引用本文:
肖天存, 安立敦, 马军. 负载型贵金属催化剂Pd(Pt)/A12O3的硫中毒机理[J]. 应用化学,
1993, 10(1): 30-33.
Citation: Xiao Tiancun, An Lidun, Ma Jun. MECHANISM OF SULFUR POISONING ON SUPPORTED NOBLE METAL CATALYST Pd(Pt)/Al2O3[J]. Chinese Journal of Applied Chemistry, 1993, 10(1): 30-33.
Citation: Xiao Tiancun, An Lidun, Ma Jun. MECHANISM OF SULFUR POISONING ON SUPPORTED NOBLE METAL CATALYST Pd(Pt)/Al2O3[J]. Chinese Journal of Applied Chemistry, 1993, 10(1): 30-33.
负载型贵金属催化剂Pd(Pt)/A12O3的硫中毒机理
English
MECHANISM OF SULFUR POISONING ON SUPPORTED NOBLE METAL CATALYST Pd(Pt)/Al2O3
Abstract:
With the aid of CO and pyridine as probe molecules, infrared spectrophotorneter was employed to characterize the industrial catalyst Pd(Pt)/Al2O3 used for eliminating H2 from feed CO2 in urea synthesis. It is concluded that the factor which directly causes the deactivation of the catalyst comes from S2- and S22-, and the last factor resulting in the deactivation are S(Ⅵ) species:SO42- and Al2O3-SO3-H2O compounds.
-
-
扫一扫看文章
计量
- PDF下载量: 1
- 文章访问数: 1111
- HTML全文浏览量: 112

下载: