【无机化学学报】doi: 10.11862/CJIC.20240404
In this study, ZnSnO3/NiO heterostructures were synthesized using a co-precipitation method followed by an annealing process. The gas-sensitive characteristics of the sensors based on these samples were evaluated. The results indicate that the sensor performance was optimized when the molar ratio of Ni to Zn was 1∶2. Specifically, the response values of the ZnSnO3/NiO-2-based sensor to 100 μL·L-1 triethylamine (TEA) gas at 220 ℃ reached 70.6, which were 6.1 times higher than that of the pure ZnSnO3 based sensor. The findings demonstrate that ZnSnO3/NiO heterostructures exhibited not only short response and recovery times (1 s/18 s) but also good gas selectivity, repeatability, and long-term stability. The enhanced sensing mechanism has been investigated in detail.
【物理化学学报】doi: 10.3866/PKU.WHXB202304037
聚N-异丙基丙烯酰胺(PNIPAm)交联温敏纳米纤维膜作为一种相变温度易于控制的新兴响应性材料,克服了传统PNIPAm块状水凝胶的生产成本高、响应速率慢和PNIPAm非交联温敏纳米纤维耐水性差的缺点,受到广泛研究并应用于智能开关、温度致动器、水油分离、药物、细胞控制释放和伤口敷料等领域。形貌稳定性和快速响应性是温敏纳米纤维膜在重复体积变化过程中最大的挑战,同时也作为评价PNIPAm温敏纳米纤维膜的实用性最重要指标引起了人们广泛的关注。本文全面综述了PNIPAm温敏纳米纤维膜近二十年来国内外的突破性进展和非交联作用下PNIPAm温敏纳米纤维膜的形貌变化和响应性,重点综合分析了物理和化学交联中交联反应类型、交联度、交联时间和交联分子量对PNIPAm温敏纳米纤维膜的形貌稳定性和响应行为的影响,为之后纤维膜的交联处理提供了理论支持,并对PNIPAm温敏纳米纤维膜的发展及应用前景进行了展望。
【无机化学学报】doi: 10.11862/CJIC.20240442
Herein, an FMS/CC composite was successfully fabricated by depositing FeMoS4 onto a pristine carbon fiber cloth (CC) substrate via a facile two-step hydrothermal method. The amorphous nature of the FMS/CC composite endows it with abundant catalytically active sites, thereby accelerating the reduction of I3-. More importantly, the dye-sensitized solar cells (DSSCs) prepared by scraping it on flexible titanium mesh with low resistance had low series resistance (Rs). Electrochemical characterizations revealed that the DSSCs employing the FMS/CC counter electrode achieved a power conversion efficiency (PCE) of ca. 9.51% (surpassing the ca. 8.15% efficiency of the Pt counter electrode), open-circuit voltage (Voc) of ca. 0.79 V, short-circuit current density (Jsc) of ca. 18.31 mA·cm-2, and fill factor (FF) of ca. 0.65. Moreover, after 100 times of cyclic voltammetry (CV) test, the CV curve remainedunchanged, indicating the excellent stability of FMS/CC in the electrolyte containing I3-/I-.
【大学化学】doi: 10.3866/PKU.DXHX202310126
面向化学类(非高分子)专业的高分子化学实验教学发展较为缓慢,亟需紧跟研究前沿,引入新内容。本文总结了近十年的教学改革经验,并以温敏型高分子的制备、溶液性质、光学性能与应用为例,介绍如何通过实验教学内容、实验技术、教学方法等方面的创新,设计符合理科人才培养需求的、契合时代与科学发展的、被学生喜爱与重视的一系列高分子化学实验,以有效解决培养需求与课业负担之间的矛盾,且在不新增开课、课时有限的情况下,加入到化学类专业本科教学体系中,激发学生对学科领域的兴趣,提升学生的探究和创新能力。
【物理化学学报】doi: 10.1016/j.actphy.2025.100194
自组装单层(SAMs)是当前高效率反式钙钛矿太阳能电池(PSCs)中关键的空穴选择层材料(HSLs)。SAMs不仅决定了界面空穴的提取效率,还显著影响顶部钙钛矿层的薄膜质量,从而精细调控钙钛矿太阳能电池的效率和稳定性。本研究开发了一种新型SAM材料——(4-(8H-二萘并[2,3-c: 2',3'-g]咔唑-8-基)丁基)膦酸(4PADNC),它含有二萘并咔唑(DNC)结构单元,可作为反式PSCs的高性能HSL。与常用的咔唑类SAM (如4PACZ)相比,4PADNC中的DNC单元展现出扩展的π共轭特征,能够产生更大的分子偶极矩,从而调节氧化铟锡(ITO)电极的功函数,实现与钙钛矿能级的精准匹配,并显著降低界面能量损失。此外,该分子的非平面结构有效地抑制了π–π堆积,促进在ITO基底上形成致密且均匀的选择层,进而诱导高质量钙钛矿薄膜的沉积。得益于上述优势,采用4PADNC作为HSL的PSCs器件实现了24.32%的功率转换效率,显著优于基于4PACZ的参比器件(22.89%)。此外,基于4PADNC的器件还表现出卓越的热稳定性和运行稳定性。