@LP after 300 cycles. XPS spectra of (c) C 1s and (e) O 1s of NCM after cycles; XPS spectra of (d) C 1s and (f) O 1s of W-NCM@LP after cycles. (g) Schematic diagram of W-doped and Li3PO4-coated NCM cathodes.

    The effects of W doping and Li3PO4 coating on the structural integrity of the cathode and the surface CEI were further investigated by using XPS measurements. Throughout the electrochemical cycling of high-nickel ternary cathodes, Li+ undergoes continuous intercalation and deintercalation. Due to the similarity in the ionic radii between Li+ and Ni2+, some Ni2+ can infiltrate the lithium layers and occupy the positions originally occupied by Li+ during the extraction process [46]. The formation of oxygen vacancies and the migration of Ni2+ result in the emergence of a Ni–O phase on the surface of the material, thereby improving the extent of Li and Ni mixing. Consequently, by evaluating the relative abundance of the Ni–O phase on the surface of the cathode, one can assess the degree of structural degradation in high-nickel ternary-layered cathodes [47]. Figs. S7a and b (Supporting information) illustrate the Ni analysis of the oxidation states on the cycled cathode surface, with the high-resolution Ni 2p spectrum indicating distinct assignments of the Ni 2p3/2 peaks for NCM and W-NCM@LP to Ni2+ and Ni3+, respectively. Importantly, the content of Ni2+ on the NCM surface increases significantly after cycling compared to W-NCM@LP, suggesting a considerable formation of Ni–O phases on the NCM surface, thus indicating a pronounced structural degradation of the NCM. The emergence of the Ni–O rock salt phase not only impedes the deintercalation of Li+ but also contributes to stress concentration at the interface between the rock salt phase and the layered structure. This uneven stress may initiate the formation of microcracks, thereby accelerating the deterioration of NCM’s electrochemical performance.

    Peaks related to C–C, C–O, C=O bond formations and O–CO2 are evident in the C 1s spectra (Figs. 4c and d). By examining the relative intensities of these peaks, one can evaluate the extent of electrolyte decomposition and the development of the CEI. The intensities for the C–O, C=O, and O–CO2 peaks observed on the surface of the NCM cathode are considerably greater than those for W-NCM@LP, indicating a thicker CEI layer present on the NCM cathode. This thicker CEI layer results in increased resistance to Li+ transport, adversely affecting rate performance and causing capacity degradation. Furthermore, peaks corresponding to O (where M = Ni, Co, Mn), Li2CO3, and ROCO2Li (with R representing alkyl groups) were also identified in high-resolution O 1s spectra (Figs. 4e and f). The intensity of the ROCO2Li and Li2CO3 peak in the NCM sample is markedly higher than in W-NCM@LP, suggesting that the formation of this side reaction product not only consumes active lithium but also decreases the discharge capacity while increasing the interfacial impedance, further obstructing Li+ migration. In contrast, the W-NCM@LP electrode exhibited a significant reduction in the by-products of electrolyte decomposition and interfacial parasitic reactions, leading to enhanced interfacial stability. This finding implies that a thinner CEI might have formed on the W-NCM@LP surface.

    The findings of the previously mentioned research demonstrate that the incorporation of W doping and the application of a Li3PO4 surface coating substantially improve the structural and interfacial integrity of the electrode. This approach concurrently minimizes the leaching of transition metals and surface parasitic reactions. The secondary particles of the W-NCM@LP material are characterized by a distinct arrangement of rod-like primary particles that effectively impede the advancement of microcracks, thereby averting electrolyte infiltration that could result in secondary corrosion. Furthermore, the Li3PO4 layer in situ that develops on the surface of the cathode utilizes any residual lithium from the manufacturing process, thereby improving interfacial stability. This coating reduces the direct interaction between the material surface and the electrolyte, significantly reducing side reactions between the active material and the electrolyte throughout the cycling phase, thus fostering a more robust development of the CEI. Furthermore, as an ionic conducting layer, Li3PO4 facilitates efficient channels for rapid Li+ migration, strengthening Li+ diffusion and markedly enhancing the cycling performance of the electrode (Fig. 4g).

