引用本文:
黄雪红, 柯盛波, 冀敏. 交联聚苯乙烯-丁二烯-苯乙烯双极膜的制备及其在电合成环氧丁二酸中的应用[J]. 应用化学,
2010, 27(11): 1306-1312.
doi:
10.3724/SP.J.1095.2010.00026
Citation: HUANG Xue-Hong, KE Sheng-Bo, JI Min. Preparation of Cross-linking Styrene-butadiene-styrene Triblock Copolymer Hybrid Bipolar Membrane and Its Application in Electro-generation of Trans-2,3-oxiranedicarboxylic Acid[J]. Chinese Journal of Applied Chemistry, 2010, 27(11): 1306-1312. doi: 10.3724/SP.J.1095.2010.00026
Citation: HUANG Xue-Hong, KE Sheng-Bo, JI Min. Preparation of Cross-linking Styrene-butadiene-styrene Triblock Copolymer Hybrid Bipolar Membrane and Its Application in Electro-generation of Trans-2,3-oxiranedicarboxylic Acid[J]. Chinese Journal of Applied Chemistry, 2010, 27(11): 1306-1312. doi: 10.3724/SP.J.1095.2010.00026
交联聚苯乙烯-丁二烯-苯乙烯双极膜的制备及其在电合成环氧丁二酸中的应用
摘要:
以聚苯乙烯-丁二烯-苯乙烯(SBS)嵌段共聚物作为基膜材料,采用自由基接枝聚合反应,在SBS主链上引入丙烯酸(AA)、苯乙烯磺酸和γ-甲基丙烯酰氧基丙基三甲氧基硅烷(KH570)链段作为阳离子交换膜;引入丙烯酸二甲基胺基乙酯和KH570链段作阴离子交换膜,阴、阳离子交换膜经KH570结构中三甲氧基硅烷基团的水解缩合,得到含硅氧交联网的SBS接枝离子交换膜,用流延法制备了SBS双极膜。测得SBS阴膜和阳膜的吸水率分别为63.9%和72.8%,SBS阴膜和阳膜的离子交换容量分别为1.51和2.71mmol/g。将SBS双极膜作为阴阳两室隔膜,采用钨酸钠/过钨酸钠体系由阴极间接电氧化合成了环氧丁二酸。结果表明,以石墨为阴、阳电极,电流密度为2.0×10-2A/cm2、50℃反应4h,环氧丁二酸的产率为53.0%,电流效率为40.8%。
English
Preparation of Cross-linking Styrene-butadiene-styrene Triblock Copolymer Hybrid Bipolar Membrane and Its Application in Electro-generation of Trans-2,3-oxiranedicarboxylic Acid
Abstract:
The cross-linking SBS hybrid bipolar membrane(SBS BPM) was prepared by free radical reaction of SBS(styrene-butadiene-styrene triblock copolymer) with acrylic acid(AA),sulfonic styrene(StSO3H) and γ-methacryloxypropyltrimethoxysilane(KH-570) as the anode membrane,and reaction of SBS with dimethyl amino ethyl methacrylate(DMAEMA) and KH-570 as the cathode membrane.Cross-linking reaction was carried out through sol-gel reaction of trimethoxysilane group.SBS BPM exhibited high temperature tolerance(thermal degradation temperature in N2,Td was up to 186.5℃).The ion exchange capacities(IECs) of the anode and cathode membranes were 1.51 and 2.71 mmol/g,respectively.SBS hybrid bipolar membranes were used as the separator in the electrolysis cell,then using tungstate/pertungstate as the media to indirect electrooxidate maleic acid to prepare trans-2,3-oxiranedicarboxylic acid in the cathode chamber.Graphite was used as the anode and cathode electrode.At 50℃ and when the current density was 2.0 × 10-2 A/cm2 for 4 h,the yield and average current efficiency of trans-2,3-oxiranedicarboxylic acid were 53.0% and 40.8%,respectively.
-
-
扫一扫看文章
计量
- PDF下载量: 3
- 文章访问数: 854
- HTML全文浏览量: 52

下载: