Modulation effect in adjacent dual metal single atom catalysts for electrochemical nitrogen reduction reaction

Xiaonan Zheng Yang Liu Yu Yan Xiaoxiao Li Yuan Yao

Citation:  Xiaonan Zheng, Yang Liu, Yu Yan, Xiaoxiao Li, Yuan Yao. Modulation effect in adjacent dual metal single atom catalysts for electrochemical nitrogen reduction reaction[J]. Chinese Chemical Letters, 2022, 33(3): 1455-1458. doi: 10.1016/j.cclet.2021.08.102 shu

Modulation effect in adjacent dual metal single atom catalysts for electrochemical nitrogen reduction reaction

English

  • Ammonia (NH3) is of great significance and widely used in agriculture, industry, and sustainable energy conversion [1, 2]. In industry, Haber–Bosch method is currently used for large-scale ammonia production at high temperature and high pressure over Fe-based or Ru-based catalysts, which requires high energy input and emits a large amount of greenhouse gases [3, 4]. Therefore, it is urgently-needed to develop green and sustainable ways for NH3 production under mild conditions [5-8]. Among the NH3 synthesis methods, electrochemical nitrogen reduction reaction (NRR) using water as the hydrogen source offers a promising way to replace the high-energy-consuming and environment-polluting Haber–Bosch method [9].

    However, it is difficult to cleave and dissociate the N≡N bond due to its high total bond energy (941 kJ/mol) [10]. For this reason, the performance of the NRR electrocatalyst has very big upgrade space due to a low yield rate of NH3 and faradaic efficiency (FE) [11-13]. Multiple materials including pure metals [14, 15], alloys [16], metal compounds [17, 18] and nonmetals [19, 20] have been applied for experimental studies of NH3 synthesis in both theory and experiment. Single-atom catalysts (SACs), isolated metal atoms anchored to supports, have been applied in many fields such as oxygen reduction reaction (ORR) [21], CO2 reduction reaction (CO2RR) [22] and oxidation of formaldehyde [23, 24] due to the 100% atomic utilization, high activity and selectivity, and durable stability [25-27]. In a series of single metal atom catalysts, many metal-nitrogen-carbon (M-N-C, M = Fe, Co, Ni, Mn, Mo, Y, Sc, etc.) have successfully developed for electrocatalysis [28-31]. In particular, inspired by the natural metalloenzyme called cytochrome c oxidase (CcO) with the adjacent Cu and Fe sites [32-34], several dual metal single atom catalysts with adjacent M-N-C dual active centers have been synthesized recently and exhibited excellent stability and catalytic performance [35-40]. For example, a highly dispersed Fe–Cu dual-atom nanozyme has been successfully constructed to mimic Cytochrome c oxidase for catalyzing ORR [37]. The dual-metal catalysts with neighboring Fe-N4-C and Co-N4-C active centers are also reported as efficient ORR catalysts [36, 39]. In addition, a dual metal single atom catalyst consisted of Cu-N4 and Zn-N4 on the N-doped carbon support was prepared and showed high ORR activity [35].

    As far as we know, there is no report of dual-metal catalysts for the NRR by now, and the in-depth analysis and understanding of structure-property relationship for the neighboring M-N-C catalysts are also insufficient. Inspired by the successful synthesis of adjacent M-N-C catalysts and their potential catalytic activity, we designed a series of non-precious metal-based neighboring M-N-C catalysts (denoted as MN4/M'N4-C), and employed the density functional theory (DFT) method to explore the NRR activity. Firstly, the stability of catalysts is evaluated, and NRR selectivity was investigated by considering *N2/*H adsorption. According to the adsorption configuration of N2, we then explore possible reaction pathways in the NRR process and screen promising catalysts for the NRR. Finally, the electronic structure analysis is performed to further understand the interaction on the adjacent dual metal single atom to achieve good NRR catalytic performance.

    Seven non-precious metal atoms (Cr, Mn, Fe, Co, Ni, Cu and Zn) were selected to anchor on N-doped graphene in pairs, constructing 28 MN4/M'N4-C catalysts in the present study as shown in Fig. 1a, motivated by that the corresponding M-N-C catalysts with N4-coordinated structure have been synthesized [41, 42] and this may contribute to the development of adjacent M-N-C dual single atom catalysts. In the optimized geometries, each metal atom bonds with four surrounding N atoms on the graphene substrate with bond length of 1.85~1.97 Å (Table S1 in Supporting information). In particular, the Cu-N and Zn-N bond lengths in CuN4/ZnN4-C were calculated to be 1.91 and 1.94 Å (Table S1), which are in agreement with the experimental results from the extended X-ray absorption fine structure (EXAFS) measurement for Cu/Zn-NC with the Cu-N and Zn-N bond lengths of 2.01 Å [35]. The dual metal single atom centers of M-N-C and M'-N-C were located in an adjacent position with the distance between two metal atoms ranging from 4.96 Å to 5.10 Å (Table S1), consistent with the corresponding experimental results that the distance between the two metal atoms is around 5.0 Å for the synthesized MN4/M'N4-C catalysts such as CuN4/ZnN4-C, FeN4/CuN4-C and FeN4/CoN4-C [35-37]. These show that our computational models for the as-designed catalysts are reliable and reasonable.

    Figure 1

    Figure 1.  (a) The structures of adjacent dual metal active sites on MN4/M'N4-C and (b) the calculated Ebind values.

    Based on the optimized geometries of the as-designed catalysts, we then evaluate their stabilities by calculating the binding energies (Ebind) using equation: Ebind= E(MN4/M'N4-C) – E(NC)– E(M) – E(M'), where E(MN4/M'N4-C) and E(NC) represent the electronic energies of catalyst and N-doped graphene substrate, respectively; E(M) and E(M') are the electronic energies of M and M' atoms, respectively. According to this definition, a lower Ebind indicates a higher thermodynamics stability of MN4/M'N4-C. As shown in Fig. 1b, one can see that the Ebind values were all negative ranging from –15.72 eV to –4.48 eV, indicating neighboring dual metal single atom can be stably anchored in the N-doped graphene. In addition, they have the similar stabilities as the experimentally synthesized FeN4/CoN4-C, FeN4/CuN4-C and CuN4/ZnN4-C which have the binding energies calculated in this study with the values of –15.33, –12.54 and –7.45 eV, respectively. It may imply that the as-designed catalysts could also be synthesized in future.

    We next investigated the adsorption of N2 molecule on MN4/M'N4-C surfaces. As shown in Fig. 2, one can see that N2 molecule can adsorb on the surface in perpendicular end-on or parallel side-on configurations. However, two metal atoms locate so far with the distance of around 5 Å so that it is not suitable for the formation of the bridge conformation in which two N atoms in N2 molecule adsorb on different metal atoms, respectively. Based on the calculated ΔG values of N2 adsorption listed in Table S2 (Supporting information), we found that the end-on configurations are more energetically favorable than the side-on configurations for both M and M' sites. Therefore, the 11 MN4/M'N4-C with negative ΔG values via N2 end-on adsorption configuration are summarized in Table 1. Although the adsorption ability of N2 on the 11 MN4/M'N4-C was relatively weak (–0.21 eV to –0.02 eV), it was still an exothermic reaction which could proceed spontaneously. In contrast, the remaining catalysts will be excluded from following study because the adsorption and activation of N2 on these catalysts hardly take place at room temperature.

    Figure 2

    Figure 2.  The N2 adsorbed on M atom by (a) end-on and (b) side-on configurations. The N2 adsorbed on M' atom by (c) end-on and (d) side-on configurations.