    In conclusion, the W-NCM@LP cathode was successfully synthesized through a dual strategy of bulk W doping and surface Li3PO4 modification. The W-doping induces unique rod-like primary particle morphology, which effectively inhibits microcrack propagation within the particles. Concurrently, the in-situ formed Li3PO4 coating not only passivates residual lithium species but also constructs a conductive interface that facilitates Li+ transport and suppresses excessive cathode-electrolyte interphase formation. Benefiting from the synergistic interaction between W doping and Li3PO4 surface coating, the W-NCM@LP cathode delivers exceptional cycling stability, maintaining a discharge-specific capacity of 175.6 mAh/g after 300 cycles, while preserving structural integrity, with no microcracks observed on the secondary particle surfaces. This study demonstrates a rational design strategy that synergistically combines particle microstructure engineering with protective surface coating, offering valuable insights for developing high-performance nickel-rich layered cathode materials.

    Wanming Teng: Writing – original draft, Validation, Data curation, Conceptualization. Zhizhan Li: Validation, Data curation. Jinguo Cheng: Validation, Investigation. Pei Xiao: Validation, Investigation. Jiaye Liu: Validation, Investigation. Kangli Wang: Investigation, Funding acquisition. Hongfang Liu: Validation, Project administration. Kai Jiang: Investigation, Funding acquisition. Deli Wang: Writing – review & editing, Project administration, Investigation, Conceptualization.

    The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

    This work was supported by the National Natural Science Foundation (No. 22279036), the Fundamental Research Funds for the Central Universities (No. 2025BRA003) and the Innovation and Talent Recruitment Base of New Energy Chemistry and Device (No. B21003).

    Supplementary material associated with this article can be found, in the online version, at doi:10.1016/j.cclet.2025.111996.


    1. [1]

      J. Lu, C. Xu, W. Dose, S. Dey, et al., Chem. Soc. Rev. 53 (2024) 4707–4740. doi: 10.1039/d3cs00741c

    2. [2]

      L. Wang, J. Wang, Y. Lu, et al., Chem. Soc. Rev. 54 (2025) 1234–1256. doi: 10.3390/biology14091234

    3. [3]

      J.J. Fang, Y.H. Du, Z.J. Li, et al., J. Electrochem. 30 (2024) 1–18.

    4. [4]

      Z. Deng, Y. Liu, L. Wang, et al., Mater. Today 69 (2023) 236–261. doi: 10.1016/j.mattod.2023.07.024

    5. [5]

      Z. Li, J. Qin, J. Liang, et al., Energy Storage Sci. Technol. 11 (2022) 2900–2912. doi: 10.1109/tpds.2022.3151739

    6. [6]

      W. Zhao, K. Wang, R. Dubey, et al., Mater. Today Energy 34 (2023) 101301. doi: 10.1016/j.mtener.2023.101301

    7. [7]

      C. Liao, F. Li, J. Liu, Nanomaterials 12 (2022) 1888. doi: 10.3390/nano12111888

    8. [8]

      L. Chang, W. Yang, K. Cai, et al., Mater. Horiz. 10 (2023) 4776–4826. doi: 10.1039/d3mh01151h

    9. [9]

      Y. Kim, H. Park, J.H. Warner, A. Manthiram, ACS Energy Lett. 6 (2021) 941–948. doi: 10.1021/acsenergylett.1c00086

    10. [10]

      Z. Cui, P. Zuo, Z. Guo, C. Wang, A. Manthiram, Adv. Mater. 36 (2024) 2402420. doi: 10.1002/adma.202402420

    11. [11]

      G. Zhao, Z.L. Gong, Y.X. Li, Y. Yang, J. Electrochem. 29 (2023) 3. doi: 10.1142/9789811254895_0001

    12. [12]

