Detection of Site-dependent Segmental Mobility of Polymer by Fluorescent Defocused Imaging

De-sheng Li Jing-fa Yang Jiang Zhao

Citation:  De-sheng Li, Jing-fa Yang, Jiang Zhao. Detection of Site-dependent Segmental Mobility of Polymer by Fluorescent Defocused Imaging[J]. Chinese Journal of Polymer Science, 2017, 35(12): 1488-1496. doi: 10.1007/s10118-017-1976-8 shu

Detection of Site-dependent Segmental Mobility of Polymer by Fluorescent Defocused Imaging

English


    1. [1]

      Xia, Y., Li, Y., Burts, A.O., Ottaviani, M.F., Tirrell, D.A., Johnson, J.A., Turro, N.J. and Grubbs, R.H., J. Am. Chem. Soc., 2011, 133(49):19953 doi: 10.1021/ja2085349

    2. [2]

      Das, S., Dubsky, P., van den Berg, A. and Eijkel, J.C.T., Phys. Rev. Lett., 2012, 108(13):138101 doi: 10.1103/PhysRevLett.108.138101

    3. [3]

      Luo, K., Ala-Nissila, T. and Ying, S.C., J. Chem. Phys., 2006, 124(3):034714 doi: 10.1063/1.2161189

    4. [4]

      Kong, C.Y. and Muthukumar, M., J. Chem. Phys., 2004, 120(7):3460 doi: 10.1063/1.1642588

    5. [5]

      Kumar, R. and Muthukumar, M., J. Chem. Phys., 2009, 131(19):194903 doi: 10.1063/1.3264632

    6. [6]

      Gennes, P.G.D., J. Chem. Phys., 1971, 55(2):572 doi: 10.1063/1.1675789

    7. [7]

      Ye, S., Tang, Q., Yang, J., Zhang, K. and Zhao, J., Soft Matter, 2016, 12(47):9520 doi: 10.1039/C6SM02103D

    8. [8]

      Ediger, M.D., Annu. Rev. Phys. Chem., 2000, 51:99 doi: 10.1146/annurev.physchem.51.1.99

    9. [9]

      Paeng, K. and Kaufman, L.J., Chem. Soc. Rev., 2014, 43(4):977 doi: 10.1039/C3CS60186B

    10. [10]

      Berthier, L. and Biroli, G., Rev. Mod. Phys., 2011, 83(2):587 doi: 10.1103/RevModPhys.83.587

    11. [11]

      Fox, J.T.G. and Flory, P.J., J. Appl. Phys., 1950, 21(6):581 doi: 10.1063/1.1699711

    12. [12]

      Angell, C.A., J. Phys. Chem. Solids, 1988, 49(8):863 doi: 10.1016/0022-3697(88)90002-9

    13. [13]

      Robertson, C.G. and Roland, C.M., J. Polym. Sci., Part B:Polym. Phys., 2004, 42(13):2604 doi: 10.1002/(ISSN)1099-0488

    14. [14]

      Tanaka, K., Jiang, X.Q., Nakamura, K., Takahara, A., Kajiyama, T., Ishizone, T., Hirao, A. and Nakahama, S., Macromolecules, 1998, 31(15):5148 doi: 10.1021/ma9712561

    15. [15]

      Ellison, C.J., Mundra, M.K. and Torkelson, J.M., Macromolecules, 2005, 38(5):1767 doi: 10.1021/ma047846y

    16. [16]

      Satomi, N., Tanaka, K., Takahara, A., Kajiyama, T., Ishizone, T. and Nakahama, S., Macromolecules, 2001, 34(25):8761 doi: 10.1021/ma010126w

    17. [17]

      Xie, F., Zhang, H.F., Lee, F.K., Du, B., Tsui, O.K.C., Yokoe, Y., Tanaka, K., Takahara, A., Kajiyama, T. and He, T., Macromolecules, 2002, 35(5):1491 doi: 10.1021/ma011689a

    18. [18]