    Table 1

    Table 1.  The adsorption configurations of N2 molecule and the adsorption energies of N2 molecule, H and N2H on 11 MN4/M'N4-C (The '*' donates the atom adsorbed on the surface) in eV.
    DownLoad: CSV

    As well known, hydrogen evolution reaction (HER) is the key competition reaction toward NRR, thus, the competitive adsorption between H and N2 on the catalysts was studied by comparing the changes of Gibbs free energies (ΔG(*H) and ΔG(*N2)). The results listed in Table 1 showed that the ΔG(*N2) are all negative, whereas the ΔG(*H) values are all positive. It means that N2 is preferentially adsorbed onto the screened 11 MN4/M'N4-C rather than H, preventing the accumulation of H-adatoms and exhibiting good selectivity for electrochemical NRR.

    The first hydrogenation step (*N2 + H+ + e→*N2H) is usually considered as the potential determining step (PDS) for electrochemical NRR, and high-activity catalysts should have ΔG(*N2H) values of less than the ΔGmax of the well-established Ru(0001) stepped surface (0.98 eV) [12], which was set as the criterion for metal-based catalysts due to the highest NRR theoretical activity among bulk metal surfaces [43, 44]. As shown in Table 1, 5 CrN4/M'N4-C (M' = Cr, Mn, Fe, Cu and Zn) presented the ΔG(*N2H) values of about 0.60 eV, which suggests that they meet the requirements above and will be further studied and discussed.

    Since N2 molecule prefers the end-on adsorption configuration on the 5 CrN4/M'N4-C, the typical NRR reaction pathways including distal and alternating pathways were considered to reveal the catalytic mechanism (Fig. 3a). In the distal pathway, the first three proton-electron (H+ + e) pairs are preferentially added on the distal N atom, leading to the generation of the first NH3 molecule, and then another three proton-electron (H+ + e) pairs attack the remaining N atom to release the second NH3. In the alternating pathway, six proton-electron (H+ + e) pairs alternately hydrogenate two N atoms. The produced NH3 can be easily protonated to NH4+ and released into solution under the electrochemical conditions [45, 46], so the further protonation of *NH3 into NH4+ was not considered.

    Figure 3

    Figure 3.  (a) Schematic representation of distal and alternating pathways for NRR in end-on configuration. Gibbs free energy diagrams of the NRR at zero potential (blake lines) and an applied potential (red lines) via the (b) distal and (c) alternating pathway on CrN4/MnN4-C.

    By taking the CrN4/MnN4-C as an example, as shown in Figs. 3b and c, it can be seen that the first two steps of the alternating and distal pathways, namely N2 adsorption and *N2H formation, were the same. The ΔG values of the first two steps were –0.05 and 0.62 eV, respectively. After adsorbed N2 is hydrogenated, the generated *N2H intermediate can proceed via distal or alternating pathways. In the distal pathway (Fig. 3b), the next hydrogenation to form *N-NH2 is slightly endothermic with a free energy change of 0.14 eV. One can see that *N-NH2 can be hydrogenated to release the first NH3 to form *N with free energy change of −1.02 eV. The free energy changes for the continuous hydrogenations of *N to form *NH, *NH2 and *NH3 were calculated to be −0.05, −0.56 and −0.20 eV, respectively. Regarding the alternating pathways on CrN4/MnN4-C (Fig. 3c), the second hydrogenation on the other nitrogen to form *NH-NH will proceed after overcoming a positive free energy change of 0.35 eV. In the subsequent steps, the intermediates *NH-NH2 and *NH2-NH2 are formed with the free energy change values of −0.19 and 0.06 eV, respectively. A negative free energy change of −1.71 eV is obtained with the formation of the first NH3. Finally, the second NH3 molecule can be formed with a downhill step of −0.20 eV. Therefore, the formation of *N2H species is the PDS due to the maximum ΔG values (0.62 eV) among all the elementary steps for CrN4/MnN4-C. When U = −0.62 V is applied, all elementary reactions become downhill, and the whole electrochemical NRR processes turn to be spontaneous.

    According to the detailed ΔG values of CrN4/CrN4-C, CrN4/FeN4-C, CrN4/CuN4-C and CrN4/ZnN4-C in Table S3 (Supporting information), we can find that the free energy change of PDS for these catalysts are 0.63, 0.63, 0.64 and 0.63 eV, respectively. Hereby, the computed UL for 5 CrN4/M'N4-C is from −0.64 V to −0.62 V, which are much lower than that for recently reported ruthenium SAC Ru1-N3 (−0.73 V) with the yield rate of 120.9 µgNH mgcat.−1 h−1 [47]. The UL results also indicate the better NRR activity of 5 CrN4/M'N4-C by comparing with the single atom catalysts with the same metal atom such as Cr anchored on defective graphene (−0.98 V) [44], single Mn-N4 sites anchored on porous carbon (−1.04 V) [48], Fe-N4/graphene (−1.35 V) [49], Cu on N-doped carbon (−1.85 V) [50]. Besides, considering that NRR is conducted in aqueous electrolytes, the solvation effect has been also studied on CrN4/M'N4-C (M' = Cr, Mn, Fe, Cu and Zn) along distal pathway. As shown in Fig. S1 (Supporting information), the solvation effect could reduce the limiting potential in the range of −0.49 eV to −0.37 V. Here, CrN4/M'N4-C (M' = Cr, Mn, Fe, Cu and Zn) is expected as promising candidates for electrochemical NRR.

    To clarify the origin of the catalytic activity of the 5 CrN4/M'N4-Cs (M' = Cr, Mn, Fe, Cu and Zn), we first analyzed corresponding charge density difference (Fig. 4a) and partial density of states (Fig. 4b) of the adsorbed N2 molecule on CrN4/MnN4-C as an example. The charge density difference results confirmed that both positive and negative charges accumulate around the adsorbed N2 molecule and Cr atom of CrN4/MnN4-C, which is beneficial to promote the "acceptance–donation" process [5, 51] that metal atom donates electrons to the antibonding orbitals of N2 and accepts lone-pair electrons of N2. In addition, it is noted that a small part of positive charge accumulated on Mn atom, which suggests that Mn atom probably plays a role in electron transfer to Cr atom due to the so-called modulation effect [38] and promotes the N2 activation on Cr active site. The modulation effect of CrN4/MnN4-C, where Cr atom is the only active center, while Mn atom is considered as the modulator, is completely different from the previously reported synergetic effect on double-atom catalysts (DACs) such as (Fe, Co)/CNT [52] and Ni/Fe-N-C [53], in which binary metal is demonstrated as one active center to catalyze reactions. Additionally, the computed partial density of states (PDOS) of N2 adsorption on CrN4/MnN4-C showed that the hybridization mainly occurred between Cr d-orbital and N2 p-orbital, and there was a small part of orbital overlap between Mn d-orbital and N2 p-orbital. These results clarified the origin of the activation of N2 molecule on CrN4/MnN4-C. To deeply understand the catalytic mechanism, the charge transfer variations on the basis of Bader charge differences of all reaction intermediates NxHy adsorbed on CrN4/MnN4-C via the distal pathway are summarized in Fig. 4c. Obviously, the charge was transferred from CrN4 to the adsorbed NxHy species for most of the elementary reaction steps. Even though the NxHy intermediates were mainly located at the CrN4 active site, the neighbored MnN4 acted as a reservoir to store or release electrons when needed. Consequently, the modulation effect between the dual metal single atoms is effective in electron transfer, leading to the activation of N2 and then promotes the subsequent hydrogenation step of NRR.

    Figure 4

    Figure 4.  (a) Charge density difference maps of N2 adsorption on CrN4/MnN4-C, where the isosurface value is set to be 0.005 e/Å3. The positive and negative charges are shown in cyan and yellow, respectively. (b) Partial density of states (PDOS) of N2 adsorption on CrN4/MnN4-C. (c) The Bader charge variation of the CrN4/MnN4-C along distal pathway.

    In conclusion, a series of energetically stable adjacent dual metal single atom supported on N-doped graphene (MN4/M'N4-C) are designed for electrochemical NRR by means of DFT calculations. Based on the results of N2 adsorption free energy, and Gibbs free energy change of NRR, it was predicted that 5 CrN4/M'N4-C (M' = Cr, Mn, Fe, Cu and Zn) exhibited promising NRR activity with the limiting potential of −0.64 V to −0.62 V. The modulation effect is observed in the adjacent dual metal single atom catalysts based on the analysis of charge distribution and PDOS. This work not only provides new insight for developing neighboring dual single atom catalysts at atomic level, but also highlights the importance of the modulation effect between the multi-active centers.