      N.Y. Park, S.B. Kim, M.C. Kim, et al., Adv. Energy Mater. 13 (2023) 2301530. doi: 10.1002/aenm.202301530

    13. [13]

      M. Jiang, P. Wang, Q. Chen, et al., Chin. Chem. Lett. 36 (2025) 110040. doi: 10.1016/j.cclet.2024.110040

    14. [14]

      M. Yoon, Y. Dong, J. Hwang, et al., Nat. Energy 6 (2021) 362–371. doi: 10.1038/s41560-021-00782-0

    15. [15]

      H. Yu, Y. Cao, L. Chen, et al., Nat. Commun. 12 (2021) 4564–4578. doi: 10.1038/s41467-021-24893-0

    16. [16]

      H. Tang, D. Liu, J. Huang, et al., Chin. Chem. Lett. 36 (2025) 109987. doi: 10.1016/j.cclet.2024.109987

    17. [17]

      X. Qu, H. Huang, T. Wan, et al., Nano Energy 91 (2022) 106665. doi: 10.1016/j.nanoen.2021.106665

    18. [18]

      X. Zhou, F. Hong, S. Wang, et al., eScience 4 (2024) 100276. doi: 10.1016/j.esci.2024.100276

    19. [19]

      Z. Li, Y. Wang, J. Wang, et al., Nat. Commun. 15 (2024) 10216. doi: 10.1038/s41467-024-54637-9

    20. [20]

      C. Zhang, W. Zhao, S.H. Park, et al., Adv. Funct. Mater. 33 (2023) 2213860. doi: 10.1002/adfm.202213860

    21. [21]

      H.H. Ryu, S.B. Lee, C.S. Yoon, Y.K. Sun, ACS Energy Lett. 7 (2022) 3072–3079. doi: 10.1021/acsenergylett.2c01670

    22. [22]

      J. Liang, Z. Li, J. Cheng, et al., Nano Res. 16 (2023) 4987–4995. doi: 10.1007/s12274-022-5221-6

    23. [23]

      G.T. Park, N.Y. Park, T.C. Noh, et al., Energy Environ. Sci. 14 (2021) 5084–5095. doi: 10.1039/d1ee01773j

    24. [24]

      N.Y. Park, H.H. Ryu, G.T. Park, T.C. Noh, Y.K. Sun, Adv. Energy Mater. 11 (2021) 2003767. doi: 10.1002/aenm.202003767

    25. [25]

      A. Martin, F. Reissig, L. Frankenstein, et al., Adv. Energy Mater. 12 (2022) 2103045. doi: 10.1002/aenm.202103045

    26. [26]

      J. Jian, X. Xu, X. Pan, et al., Chem. Eng. J. 496 (2024) 154344. doi: 10.1016/j.cej.2024.154344

    27. [27]

      T. Xu, C. Liu, Z. Guo, et al., J. Mater. Sci. 56 (2021) 2399–2411. doi: 10.1007/s10853-020-05306-x

    28. [28]

      H.H. Sun, U.H. Kim, J.H. Park, et al., Nat. Commun. 12 (2021) 6552. doi: 10.1038/s41467-021-26815-6

    29. [29]

      U. Nisar, N. Muralidharan, R. Essehli, et al., Energy Storage Mater. 38 (2021) 309–328. doi: 10.1016/j.ensm.2021.03.015

    30. [30]

      W. Bao, G. Qian, L. Zhao, et al., Nano Lett. 20 (2020) 8832–8840. doi: 10.1021/acs.nanolett.0c03778

    31. [31]

      W. Liu, X. Li, D. Xiong, et al., Nano Energy 44 (2018) 111–120. doi: 10.15302/j-sscae-2018.02.017

    32. [32]

      H. Ding, Y. Su, X. Wang, et al., J. Colloid Interface Sci. 687 (2025) 118–130. doi: 10.1016/j.jcis.2025.02.051

    33. [33]