      Zhang, L. and Torkelson, J.M., Polymer, 2015, 65:105 doi: 10.1016/j.polymer.2015.03.056

    19. [19]

      Miwa, Y., Shimada, S., Urakawa, O. and Nobukawa, S., Macromolecules, 2010, 43(17):7192 doi: 10.1021/ma1013644

    20. [20]

      Miwa, Y., Yamamoto, K., Sakaguchi, M., Sakai, M., Makita, S. and Shimada, S., Macromolecules, 2005, 38(3):832 doi: 10.1021/ma048287y

    21. [21]

      Plaza-García, S., Lund, R., Alegría, A., Colmenero, J., Janoski, J. and Quirk, R.P., Macromolecules, 2011, 44(19):7810 doi: 10.1021/ma2014436

    22. [22]

      Simpson, A.J., McNally, D.J. and Simpson, M.J., Prog. Nucl. Magn. Reson. Spectrosc., 2011, 58(3-4):97 doi: 10.1016/j.pnmrs.2010.09.001

    23. [23]

      Zheng, Z.L., Kuang, F.Y. and Zhao, J., Macromolecules, 2010, 43(7):3165 doi: 10.1021/ma902569n

    24. [24]

      Zhang, H., Tao, K., Liu, D., Wu, K., Wang, F., Yang, J. and Zhao, J., Soft Matter, 2016, 12(35):7299 doi: 10.1039/C6SM01447J

    25. [25]

      Deres, A., Floudas, G.A., Müllen, K., van der Auweraer, M., de Schryver, F., Enderlein, J., Uji-i, H. and Hofkens, J., Macromolecules, 2011, 44(24):9703 doi: 10.1021/ma201449p

    26. [26]

      Uji-i, H., Melnikov, S.M., Deres, A., Bergamini, G., de Schryver, F., Herrmann, A., Müllen, K., Enderlein, J. and Hofkens, J., Polymer, 2006, 47(7):2511 doi: 10.1016/j.polymer.2005.11.094

    27. [27]

      Enderlein, J., Phys. Rev. Lett., 2012, 108(10):108101 doi: 10.1103/PhysRevLett.108.108101

    28. [28]

      Matyjaszewski, K., Macromolecules, 2012, 45(10):4015 doi: 10.1021/ma3001719

    29. [29]

      Braeken, E., de Cremer, G., Marsal, P., Pèpe, G., Müllen, K. and Vallée, R.A.L., J. Am. Chem. Soc., 2009, 131(34):12201 doi: 10.1021/ja901636v

    30. [30]

      Schroeyers, W., Vallée, R., Patra, D., Hofkens, J., Habuchi, S., Vosch, T., Cotlet, M., Müllen, K., Enderlein, J. and de Schryver, F.C., J. Am. Chem. Soc., 2004, 126(44):14310 doi: 10.1021/ja0474603

    31. [31]

      Dorfschmid, M., Müllen, K., Zumbusch, A. and Wöll, D., Macromolecules, 2010, 43(14):6174 doi: 10.1021/ma100888s

    32. [32]

      Bailey, N.P., Schrøder, T.B. and Dyre, J.C., Phys. Rev. Lett., 2009, 102(5):055701 doi: 10.1103/PhysRevLett.102.055701

    33. [33]

      Chaudhuri, P., Berthier, L. and Kob, W., Phys. Rev. Lett., 2007, 99(6):060604 doi: 10.1103/PhysRevLett.99.060604

    34. [34]

      Adam, G. and Gibbs, J.H., J. Chem. Phys., 1965, 43(1):139 doi: 10.1063/1.1696442

    35. [35]

      Gibbs, J.H. and DiMarzio, E.A., J. Chem. Phys., 1958, 28(3):373 doi: 10.1063/1.1744141

  • 加载中
计量
  • PDF下载量:  0
  • 文章访问数:  2388
  • HTML全文浏览量:  340
文章相关
  • 发布日期:  2017-12-05
  • 收稿日期:  2017-04-08
  • 接受日期:  2017-05-10
  • 修回日期:  2017-05-09
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章