    The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

    This work was supported by the open project of State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology (No. AWJ-19M07) and the National Natural Science Foundation of China (No. U2067216).

    Supplementary material associated with this article can be found, in the online version, at doi:10.1016/j.cclet.2021.08.102.


    1. [1]

      S.L. Foster, S.I.P. Bakovic, R.D. Duda, et al., Nat. Catal.1 (2018) 490-500. doi: 10.1038/s41929-018-0092-7

    2. [2]

      M. Kitano, Y. Inoue, Y. Yamazaki, et al., Nat. Chem. 4 (2012) 934-940. doi: 10.1038/nchem.1476

    3. [3]

      A. Banerjee, B.D. Yuhas, E.A. Margulies, et al., J. Am. Chem. Soc. 137 (2015) 2030-2034. doi: 10.1021/ja512491v

    4. [4]

      C.J.M. van der Ham, M.T.M. Koper, D.G.H. Hetterscheid, Chem. Soc. Rev. 43 (2014) 5183-5191. doi: 10.1039/C4CS00085D

    5. [5]

      C. Ling, X. Niu, Q. Li, A. Du, J. Wang, J. Am. Chem. Soc. 140 (2018) 14161-14168. doi: 10.1021/jacs.8b07472

    6. [6]

      Y. Zhao, Y. Zhao, G.I.N. Waterhouse, et al., Adv. Mater. 29 (2017) 1703828. doi: 10.1002/adma.201703828

    7. [7]

      N. Lazouski, M. Chung, K. Williams, M.L. Gala, K. Manthiram, Nat. Catal. 3 (2020) 463-469. doi: 10.1038/s41929-020-0455-8

    8. [8]

      J.S. Anderson, J. Rittle, J.C. Peters, Nature501 (2013) 84-87. doi: 10.1038/nature12435

    9. [9]

      X. Guo, H. Du, F. Qu, J. Li, J. Mater. Chem. A7 (2019) 3531-3543. doi: 10.1039/c8ta11201k

    10. [10]

      W. Song, J. Wang, L. Fu, et al., Chin. Chem. Lett. 32 (2021) 3137–3142. doi: 10.1016/j.cclet.2021.02.043

    11. [11]

      S. Licht, B. Cui, B. Wang, et al., Science345 (2014) 637. doi: 10.1126/science.1254234

    12. [12]

      E. Skúlason, T. Bligaard, S. Gudmundsdóttir, et al., Phys. Chem. Chem. Phys. 14 (2012) 1235-1245. doi: 10.1039/C1CP22271F

    13. [13]

      J.H. Montoya, C. Tsai, A. Vojvodic, J.K. Nørskov, ChemSusChem8 (2015) 2180-2186. doi: 10.1002/cssc.201500322

    14. [14]

      H. Wang, H. Yu, Z. Wang, et al., Small15 (2019) 1804769. doi: 10.1002/smll.201804769

    15. [15]

      G. Rostamikia, S. Maheshwari, M.J. Janik, Catal. Sci. Technol. 9 (2019) 174-181. doi: 10.1039/c8cy01845f

    16. [16]

      R. Manjunatha, A. Schechter, Electrochem. Commun. 90 (2018) 96-100. doi: 10.1016/j.elecom.2018.04.008

    17. [17]

      T. Wu, X. Zhu, Z. Xing, et al., Angew. Chem. Int. Ed. 58 (2019) 18449-18453. doi: 10.1002/anie.201911153

    18. [18]

      J. Sun, W. Kong, Z. Jin, et al., Chin. Chem. Lett. 31 (2020) 953-960. doi: 10.1016/j.cclet.2020.01.035

    19. [19]

      W. Qiu, X.Y. Xie, J. Qiu, et al., Nat. Commun. 9 (2018) 3485. doi: 10.1038/s41467-018-05758-5

    20. [20]

      R. Wang, C. He, W. Chen, C. Zhao, J. Huo, Chin. Chem. Lett. 32 (2021) 3821–3824. doi: 10.1016/j.cclet.2021.05.024

    21. [21]

      J. Li, S. Chen, N. Yang, et al., Angew. Chem. Int. Ed. 58 (2019) 7035-7039. doi: 10.1002/anie.201902109

    22. [22]

      H. Yang, Y. Wu, G. Li, et al., J. Am. Chem. Soc. 141 (2019) 12717-12723. doi: 10.1021/jacs.9b04907

    23. [23]

      J. Zhou, G. Liu, Q. Jiang, et al., Chin. J. Catal. 41 (2020) 1633-1644. doi: 10.1016/S1872-2067(20)63571-9

    24. [24]

      G. Liu, J. Zhou, W. Zhao, Z. Ao, T. An, Chin. Chem. Lett. 31 (2020) 1966-1969. doi: 10.1016/j.cclet.2019.12.023

    25. [25]

      A. Wang, J. Li, T. Zhang, Nat. Rev. Chem. 2 (2018) 65-81. doi: 10.1038/s41570-018-0010-1

    26. [26]

      L. Zhang, Y. Ren, W. Liu, A. Wang, T. Zhang, Natl. Sci. Rev. 5 (2018) 653-672. doi: 10.1093/nsr/nwy077

    27. [27]

      L. Fu, R. Wang, C. Zhao, et al., Chem. Eng. J. 414 (2021) 128857. doi: 10.1016/j.cej.2021.128857

    28. [28]

      J. Liu, X. Kong, L. Zheng, et al., ACS Nano14 (2020) 1093-1101. doi: 10.1021/acsnano.9b08835

    29. [29]

      X. Wang, X. Peng, W. Chen, et al., Nat. Commun. 11 (2020) 653. doi: 10.1007/978-981-15-2914-6_62

    30. [30]

      M. Zhang, Y.G. Wang, W. Chen, et al., J. Am. Chem. Soc. 139 (2017) 10976-10979. doi: 10.1021/jacs.7b05372

    31. [31]

      L. Chen, C. He, R. Wang, et al., Chin. Chem. Lett. 32 (2021) 53-56. doi: 10.1016/j.cclet.2020.11.013

    32. [32]

      M.R.A. Blomberg, P.E.M. Siegbahn, G.T. Babcock, M. Wikström, J. Am. Chem. Soc. 122 (2000) 12848-12858. doi: 10.1021/ja002745a

    33. [33]

      T. Tsukihara, H. Aoyama, E. Yamashita, et al., Science272 (1996) 1136. doi: 10.1126/science.272.5265.1136

    34. [34]

      M. Wikström, K. Krab, V. Sharma, Chem. Rev. 118 (2018) 2469-2490. doi: 10.1021/acs.chemrev.7b00664

    35. [35]

      M. Tong, F. Sun, Y. Xie, et al., Angew. Chem. Int. Ed. 60 (2021) 14005-14012. doi: 10.1002/anie.202102053

    36. [36]

      H. Li, Y. Wen, M. Jiang, et al., Adv. Funct. Mater. 31 (2021) 2011289. doi: 10.1002/adfm.202011289

    37. [37]

      C. Du, Y. Gao, H. Chen, et al., J. Mater. Chem. A8 (2020) 16994-17001. doi: 10.1039/d0ta06485h

    38. [38]

      D. Wang, A. Han, X. Wang, et al., Angew. Chem. Int. Ed. 60 (2021)19262-19271. doi: 10.1002/anie.202105186

    39. [39]

      D. Wang, H. Xu, P. Yang, et al., J. Mater. Chem. A9 (2021) 13678-13687. doi: 10.1039/d1ta03176g

    40. [40]

