AlF3包覆对Li1.2Mn0.534Ni0.133Co0.133O2正极材料电化学性能的影响

王旭阳 叶学海 郅晓科 何爱珍 赵桢 章甦 时洁

引用本文: 王旭阳, 叶学海, 郅晓科, 何爱珍, 赵桢, 章甦, 时洁. AlF3包覆对Li1.2Mn0.534Ni0.133Co0.133O2正极材料电化学性能的影响[J]. 无机化学学报, 2013, 29(4): 774-778. doi: 10.3969/j.issn.1001-4861.2013.00.067 shu
Citation:  WANG Xu-Yang, YE Xue-Hai, ZHI Xiao-Ke, HE Ai-Zhen, ZHAO Zhen, ZHANG Su, SHI Jie. Effects of AlF3 Coating on the Electrochemical Performance of Li1.2Mn0.534Ni0.133Co0.133O2 Cathode Materials[J]. Chinese Journal of Inorganic Chemistry, 2013, 29(4): 774-778. doi: 10.3969/j.issn.1001-4861.2013.00.067 shu

AlF3包覆对Li1.2Mn0.534Ni0.133Co0.133O2正极材料电化学性能的影响

摘要: 通过共沉淀法制备锂离子电池富锂锰基正极材料Li1.2Mn0.534Ni0.133Co0.133O2, 并对其进行AlF3包覆。实验结果表明, 通过AlF3包覆, 材料的电化学性能得到明显提高。在0.2C下, 包覆前材料的首次放电比容量为253 mAh·g-1, 首次充放电效率仅为88.8%。经过AlF3包覆, 材料的首次放电比容量提高到294 mAh·g-1, 首次充放电效率高达96.4%。同样, 在1.0C下循环50次, 未包覆材料的放电比容量由225 mAh·g-1降到185 mAh·g-1, 容量保持率仅为82.2%。经过AlF3包覆, 材料的放电比容量由230 mAh·g-1仅降为222 mAh·g-1, 容量保持率高达96.5%。

English

  • 
    1. [1] LI Jie-Bin(李节宾), XU You-Long(徐友龙), DONG Xin(董 鑫), et al. Chinese J. Inorg. Chem.(Wuji Huaxue Xuebao), 2012,28(6):1125-1130[1] LI Jie-Bin(李节宾), XU You-Long(徐友龙), DONG Xin(董 鑫), et al. Chinese J. Inorg. Chem.(Wuji Huaxue Xuebao), 2012,28(6):1125-1130

    2. [2] DU Ke(杜柯), ZHAO Jun-Feng (赵军峰), WANG Wei-Gang (王伟刚), et al. Chinese J. Inorg. Chem.(Wuji Huaxue Xuebao), 2012,28(1):74-80[2] DU Ke(杜柯), ZHAO Jun-Feng (赵军峰), WANG Wei-Gang (王伟刚), et al. Chinese J. Inorg. Chem.(Wuji Huaxue Xuebao), 2012,28(1):74-80

    3. [3] ZHENG Jian-Ming(郑建明), WU Xiao-Biao(吴晓彪), YANG Yong(杨勇). Chinese J. Power Sources(Dianyuan Jishu), 2011,35(10):1188-1192[3] ZHENG Jian-Ming(郑建明), WU Xiao-Biao(吴晓彪), YANG Yong(杨勇). Chinese J. Power Sources(Dianyuan Jishu), 2011,35(10):1188-1192

    4. [4] Johson C S, Li N C, Lefief C, et al. Chem. Mater., 2008,20 (19):6095-6106[4] Johson C S, Li N C, Lefief C, et al. Chem. Mater., 2008,20 (19):6095-6106

    5. [5] Thackeray M, Kang S H, Johnson C S, et al. J. Mater. Chem., 2007,17(3):112-3125[5] Thackeray M, Kang S H, Johnson C S, et al. J. Mater. Chem., 2007,17(3):112-3125

    6. [6] DU Ke(杜 柯), HUANG Xia(黄霞), YANG Fei(杨菲), et al. Chinese J. Inorg. Chem.(Wuji Huaxue Xuebao), 2012,28(5): 983-988[6] DU Ke(杜 柯), HUANG Xia(黄霞), YANG Fei(杨菲), et al. Chinese J. Inorg. Chem.(Wuji Huaxue Xuebao), 2012,28(5): 983-988

    7. [7] XIN Sen(辛森), GUO Yu-Guo(郭玉国), WAN Li-Jun(万立 骏). Scientia Sinica Chimica(Zhongguo Kexue: Huaxue), 2011,41(8):1229-1239[7] XIN Sen(辛森), GUO Yu-Guo(郭玉国), WAN Li-Jun(万立 骏). Scientia Sinica Chimica(Zhongguo Kexue: Huaxue), 2011,41(8):1229-1239

    8. [8] He W, Qian J F, Cao Y L, et al. RSC Advances, 2012,2: 3423-3429[8] He W, Qian J F, Cao Y L, et al. RSC Advances, 2012,2: 3423-3429

    9. [9] Jung Y S, Cavanagh A S, Yan Y F, et al. J. Electrochem. Soc., 2011,158(12):A1298-1302[9] Jung Y S, Cavanagh A S, Yan Y F, et al. J. Electrochem. Soc., 2011,158(12):A1298-1302

    10. [10] Wu Y, Manthiram A. Solid State Ionics, 2009,180(1):50-56[10] Wu Y, Manthiram A. Solid State Ionics, 2009,180(1):50-56

    11. [11] Lee E S, Manthiram A. J. Electrochem. Soc., 2011,158(1): A47-A50[11] Lee E S, Manthiram A. J. Electrochem. Soc., 2011,158(1): A47-A50

    12. [12] HU Chuan-Yue(胡传跃), GUO Jun(郭军), WANG Xing-Yan (汪形艳), et al. J. Xiangtan Normal Univ.(Xiangtan Shifan Xueyuan Xuebao), 2009,31(3):15-17[12] HU Chuan-Yue(胡传跃), GUO Jun(郭军), WANG Xing-Yan (汪形艳), et al. J. Xiangtan Normal Univ.(Xiangtan Shifan Xueyuan Xuebao), 2009,31(3):15-17

    13. [13] Zheng J M, Zhang Z R, Wu X B, et al. J. Electrochem. Soc., 2008,155(10):A775-A782[13] Zheng J M, Zhang Z R, Wu X B, et al. J. Electrochem. Soc., 2008,155(10):A775-A782

    14. [14] Deng H, Belharouak I, Yoon C S, et al. J. Electrochem. Soc., 2012,157(10):A1035-A1039[14] Deng H, Belharouak I, Yoon C S, et al. J. Electrochem. Soc., 2012,157(10):A1035-A1039

    15. [15] Sun Y K, Cho S W, Lee S W, et al. J. Electrochem. Soc., 2007,154(3):A168-A172[15] Sun Y K, Cho S W, Lee S W, et al. J. Electrochem. Soc., 2007,154(3):A168-A172

    16. [16] Liu B, Zhang Q, He S C, et al. Electrochim. Acta, 2011,56 (19):6748-6751[16] Liu B, Zhang Q, He S C, et al. Electrochim. Acta, 2011,56 (19):6748-6751

    17. [17] Shi J Y, Yi C W, Kim K. J. Power Sources, 2010,195:6860-6866[17] Shi J Y, Yi C W, Kim K. J. Power Sources, 2010,195:6860-6866

    18. [18] Woo S U, Yoon C S, Amine K, et al. J. Electrochem. Soc., 2007,154(10):A1005-A1009[18] Woo S U, Yoon C S, Amine K, et al. J. Electrochem. Soc., 2007,154(10):A1005-A1009

    19. [19] Lee D J, Lee K S, Sun Y K. J. Power Sources, 2011,196: 1353-1357[19] Lee D J, Lee K S, Sun Y K. J. Power Sources, 2011,196: 1353-1357

    20. [20] Yang K, Fan L Z, Guo J, et al. Electrochim. Acta, 2012,63: 363-368[20] Yang K, Fan L Z, Guo J, et al. Electrochim. Acta, 2012,63: 363-368

    21. [21] Gao J, Manthiram A. J. Power Sources, 2009,191(2):644-647[21] Gao J, Manthiram A. J. Power Sources, 2009,191(2):644-647

    22. [22] LI Jie(李劼), ZHENG Jian-Ming(郑建明), GUO Xiao-Jian(郭 晓健). Chem. J. Chinese Universities(Gaodeng Xuexiao Huaxue Xuebao), 2006,27(7):1311-1314[22] LI Jie(李劼), ZHENG Jian-Ming(郑建明), GUO Xiao-Jian(郭 晓健). Chem. J. Chinese Universities(Gaodeng Xuexiao Huaxue Xuebao), 2006,27(7):1311-1314

    23. [23] Robertson A D, Bruce P G. Chem. Mater., 2003,15(10):1984 -1992[23] Robertson A D, Bruce P G. Chem. Mater., 2003,15(10):1984 -1992

    24. [24] Li G R, Feng X, Gao X P, et al. Electrochim. Acta, 2012, 78:308-315[24] Li G R, Feng X, Gao X P, et al. Electrochim. Acta, 2012, 78:308-315

    25. [25] Kim J H, Parka M S, Song J H, et al. J. Alloys Compd., 2012,517:20-25[25] Kim J H, Parka M S, Song J H, et al. J. Alloys Compd., 2012,517:20-25

  • 加载中
计量
  • PDF下载量:  239
  • 文章访问数:  827
  • HTML全文浏览量:  46
文章相关
  • 收稿日期:  2012-08-26
  • 网络出版日期:  2012-09-28
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

/

返回文章