引用本文:
张碧泉, 卢兆忠, 王玉玲. 碱性锌锰电池用化学二氧化锰的研制[J]. 应用化学,
1998, 15(2): 67-70.
Citation: Zhang Biquan, Lu Zhaozhong, Wang Yuling. Preparation of CMD for Alkaline Zinc-Mangenese Battery[J]. Chinese Journal of Applied Chemistry, 1998, 15(2): 67-70.

Citation: Zhang Biquan, Lu Zhaozhong, Wang Yuling. Preparation of CMD for Alkaline Zinc-Mangenese Battery[J]. Chinese Journal of Applied Chemistry, 1998, 15(2): 67-70.

碱性锌锰电池用化学二氧化锰的研制
English
Preparation of CMD for Alkaline Zinc-Mangenese Battery
Abstract:
The chemical manganese dioxide(CMD) for alkaline zinc manganese battery was prepared through direct oxidation or V-MnO2 by chlorine gas in sulfuric acid medium at 85-90 ℃ with addition of MgO as pH regulator, followed by protonation with KMnO4 solution. The CMD obtained was an n-type semiconductor and showed an improved electrochemical property. The sample battery LR03 showed a good discharge behavior.
-
Key words:
- chemical manganese dioxide
- / preparation
- / alkaline zinc-manganese battery
-
-