      Y. Luo, J. Zhang, J. Chen, et al., J. Catal. 397 (2021) 223-232. doi: 10.1016/j.jcat.2021.03.030

    41. [41]

      D. Wang, X. Pan, P. Yang, et al., ChemSusChem14 (2021) 33-55. doi: 10.1002/cssc.202002137

    42. [42]

      J. Zhang, H. Yang, B. Liu, Adv. Eng. Mater. 11 (2021) 2002473. doi: 10.1002/aenm.202002473

    43. [43]

      X. Guo, J. Gu, S. Lin, et al., J. Am. Chem. Soc. 142 (2020) 5709-5721. doi: 10.1021/jacs.9b13349

    44. [44]

      C. Choi, S. Back, N.Y. Kim, et al., ACS Catal. 8 (2018) 7517-7525. doi: 10.1021/acscatal.8b00905

    45. [45]

      A. Clayborne, H.J. Chun, R.B. Rankin, J. Greeley, Angew. Chem. Int. Ed. 54 (2015) 8255-8258. doi: 10.1002/anie.201502104

    46. [46]

      H.J. Chun, V. Apaja, A. Clayborne, K. Honkala, J. Greeley, ACS Catal. 7 (2017) 3869-3882. doi: 10.1021/acscatal.7b00547

    47. [47]

      Z. Geng, Y. Liu, X. Kong, et al., Adv. Mater. 30 (2018) 1803498. doi: 10.1002/adma.201803498

    48. [48]

      L. Han, M. Hou, P. Ou, et al., ACS Catal. 11 (2021) 509-516. doi: 10.1021/acscatal.0c04102

    49. [49]

      D. Jiao, Y. Liu, Q. Cai, J. Zhao, J. Mater. Chem. A9 (2021) 1240-1251. doi: 10.1039/d0ta09496j

    50. [50]

      L. Han, Z. Ren, P. Ou, et al., Angew. Chem. Int. Ed. 60 (2021) 345-350. doi: 10.1002/anie.202010159

    51. [51]

      M.A. Légaré, G. Bélanger-Chabot, R.D. Dewhurst, et al., Science359 (2018) 896. doi: 10.1126/science.aaq1684

    52. [52]

      J. Wang, W. Liu, G. Luo, et al., Energy Environ. Sci. 11 (2018) 3375-3379. doi: 10.1039/c8ee02656d

    53. [53]

      W. Ren, X. Tan, W. Yang, et al., Angew. Chem. Int. Ed. 58 (2019) 6972-6976. doi: 10.1002/anie.201901575

  • Figure 1  (a) The structures of adjacent dual metal active sites on MN4/M'N4-C and (b) the calculated Ebind values.

    Figure 2  The N2 adsorbed on M atom by (a) end-on and (b) side-on configurations. The N2 adsorbed on M' atom by (c) end-on and (d) side-on configurations.

    Figure 3  (a) Schematic representation of distal and alternating pathways for NRR in end-on configuration. Gibbs free energy diagrams of the NRR at zero potential (blake lines) and an applied potential (red lines) via the (b) distal and (c) alternating pathway on CrN4/MnN4-C.

    Figure 4  (a) Charge density difference maps of N2 adsorption on CrN4/MnN4-C, where the isosurface value is set to be 0.005 e/Å3. The positive and negative charges are shown in cyan and yellow, respectively. (b) Partial density of states (PDOS) of N2 adsorption on CrN4/MnN4-C. (c) The Bader charge variation of the CrN4/MnN4-C along distal pathway.

    Table 1.  The adsorption configurations of N2 molecule and the adsorption energies of N2 molecule, H and N2H on 11 MN4/M'N4-C (The '*' donates the atom adsorbed on the surface) in eV.

    下载: 导出CSV
  • 加载中
计量
  • PDF下载量:  7
  • 文章访问数:  1189
  • HTML全文浏览量:  101
文章相关
  • 发布日期:  2022-03-15
  • 收稿日期:  2021-08-02
  • 接受日期:  2021-08-22
  • 修回日期:  2021-08-20
  • 网络出版日期:  2021-08-26
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章