      Z. Tan, X. Chen, Y. Li, et al., Adv. Funct. Mater. 33 (2023) 202215123.

    34. [34]

      P. Yan, J. Zheng, J. Liu, et al., Nat. Energy 3 (2018) 600–605. doi: 10.1038/s41560-018-0191-3

    35. [35]

      Q. Han, H. Yu, L. Cai, et al., Proc. Natl. Acad. Sci. U. S. A. 121 (2024) e2317282121. doi: 10.1073/pnas.2317282121

    36. [36]

      U.H. Kim, H.H. Ryu, J.H. Kim, et al., Adv. Energy Mater. 9 (2019) 1803902. doi: 10.1002/aenm.201803902

    37. [37]

      Z. Li, X. Huang, J. Liang, et al., J. Energy Chem. 77 (2023) 461–468. doi: 10.1016/j.jechem.2022.11.002

    38. [38]

      J. Zhang, D. Zhou, W. Yang, et al., J. Electrochem. Soc. 166 (2019) A4097–A4105. doi: 10.1149/2.0641916jes

    39. [39]

      F. Xin, A. Goel, X. Chen, et al., Chem. Mater. 34 (2022) 7858–7866. doi: 10.1021/acs.chemmater.2c01461

    40. [40]

      R. Yang, J. Xie, J. Li, et al., Small 21 (2025) 202409426.

    41. [41]

      F. Du, H. Qu, X. Yu, Chem. Eng. J. 492 (2024) 152357. doi: 10.1016/j.cej.2024.152357

    42. [42]

      H.H. Ryu, K.J. Park, D.R. Yoon, et al., Adv. Energy Mater. 9 (2019) 1902698. doi: 10.1002/aenm.201902698

    43. [43]

      T. Liu, L. Yu, J. Lu, et al., Nat. Commun. 12 (2021) 6024. doi: 10.1038/s41467-021-26290-z

    44. [44]

      X. Ou, T. Liu, W. Zhong, et al., Nat. Commun. 13 (2022) 2319. doi: 10.1038/s41467-022-30020-4

    45. [45]

      C.H. Jung, D.H. Kim, D. Eum, et al., Adv. Funct. Mater. 31 (2021) 2010095. doi: 10.1002/adfm.202010095

    46. [46]

      X. Xiong, Z. Wang, X. Yin, H. Guo, X. Li, Mater. Lett. 110 (2013) 4–9. doi: 10.1016/j.matlet.2013.07.098

    47. [47]

      K. Yuan, N. Li, R. Ning, et al., Nano Energy 78 (2020) 105239. doi: 10.1016/j.nanoen.2020.105239

  • Figure 1  (a) Schematic diagram of W-NCM@LP preparation. (b–d) XRD patterns of NCM, W-NCM, W-NCM@LP cathodes and the magnified sections of characteristic peaks. (e) Magnified XRD profiles and intensity ratio of (003)/(104) peaks. (f–h) Rietveld refinement of XRD for all samples.

    Figure 2  SEM images of (a) NCM and (b) W-NCM@LP. (c) TEM and (d–i) EDS patterns of W-NCM@LP.

    Figure 3  (a) Initial charge-discharge curves at 0.1 C and 25 ℃. (b) Rate performance. (c) Cycle performance at 0.5 C. (d) Capacity retention at 0.5 C.

    Figure 4  SEM images of the cathodes: (a) NCM and (b) W-NCM@LP after 300 cycles. XPS spectra of (c) C 1s and (e) O 1s of NCM after cycles; XPS spectra of (d) C 1s and (f) O 1s of W-NCM@LP after cycles. (g) Schematic diagram of W-doped and Li3PO4-coated NCM cathodes.

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  131
  • HTML全文浏览量:  12
文章相关
  • 发布日期:  2027-01-12
  • 收稿日期:  2025-06-20
  • 接受日期:  2025-10-21
  • 修回日期:  2025-10-15
  • 网络出版日期:  2025-10-22
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章